Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Bondo type product to fill small miter joints prior to finishing

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Bondo type product to fill small miter joints prior to finishing

8/1/17       
Leslie Desnick Member

We are looking for a filler for maple mitered frames to fill small seams in miters prior to finishing with pre cat primers and top coats with both solvent and waterborne. The key issue is the frames are cured in a PrimeHeat batch tunnel and the miter is sometimes sinking slightly. We think we need a putty that will stretch when going through the heat. Any help would be appreciated.

8/2/17       #2: Bondo type product to fill small mi ...
kevin

have you tried nitrostan glazing putty?

8/2/17       #3: Bondo type product to fill small mi ...
tyler

I have been using 3M Acryl-White Glazing Putty. It fills nicely, you can get it in white, green, red, etc. Dries fast and i've not noticed much in the way of shrinkage.

8/2/17       #4: Bondo type product to fill small mi ...
Adam

Bondo is a polyester resin based filler. It would be the worst choice. It takes a very long time to cure under normal conditions and shrinks considerably. Often people will apply it, wait a few hours for it to harden, sand it, and paint it. It then continues to shrink over the next week, which leads to telegraphing thru the finish. The only way to repair it is another coat of a stable filler and a repaint.

Bondo is a great product for fixing many things. We often get away with it when burying it with house paint. In the shop it works okay if a lump of its left to cure for a few days and then buried under plenty of primer.

I would expect your heating process to shrink the bondo very fast. Its brittle and will crack in the miter.

I would likewise try the 3m Acryl marine putty. It fills much larger defects than nitrostan(pin holes). Its often used on wooden boats which move around. It has almost zero shrinkage due to its high flash off solvent base.

8/2/17       #5: Bondo type product to fill small mi ...
Adam

Which glue are you using in the miters? Anything other than a TB1 glue will shrink.

8/2/17       #6: Bondo type product to fill small mi ...
Les Member

Thanks for your help. I will be trying these products.
I do have one question for Adam:
What is TB1? Is this a product or a type of
putty?

8/3/17       #7: Bondo type product to fill small mi ...
kevin

its glue. TiteBond1

8/3/17       #8: Bondo type product to fill small mi ...
Adam

Leslie,

Please post a closeup pic of the problem. Describe the glue and reinforcing of the miter.

8/6/17       #9: Bondo type product to fill small mi ...
Family Man

I have found that whatever vehicle of solvent I am using for topcoat we use the opposite for filler. Which for us means solvent based finishes and waterbased fillers. Otherwise we get the smallest of reactions if we use the same as you are basically softening the putty and get some telegraphing. For us Elmers interior is the go to putty we use and it is widely available.

8/7/17       #10: Bondo type product to fill small mi ...
Matt

ProH20 water based putty isn't easy to find, but I have found it to be the most useful putty in the shop. It also doesn't shrink much.

Timbermate makes a product very similar that we use if I can't find the ProH20. For some reason the ProH20 seems to hop from vendor to vendor in the quart can sizes. One week I can get it, the other, I can't.

8/7/17       #11: Bondo type product to fill small mi ...
Robert Member

Durham Rock Hard Putty is a water based putty that can be tinted with any water soluble tint. It comes in powder form and it has a good holdout on small type dents as well as gaping gaps. It wont shrink or crack. Sands real nice when dry and can be bought at a Hardware Store for a reasonable price. I highly recommend it.

8/10/17       #12: Bondo type product to fill small mi ...
Hen Bob Member

I 2nd the ProH20 Great product. I get it from Baer.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)