Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Finish Products & Techniques

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Finish Products & Techniques

9/26/15       
Josh Member

I've recently taken on some small batch production work making wood plaques, trophy stands, signs and so on. I'm looking for some advice on what the best finish products and techniques would be for a one man operation needing to keep expenses and finish time to a minimum. This contract has potential to yield pretty high quantities of products and hand rubbed stains with spray on urethane is way too time consuming. Need help!

9/26/15       #2: Finish Products & Techniques ...
Denny J

This is why nobody else is doing it. Small items have a high cost to finish and without the right setup it is hard to make money on.

How many pieces will you do a week, how big are they, what wood and color do they need to be and how much does the finishing budget allow per piece?

9/27/15       #3: Finish Products & Techniques ...
Josh Member

Quantity could be anywhere from 10 to 50 pieces per week. I'm primarily working with red oak but am trying to find a cost effective species that's easier to work. Pieces range in size from a small 12"x12" plaque to a 4'x8' sign. Stain colors can range as well but most of it is the typical golden oak. I haven't quite figured out how much to allow for finishing.

9/27/15       #4: Finish Products & Techniques ...
RobertJ

Spray Stain and UV curtain coater.

The above method is the most efficient.
Everything else is time and materials, and
Labor intensive and costly.

9/27/15       #5: Finish Products & Techniques ...
Denny J

My $.02 would consist of the following:

Plaques,trophy bases and such are not high usage items.They are also not color specific so rather than using oak and adding the cost to prep and stain, I would use a wood such as Walnut,Maple,Cherry etc that look good without any stain in order to eliminate a step as well as inventory. A small increase in price on wood can be made up with lower finishing costs.

Secondly, on the finish schedule the volume is far too low to consider production systems like UV and the durability is not warranted. I would set a minimum number of products needed to fill a full work day and then divide that number by your shop rate to figure out what to charge and then only finish them in batches so you are efficient.

As far as the product, any nitrocellulose lacquer will work if you have a booth and 2 coats would be acceptable. If no spray booth I would look at just using a tung oil or similar finish as that would be very quick and easy on small pieces.

If you have access to similar products being produced in the price range you are at, figure out what finishes they use as well and match it.

9/27/15       #6: Finish Products & Techniques ...
jimmy cream

why not pre-cat ?

agreed that durability is not a major concern ; but pre-cat is no more difficult to use than nitro , no more costly ( I pay more for nitro than pre-cat from my supplier ) , and builds a bit better .

9/27/15       #7: Finish Products & Techniques ...
JeffA

Curtain coater and UV coatings? I used to purchase UV in drums and it was over $45.00 a gallon. I'm sure Josh is a small user and would have to pay through the nose for that. As for the curtain coater, I wonder if mine is still in the back of my garage?

9/27/15       #8: Finish Products & Techniques ...
Josh Member

Thanks for all the helpful information everyone. I'm going to be speaking with a local finish supplier tomorrow about products. I've avoided 2 part laquers because we do not have a spray booth and can't afford one right now. I'm currently spraying General Finishes Arm R Seal over their oil based stains. The process is just too labor intensive. I'm doing one coat of wiping stain, then 2/3 coats of Arm R Seal to get a decent finish. If I go with a laquer, should I add a sanding sealer in the mix? I like the idea of a wipe on togue oil type finish, but am afraid the customer wants to keep some color options other than natural wood.

9/27/15       #9: Finish Products & Techniques ...
Denny J

Josh
Generally money talks and if you tell the customer it is going to cost a premium to have the option of colors they will suddenly find clear coats more than sufficient.

If they do insist on stains, explain to them the process and the need for additional charges and if they agree the extra steps add value to the product then you can increase your rate accordingly.

As to the question from the poster about Pre cat vs NC, If you can do it for the same or less then sure. In my area NC is less expensive than PreCat and has the advantage of burn in without needed to scuff without worrying about recoat windows. But I am not saying it wont work.

9/28/15       #10: Finish Products & Techniques ...
Howard

If you must stain, use a fast drying NGR or alcohol based stain. The quick dry time allows you to go right to finishing. Have you thought about spraying shellac, since you don;t have a booth it dries very fast so no worries with dust. A coat of wax and then a power buffing and you're good to go.

9/30/15       #11: Finish Products & Techniques ...
John Member

SW's BAC Wiping Stains can be brush or spray applied, then wiped, and topcoated in a couple of hours. They are terrific but my experience is limited compared to many others here. Arm-R-Seal is a great product but it dries far too slowly and the overspray makes a mess. I'd switch to a waterborne like GF's Enduro Lacquer. It dries quickly, and can be scuff sanded and recoated in about an hour. Cleanup is a breeze.

I'd get away from oak, too. Cherry, walnut, or alder would be far better for ease of finishing.

John

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)