Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: 3M respirator filter for Conversion varnish

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

3M respirator filter for Conversion varnish

8/11/17       
al

What respirator cartridge # and pre -filter do most use when spraying conversion varnish?
Thanks,
Al

8/11/17       #2: 3M respirator filter for Conversion ...
Leo G

3M™ Organic Vapor/Acid Gas Cartridge 6003

8/12/17       #3: 3M respirator filter for Conversion ...
Mastercabman

What Leo said!
Also when not using
put the respirator
in a Ziploc bag or sealed container
Once you open the filters package
They are constantly working

8/12/17       #4: 3M respirator filter for Conversion ...
Bart

Absolutely keep them in a sealed container. Technically the charcoal is good for a few months depending on concentration of fumes. Back in the day making surfboards for a living when I lived in a respirator for hours a day I switched out 2-3X a month. The particulate filter once a month. I hope you're using a full face mask with the CV.

my2cts

8/12/17       #5: 3M respirator filter for Conversion ...
Leo G

Pretty sure a pair of cartridges are good for about 8-10 hours of heavy concentrated use. In the sprayroom with a fan taking a good portion of the fumes away from you they will last longer.

I would think that you should change them at least weekly.

8/12/17       #6: 3M respirator filter for Conversion ...
chris

get yourself a supplied air system.

8/12/17       #7: 3M respirator filter for Conversion ...
al

Chris,
What brand of supplied air system do you have? I am considering one.

8/13/17       #9: 3M respirator filter for Conversion ...
chris

I have a 3m versaflow system
very comfortable. also supplies coool air which is great in summer.
make sure you get a supply air hose which is made for supplied air not just a regular hose.

8/13/17       #10: 3M respirator filter for Conversion ...
Bart

General rule of thumb is 40hrs of usage or one month for most respirators at high concentrations. An hour here and there spraying with a good exhaust system is not to taxing an environment. High humidity can really affect the filter life in a negative way.

my2cts

8/13/17       #11: 3M respirator filter for Conversion ...
Adam

Go to the grocery store and buy one of those newer plastic food containers that have the silicone gaskets. I have one big enough the whole half mask with the filters attached goes in. The plastic bag idea with filters never works out well.

8/14/17       #12: 3M respirator filter for Conversion ...
al

Chris,
Do you have the battery one with filter you put on your belt or air from a compressor
with no filter? I can only find Versaflow with battery setup and not from compressor.

8/14/17       #13: 3M respirator filter for Conversion ...
chris

i have the one hooked up to my compressor
3m versaflo SA-100-PSK.

8/14/17       #14: 3M respirator filter for Conversion ...
al

Ok found it. If using your shop compressor is there a special filter that keeps impurities out
of breathing tube?

8/15/17       #15: 3M respirator filter for Conversion ...
chris

i have 2 filters inline and a water separator.

8/16/17       #16: 3M respirator filter for Conversion ...
DannyB

Note that 3M now has a cartridge with an indicator to tell you when to replace it.
If you aren't going to use supplied air, it's definitely worth it

8/16/17       #17: 3M respirator filter for Conversion ...
al

Info seems to be a little scarce on the supplied air systems. The one Chris uses is I believe called high
pressure system because he is using his shop compressor. I can't find enough info but I think the high pressure system requires quite a bit of cfm to operate it. The low pressure systems use a little compressor just for the breathing apparatus and nothing else. I've been on 3m website and a company called Allegro, Allegro sells complete system with the small compressor while it looks like 3m just sells
the mask, hoses, etc.

8/16/17       #18: 3M respirator filter for Conversion ...
chris

give Northern safety a call at 800 922 8553.
their technical support dept. can help you decide.

8/16/17       #19: 3M respirator filter for Conversion ...
CraigM

I use the Allegro half mask system. The compressor has held up well, but I have had to replace the straps on the mask a few times.

Allegro Safety

8/17/17       #20: 3M respirator filter for Conversion ...
DannyB

For the high pressure systems, you have a couple options.
1. They make portable boxes that provide everything you need. http://www.airsystems.com/index.php/2009-03-24-20-38-35/breather-box

2. You can go with a non-portable filter set.
http://www.airsystems.com/index.php/2009-03-24-20-38-35/air-panels

(these are just examples, 3m makes one, etc).

As someone else said, allegro (and others) make portable breathing pumps. These are just oilless rotary vane pumps from gast with the right set of filters and adapters (but, in my limited experience, you can't really get them cheaper from gast than allegro is selling them :P)

Allegro sells face masks that go with them, but they can also be made compatible with others.

For example, i found the allegro facemask to be a bit annoying. 3m makes a low pressure (and high pressure) breathing adapter for their half and full mask respirators.

http://www.3m.com/3M/en_US/company-us/all-3m-products/~/3M-Dual-Ai
rline-Back-Mounted-Adapter-Kit-SA-2000LP-Low-Pressure-1-EA-Case?N=5002385+3294780
269&rt=rud
(they have front mounted too)

These are attached where the cartridges normally go, in the same way.

I use an allegro pump with 3m masks and am quite happy with this set up.

8/17/17       #21: 3M respirator filter for Conversion ...
Richard

For those that use the Allegro half mask system, or similar how do you deal with the hose?
I always found it to be the weak link of the system, heavy and not very flexible. It makes me feel like I'm on leash.
I would love to find one that allows me to attach it from the ceiling allowing easier movement around the spray room.

8/18/17       #22: 3M respirator filter for Conversion ...
ColorPro Member

I cant stand using full masks tbh, they really get in the way.

I use a binks millennium 3000 with organic vapors cartridges and R95 particulate pre filters.

I use the cartridges till I begin to smell vapor and then change em out...2-3 months. pre filters I change out when they get dirty.

mask is light, comfy and have used em fpr 10 or so years

8/19/17       #23: 3M respirator filter for Conversion ...
DannyB Member

Richard,
You can use any hose you like, you just want to use things that ideally are rated for breathing air. They just give one that is cheap and effective (being rubber) :)

It also depends how much you are willing to spend.
You could easily just run a copper drop to the ceiling and suspend the hose from there.
You can also find plenty of very flexible scuba hose that is rated for breathing you can use (though sadly, miflex no longer does custom lengths).

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)