1 Piece routed MDF door - shaker style

7/5/18       
saturnfan

I am new to CNC and looking for an advice to make 1 piece routed mdf door (shaker style) using Biesse cnc router. Pocket is 1/4" Deep. What kind of router bit do I need? How many pass do I need to get good finish? How long does it take to cut one 4' x 8' sheet. I am also wondering if it will be feasible for me to make my own doors with good quality or outsource it. How are you guys doing it?


View higher quality, full size image (500 X 662)

7/6/18       #2: 1 Piece routed MDF door - shaker st ...
Dropout Member

2" diamond, then 3/8 or 1/2 on the perimeter, then 1/8 on the perimeter.

It's very doable. Thousands of these doors are made every day.

The hard part is balancing the depth of the three tools with the tendency of the MDF to raise off the table as you cut the pockets. Melamine backed MDF helps. Some have said that you should cut the outside dimension first (not all the way through) to avoid that.

7/6/18       #3: 1 Piece routed MDF door - shaker st ...
Jared

Ditto on MDF bending when you cut that front pocket. For doors bigger than 24" wide or tall, I go through the trouble of first cutting a 1/8" deep pocket on the back side of the doors, and it seems to mitigate the warp somewhat. Not sure what software you're using, but Cabinet Vision makes it easy to do this. I use a 1-1/2 diameter mini flycutter from Amana to hog out most of the pocket, then work the pocket's perimeter with a 1/4" downshear, then sharpen the corners with a 1/16" downshear. I prefer sharp inside corners because most of our doors get applied moulding of some kind, and a 1/32" radius on the inside is sharp enough for the moulding miter.

Time per sheet depends on cutters. I do a lot of back-side cutting: door hinges, drawer adjuster holes and back-routing pockets for big doors. With front and back processing it can add up to 20ish min per sheet. It's still considerably faster and more accurate than stick-built shaker doors.

7/10/18       #4: 1 Piece routed MDF door - shaker st ...
saturnfan Member

I contacted a local sales guy and he advised me to buy Royce Ayr - Diamond pocketing tool, Vortex upcut Bottom Surfacing Cutter 3/8" and 1/8".

I am planning to use mdf with melamine back but I am concerned that mdf will raise off the table with upcut router bit. What do you guys think?
Thanks a lot.

7/10/18       #5: 1 Piece routed MDF door - shaker st ...
Jared

Depends on the strength of your hold-down vacuum, and also on the order in which you cut. Cut all the pockets first, then the perimeter and you should be ok.

7/11/18       #6: 1 Piece routed MDF door - shaker st ...
saturnfan Member

What's the purpose of using 1/4" downcut and then again 1/16" downcut?
thanks

7/11/18       #7: 1 Piece routed MDF door - shaker st ...
Jared

It's to sharpen the inside corners quickly. The area my 1-1/4 cutter misses is too big for a 1/16 to quickly route out. The 1/4 bit makes quick work of it and makes less area for the 1/16 to finish the job.

8/23/23       #8: 1 Piece routed MDF door - shaker st ...
Rudi Froese

hello i have a question what kind of mdf do you guys use for making the doors so it does not turn all fuzy in the poket after cutting it i was told hdf but i cant find it

4/4/26       #11: 1 Piece routed MDF door - shaker st ...
jeff bowen

tools today has a free program that i downloaded and used works great just doesnt include the pocket for the euro style hinges but thats easy enough with the Kreg jig


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA
    Sponsors
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • Country Saw and Knife
      Complete Sharpening Services for Wood and Metal Saw Blades, Jointer Knives, and Bandsaw Blades
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • Weinig Group-USA
      Wood Moulders and Knife Grinding Equipment
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Felder USA
      High Quality Woodworking Machines and Tools

    Become a Sponsor today!