Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: fine finish + exterior

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

fine finish + exterior

9/4/16       
Jay

fine finish + exterior, -here's another:
"high jump + low ceiling"

I primarily use SW Kemvar Plus and F3 Kemvar lines for most of what I finish
(for example: ngr dye stain, wash coat, BAC wiping stain, sealer, glaze, sealer, toner, top coat, is a typical schedule...

I just took on a very high end Entry Door project, and Im having a devil of a time finding a finish system in which to use...

my 1st thoughts were 2k (aliphatic) polyurethane , yet everyone Im finding are clearly marketed as "interior"

My multi-step CV finishes are quite distinctive, and are part of ou appeal, but of course these are for interior applications only.

can anyone recommend any suggestions which we might look into?

SW rep is stuck at "a couple coats of Sikkens or a Spar Varnish"
and while a really nice & durable finish can definitely be obtained with single products like those, Id much prefer the versatility of our CV systems...

9/4/16       #2: fine finish + exterior ...
CraigM

Look into Sirca (or any of the Italian companies), they seem to have the best exterior clears. I have mainly used the Sirca products with good results. I have generally put them over spray or wiping stains with a spray glaze if needed, have not made toners with them.

9/5/16       #3: fine finish + exterior ...
nick

d-dur from chemcraft is available through Wurth louis &Co. Euro X from M L Campbell. Both are 2k pu and rated for exterior. spendy...$200.00 (+/-) per gallon (poly, hardener, reducer).
If your door is out of the weather a bit: Rudd Prothane would work (1k poly, $40-$60 per gal.)). or you could go WB...many options there (Target 9300 comes to mind)
You should be able to do your multi-step finish with any of these products.
Nothing lasts outside so to protect your work for the long term, consider selling your customer a maintenance contract.

9/5/16       #4: fine finish + exterior ...
Leo G

I used the Target EM 9300 and it worked well. Has to go on at 2-3 mil so expect to put a few coats on. It doesn't have a dry film mil thickness so you can put on plenty of coats. It can be sprayed or brushed, so periodic maintenance can be done onsite with a brush.

The door I did was 7 years ago. It's in a protective area but is exposed to the weather. Can't tell you how this might react if it's a full sun door.

9/5/16       #5: fine finish + exterior ...
Gerry

If you have a distributor for ICA in your vicinity I think it would do the job for you. You need to add their UV inhibitor to the finish but it is very durable. I have been using their OAC363 product and it can be used with their toners and glaze products.

The cost can add up with all the components required.

HTH
Gerry

9/6/16       #6: fine finish + exterior ...
RobertJ

Keep in mind the need to 'refinish' the door down the road. If you are glazing and toning the door I doubt they are going to be UV resistant. If you can get ICA coatings in your area, let them make you one of their stains. Otherwise, use 2K Poly. Good for 5 years if not in direct sunlight.

9/6/16       #7: fine finish + exterior ...
kevin

use sherwin williams F63FH2. it is exterior polyurethane. Its right in line with the products your familiar with and is super durable.

9/7/16       #8: fine finish + exterior ...
Bill Richardson  Member

Website: http://www.awwtx.com

I've used Klima from Ilva with good results.

http://www.ics-ilva.com/exterior-waterborne-finishes.php

9/8/16       #9: fine finish + exterior ...
dar

2k way to go still wont last in direct sun, Gerry what is oac363 from ICA ? I use lp157
for exterior , is this something new?

9/8/16       #10: fine finish + exterior ...
Robert Member

Has anyone tried an Automotive clear for an application like Jay's ?

9/8/16       #11: fine finish + exterior ...
Gerry

Hi Dar,

I first used OAC 363 when it was recommended by the ICA rep for a fiberglass door. I have attached the spec sheet. It is available in higher gloss, the one I have been using is 20 degree.

Click the link below to download the file included with this post.

oac363g20.pdf



Click the link below to download the file included with this post.

OAC363G20_____________2014.pdf

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)