Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: stain mixing

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

stain mixing

2/19/16       
Dave

i have a millworker doing about 100k of work at my jobsite and for budget and time reasons we were gonna do a few of the add ons ourselves. it was a long process of them getting the right color that the client liked so I asked him for the recipe/formula of the stain mix so we could match it with our own woodwork. after we completed the finish it didn't match at all. he now states that "every finisher should know you need to add a reducer to the stain based on how youre applying it.". the stain was a blend of 3 Mohawk penetrating wiping stains. what are your thoughts on that? i am not a professional wood finisher but have never used a reducer and it doesn't come to mind to ask when using a wiping wood stain.

2/19/16       #2: stain mixing ...
Robert Member

Is it on Maple...maybe they meant a conditioner.
The type of wood and how its sanded etc... has a big influence on how the color comes out. Got some pictures you could share.

2/19/16       #3: stain mixing ...
denny

Well...I made stains for years. If he was matching something in the field, and getting client approval (adjusting the color a few times), I am not sure how he would be able to develop a repeatable "formula". The real question is...where is the stain.?
"You" ALWAYS make 2x-3x as much as you need.....especially considering he knew you would need it.!
Stain is cheap, labor is expensive.....he did not have one drop left.?

2/19/16       #4: stain mixing ...
nick

I'm sorry to say...what every finisher learns (usually the hard way...like yourself) is to have an approved sample handy when staining and to check it often against what your staining while your staining.
If you're asking whose fault it is now that you have the wrong color? the answer is always; everybody involved. If you're asking whose libel? in my experience, it the person who did the finishing.

2/19/16       #5: stain mixing ...
rich c.

Two people working from the same can of penetrating wiping stain, can get two different final colors. How wet you keep it when applying, how fast you wipe it off, how large of area you work, etc. As Robert mentioned, preparation and what grit sand paper you use makes a difference too. Not to mention different boards from different trees, and different sheets of plywood as well.

2/20/16       #6: stain mixing ...
Alessio

As a finisher, in the past I've made a stain to match a requested colour on oak for example, but for whatever reason, when all the parts were ready for finishing they are aldready darker than my control sample. At this point you can reduce your stain mixture, and through shading/toning work back up to your control sample. Be careful to use the right reducer, the solvent must evaporate slowly enough to let the stain dry, or else you will have problems when you spray your lacquer

2/20/16       #7: stain mixing ...
Alan  Member

As a finisher, one always has to be able to make adjustments on the fly. Many times I have matched a stain sample, only to have the job come in and have the wood be a slightly different color (more red, tan etc.), making the stain look a little different from the control sample. One has to make an adjustment sometimes changing the viscosity of the stain (adding reducer/retarder), possibly changing up the sanding schedule (lower/higher grit), adding more clear base to the stain to keep it from giving more grain bite, or even changing the way the stain is applied. A good finisher knows how to make these adjustments and keep the job moving. I understand wanting to save some time and money by doing the finishing yourself. No offence intended, but perhaps this may be one of those cases where it would have been better to let the professional finisher perform his craft that he has honed over the years? I could not build a marvelous piece of furniture, even though I have seen it done many times, and I know how to run a table saw and a router, etc. I know my limitations. I would let the master craftsman who has spent his life building furniture do that for me. Just my opinion, anyway.

2/20/16       #8: stain mixing ...
Pat

It's fairly common to reduce stain to tone down the intensity of the color. If used, the amount of reducer in the mix is a key part of the recipe. He should have given it to you. However, all of the other advice about application methods, timing, wiping, etc. are also true, and especially the need to match against a control sample. That's on you. It's a painful lesson that most of us have probably experienced.

2/22/16       #9: stain mixing ...
Dave

Thanks everyone for the responses. I know in the end its our responsibility to ensure an accurate match. I was more wondering about his common response that every good finisher knows youll need to add a reducer, but I asked him for his formula on the exact same product, and the client was ok with a slight variation of theirs vs ours but he reduced it so much 10 reducer to 1 stain that it wasn't even close. oh well should have done a sample to be approved.

2/24/16       #10: stain mixing ...
Scott

It is not common practice to reduce stain. It is done when needed for a desired color only. If that was part of the formula than he should have told you but you also should of had a sample board from him to check your stain against.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)