Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Surf Prep System

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Surf Prep System

12/29/16       
scott

We spray Magna Max pre cat and CV, hand sand between each coat, is anyone familiar with the surf prep system and does it work well for the in between sanding of coats? Is there an issue with sanding thru the previous coat? Any answers appreciated would like to speed up the finishing process. Paint finish = 2 coats of clawlock and 3 coat of magnamax. wood finish= stain, 3 coats of satin magnamax.

12/29/16       #2: Surf Prep System ...
JoeW Member

I have used the Surf Prep for couple years now with MLC waterborne products. It has worked great. Just make sure you let the product dry properly. I have seen it demonstrated on other MLC solvent based products and it worked great.

I would never go back to hand sanding it has saved me a great deal of time. Once you try it you will be amazed.

12/29/16       #3: Surf Prep System ...
JoeW Member

Also. It is rare to see a sand thru.. You have to really get careless for that to happen.

12/31/16       #4: Surf Prep System ...
Dan cook

If you get a sand thru what can you do to hide it again? Seems like there is always a kind of halo effect once that happens and stripping the finish off is a huge pain.

12/31/16       #5: Surf Prep System ...
Dean Member

Is this system much different than putting a thick interface pad on a festool sander? I really do not want to get into air sanders. I have enough money in Festool stuff already. I am a painting contractor, so need stuff that works well in the shop and in the field.

1/1/17       #6: Surf Prep System ...
JoeW Member

Dean,

There is an electric Surf Prep now. I too would rather use electric over air. But The electric wasn't available at the time I purchased.

I too am highly invested in Festool. I use it for everything except sanding between finishes. I spray only waterborne precat Lacquer. I tried most every combination with the festool sanders and just couldn't make it work for me. Then my supplier stopped by my shop and wanted to demo the Surf Prep for me. I bought it that day.. It is so easy and fast. And best of all the sanding pads don't clog. Unless of course you try to sand too soon.

1/1/17       #7: Surf Prep System ...
Charles

If I understand it correctly, the "electric" version includes an air pump that drives the sander? I was looking at the 3x4 version. So, it really is still an air sander? Is this correct?

I am thinking of using one for scuff sanding in-between coats during the finishing process. Specifically for flat panel (AKA Shaker style) doors. A round R/O sander cannot get into the square corners on the flat panels, of course. BTW, the cabinet doors that I am sanding are quite large, almost the size of walk doors. Hand-sanding is not working well for me.

I would prefer an electric sander. According to the Surf Prep website, their air sanders would consume a bit more air than I have available. Or, at least the compressor would be running almost constantly.

1/3/17       #8: Surf Prep System ...
Lorraine Member

We use Surf Prep on both solvent and waterbased finishes with great results.
Fine and super fine flat and thicker sponged pads 180 220 is what we found to be most affective in most finishes we do.

1/6/17       #10: Surf Prep System ...
Denny J

Good information on this. I am going to get the surge sander from power process to demo next week.

2/2/17       #11: Surf Prep System ...
Abrasive

"If I understand it correctly, the "electric" version includes an air pump that drives the sander"

That box i think is the electronic speed controller for the brushless motor.

3/5/17       #12: Surf Prep System ...
Adam West  Member

Website: http://www.surfprepsanding.com

The box is a power supply converting 120 vac to 24 vdc for the brushless outer runner motor.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)