routing kerfkore

1/12/20       
Pat Gilbert

I need to rout some kerfkore perpendicular to the ribs. I'm concerned that the router would knock the ribs loose.

Has anyone done this?

TIA

1/12/20       #2: routing kerfkore ...
duster

I've never tried to route kerfcore, but if I was going to I'd try a down shear bit and climb feed.

1/13/20       #3: routing kerfkore ...
Mike Mandelert

Yes, you will have difficulty. I make my own, but I have a saw on the machine for a thin kerf blade. If you do have a saw, cut the shape first, then make the saw cuts. Been our standard for over 15 years.

1/13/20       #4: routing kerfkore ...
Pat Gilbert

This is a scalloped shape so it has to be routed.

Thanks for the input though

1/13/20       #5: routing kerfkore ...
Jared

I've routed it before, both with straight and downshear bits. It self-destructs like you'd imagine.

1/13/20       #6: routing kerfkore ...
Pat Gilbert

Thanks Jared

1/14/20       #7: routing kerfkore ...
BH Davis  Member

Website: http://www.bhdavis.net

Pat,

One sheet or a large run? If just one sheet perhaps you could rip some filler strips and set them in the slots. Then either kerf down if that can be accomplished without the strips falling out or kerf up with a waste cover sheet (depending on the porosity of the kerf core material).

BH Davis

1/14/20       #8: routing kerfkore ...
Pat Gilbert

Thanks for the idea Bernie

It is just one reception desk.

1/14/20       #9: routing kerfkore ...
cabinetmaker

I Plam the keercore and throw it on the machine Plam side down. We estimate what’s cut where and put strips in with yellow glue overnight Including the access panels for the back area of the reception desk. We use a 3/16 down cut

1/14/20       #10: routing kerfkore ...
BH Davis  Member

Website: http://www.bhdavis.net

Pat,

Another way to do this is to make, say, a curved desk front full height all the way around. Assuming then that you need to cut a pattern into the face of this curved front you can cut that curve on the flat (as you would have done with the Kerfcore) on the CNC into a sheet of 3/8" wacky wood (bending ply).

You can then lay the wacky wood template onto the pre-made Kerfcore front and use it as a routing template for a hand held router with a template guide.

This should give you a clean final cut as the Kerfcore will be locked into position with, I assume, a glued on rear face layer.

An alternative of course is to just cut the pattern into 2 or 3 layers of the bending ply and laminate them together at the final curved shape. Personally I've never been a big fan of Kerfcore and almost always used multiple layers of bending ply.

BH Davis

1/15/20       #11: routing kerfkore ...
Pat Gilbert

I think I'm just going to use mdf as I can use the pony wall as a form and glue 2 3/8" mdf pieces or 1/4" (it's a big radius) with plastic resin glue.

Then make a jig for scalloping the curved piece with a hand router with a guide bushing.

This way I can laminate the edge easily.

Cabinetmaker

Are you saying you glue the filler pieces into to the edge of where you are routing so that they don't interfere with kerkore after the material is cut?

Thanks both of you for good ideas

1/15/20       #12: routing kerfkore ...
jerry Member

We use wiggle board for this kind of stuff

1/16/20       #13: routing kerfkore ...
cabinetmaker

Pat we have run a ton of kerfcore for several projects and have learned just a little extra time in a prep leads to a lot less frustration

Yes estimate the cut area and place filler pieces in the kerf section just enough to let the router cut into solid areas and reduce the blow out. So instead of a just a bunch broken slats after the fact, we have good solid areas that can be painted or laminated

1/17/20       #14: routing kerfkore ...
Pat Gilbert

Thanks Cabinetmaker

What is the advantage of this over forming the on the pony wall? Do you laminate before bending?


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • Weinig Group-USA
      Wood Moulders and Knife Grinding Equipment
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Country Saw and Knife
      Complete Sharpening Services for Wood and Metal Saw Blades, Jointer Knives, and Bandsaw Blades
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!

    Become a Sponsor today!