Subject: Re: Cat AAA H2O and Tip clogging nitemare

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Cat AAA H2O and Tip clogging nitemare

7/17/16       
Shawn Lalande Member

I am in the process of spraying 2000 sq ft of panels and doors for a full house project. I have a CA technologies AAA H2o set up and using a 409F tip
I started with Val spar zenith which worked real well but my supplier only had 1 pail so I switched to ML Campbell Aqualente which I have used before with this setup and had no problems. The minute this batch of Aqualente hit the tip it clogged the tip. I clean the tip and repeat several times; same thing. I reduce the Aqualente it starts to spray this last for several hours clogs again same thing clean tip won't spray, clean again won't spray. At this point the gun and pump get torn apart and cleaned thoroughly no problems there. Clean tips I have 3 and try again sprays for a few minutes tip clogged, 2nd tip same thing, 3rd tip same, I give up, the gun will spray everything but the Aqualente has any one had this type of problem with AAA setup and water borne top coat.

7/18/16       #2: Cat AAA H2O and Tip clogging nitema ...
Shane

sounds like the waterborne is full of solids that are not broken up properly. Mix well and run the whole batch of paint through a fine cone strainer into a fresh clean containe rand be disgusted how much lint hair and solid chunks are in a stock can of paint... We strain everything through fine strainers before topcoating. amazing the junk that's in your paint. Obviously make sure to flush your lines with a couple batches of appropriate clean solvent. Clean your screens. Take off tip seal and clean behind there and give the tip a slight poke with the tip needle...... all better?

7/18/16       #3: Cat AAA H2O and Tip clogging nitema ...
Shawn Lalande Member

Done all that except straining; thought filters took care of that. I have cleaned tips thoroughly probably 30 times behind seals and have gone through an entire package of tip cleaning needles. Whatever is blocking tips is hard and is bending needles.

7/18/16       #4: Cat AAA H2O and Tip clogging nitema ...
Bruce Hand Member

Hello wondering if you removed the screen inside the tip. I always remove the screen when spraying WB.
I purchased a ultrasonic cleaner and use a 5-1 solution of Citrasolv concentrate to clean all my tips and gun parts on my Kremlin Xcite gun
It really cleans up all the parts

7/18/16       #5: Cat AAA H2O and Tip clogging nitema ...
Mark B Member

+1 to the straining. Ive been spraying Agualente for about 5 years now and if you visually just drill the finish with a small mixer you can see the solids. Ive drilled a pail of finish for an hour and its still there. One, or even two, passes through a medium mesh screen and the finish is clear as a bell. If the finish sits for any amount of time in the pail I repeat the process (week or two).

7/18/16       #6: Cat AAA H2O and Tip clogging nitema ...
Mark B Member

Additionally, If you think about it, all those solids that came out of suspension and are now clumped together are suppose to be in your finish. When I strain once or twice there is generally little to nothing in my cone filter when done. Occasional stirring works it all through the mesh and only the coarsest material is left behind (usually very little for me).

7/19/16       #7: Cat AAA H2O and Tip clogging nitema ...
Shawn Lalande Member

Mark why would you go through all that trouble when there are other products that do not have this issue. I have have sprayed gallons of Zenith with very little clogging issues all with no straining and minimal mixing. I am done with ML Campbell. Due to a deadline I am completing this job with a gravity fed gun. I have ordered a pail of Chemcraft to try for my next project as my Zenith supplier is no longer stocking the sheen I like. Also waiting to hear from Sherman-Williams about Sayerlack which other people here have said good things about.
Thanks for your responses guys

7/19/16       #8: Cat AAA H2O and Tip clogging nitema ...
Bruce Hand Member

Hello I totally agree, I prefer SW Kem Aqua plus. The ML Campbell Aqualente did not dry as hard, and the satin had a higher sheen than what I wanted.
The Kem Aqua was 25% cheaper in my area also. Good to try different products
I did not have any issues with tip plugging but did check and clean the tip between coats. Sprayed 50 doors 2 coats per side

7/19/16       #9: Cat AAA H2O and Tip clogging nitema ...
MarkB Member

I don't use aqualente exclusively but have sprayed a lot of it due to local distribution. Even my local sherwin distributor does almost nothing with their commercial fibish line. I sprayed sayerlack AF72 for a good while and agree, the mixing issues are much less. That said I always mix/strain all my finish and don't even expect automotive finishes to require no mixing and straining. I have personally never come across any material other than solvents that don't require mixing after they have been stored for a period.

I do notice as was mentioned the new formulation of agualente is drying slower through I cant say it seems noticably softer.

I have a few gallons of other materials in the shop to test for a possible switch from mlc as well. Unfortunately I'm in a location with virtually no local distribution of many common finishes.

7/19/16       #10: Cat AAA H2O and Tip clogging nitema ...
Pat

Try a 411 tip.

7/19/16       #11: Cat AAA H2O and Tip clogging nitema ...
Shawn Lalande Member

Got the Chem-craft in this morning stirred for a minute or two put tube in pail and started spraying. Sprayed all day and them some (I am behind) no problems not one tip blockage. Very Nice stuff this Chem-Craft Acryllak lays down nice, very smooth to the touch when dry. May have been a batch of messed up Aqualente but I will not take a chance on a repeat so I think I will kept using the Chem-Craft for now

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)