Hi, I use 1/2 inch compression bits for cutting 3/4 inch ply, mdf and ply with melamine sheets. Cut quality is great on top and bottom edges but sometimes it shows some fibers on ply, striped patters (more noticeable on MDF and loosely matching the compression spiral drawing) and diagonal marks on the edge itself (from the lead ins and outs). I was wondering if using a straight cutter after would improve the overall edge finish. I am not too concern on adding additional time if this saves from doing additional manual post processing after. Many thanks!

10/20/21       #2: CNC improving edge cut quality when ...
Mike

What is your chip load? If unsure, post your feed, speed and number of flutes on your tool.

10/20/21       #3: CNC improving edge cut quality when ...
Javitojavito Member

2 flutes compression bit, cut feed 200ipm and spindle speed of 20000rpm

10/20/21       #4: CNC improving edge cut quality when ...
Stephen Williams Sponsor - Parts Cutter CNC

Website: http://www.partscuttercnc.com

Crazy slow

2 x .021 x 20000 = 840ipm

Get an Onsrud book

If you are getting milling marks its probably from movement, what kind of vacuum do you have?

10/20/21       #5: CNC improving edge cut quality when ...
Javitojavito Member

Thanks will do. Vacuum is a becker pump 5kw, seems ok for cabinet parts but drawer parts need onion skinning and/or tabs when pieces are long and very thin. Could be the slow feed rate? when using my festool hand router with a straight bit I got very smooth finish at lower feed rates. Many thanks again!

10/20/21       #6: CNC improving edge cut quality when ...
Stephen Williams Sponsor - Parts Cutter CNC

Website: http://www.partscuttercnc.com

You are killing your bits at such a slow speed.

I would say you need more vacuum

10/20/21       #7: CNC improving edge cut quality when ...
Mike

Yes, at that feedrate your chipload is 0.005 which is way to small. Can your machine get to around 800ipm? if not, slow your rpms down and up your feedrate. My typical chipload is 0.019 for a variety of materials used in cabinet making.
Chipload = Feedrate / (RPM * # of Cutting Edges)

11/2/21       #9: CNC improving edge cut quality when ...
AcctekChina Member

Website: https://www.acctekgroup.com/CNCRouter/

Generally, for holes with a diameter of less than 6mm, if the accuracy is not high, use hand pliers to clamp the workpiece for drilling; for holes of 6 to 10mm, if the workpiece is regular and even, flat-nose pliers can be used to hold the workpiece, but the workpiece should be clamped The surface is perpendicular to the spindle of the drilling machine. When drilling a hole with a larger diameter, the flat-nose pliers must be fixed with a bolt pressing plate; for larger workpieces with a hole diameter of 10mm or more, the pressing plate clamping method is used to drill the hole.


View higher quality, full size image (1165 X 465)

Economic ATC CNC Router


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • Weinig Group-USA
      Wood Moulders and Knife Grinding Equipment
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Country Saw and Knife
      Complete Sharpening Services for Wood and Metal Saw Blades, Jointer Knives, and Bandsaw Blades
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!

    Become a Sponsor today!