Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Flat Line vs. Conventional

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Flat Line vs. Conventional

11/21/17       
Family Man

I'm helping a friend here who apparently thinks highly enough of my traditional/conventional finishing knowledge that he wants me to look at flat line systems with him even though I know squat about flat line systems. I don't have four days though to sacrifice to the travel involved so I'm turning to my ace in the hole- you guys, woodwebs finish experts.

Here's my questions:
If cost were not an issue, how would you rate the finish off of a flat line vs. convential? Each aspect- stain, clears, pigments, etc

What were your biggest pitfalls when you made the switch that he should look out for?

Realistically, to do 600 doors a day how many men to run and how much would should he expect to pay for all the equipment involved to do so?

Do you have a particular system you'd recommend? Any he should stay away from? How quickly can recommended system change over to different finish?

And as I've already admitted, I know zip about flatline, what questions did I not ask that I should have asked?

I'm old school, I always worry without being able to touch and see the product as it progresses how are you going to catch the water spot, the glue spot, the areas that didn't take quite right- just dealing with the inconsistencies of wood and all the other craftsmen behind you (that never happens!)...what's your take?

Sincerely appreciate the feedback

11/21/17       #2: Flat Line vs. Conventional ...
keith

purchased falcioni used flat line sprayer about 6 yrs ago. pros are fantistic finish can't compare quality and finish speed to anything I've done in 40 years. need to be using finishes that dry very quickly. we spray precatalyzed lacquers. spray capacity we encounter is 50 cabinet doors 1 coat thru machine approximately 12 minutes. can go faster just requires more employees on exit side of machine to keep up with outflow of doors. definitely a good move to increase profitability if you work the system correctly. took about 6 months to a year to work the system to 90% good results. drying system would be a plus just requires large space for entire system. we can clear seal 50 doors first of the morning turn doors over just before morning break spray front side. sand sealer both side right after lunch spray clear coat on backs of doors by 2 and flip doors , put clear coat on front of doors just 15 minutes before shop shut down, doors ready to install first thing next morning. these times are good for 3/4 of the year based on atmospheric temp. and finish cure times. contact me for more info if needed.

11/21/17       #3: Flat Line vs. Conventional ...
Family Man

Keith,
Having a hard time following your capacity- sounds like 50 doors takes 12 minutes but then it sounds like it takes all day to get a set of doors done...not quite following. Can you expand those thoughts. Thanks-

11/22/17       #4: Flat Line vs. Conventional ...
keith

50 doors thru the machine takes 10 to 12 minutes per pass. give the doors time to cure out turn doors over run front side. give doors time to cure out sand both sides of doors run final clear finish on back of doors. turn doors over at the end of the day run front side. total spray time on a set of doors thru the machine 2 passes on each side comes out to total of about 40 minutes per set of doors.doors cure all night ready to assemble on cabinets next day. this is our procedure with only atmospheric drying in our shop no added drying fans or accessory fans. travel time thru the machine is approx. 8 feet per minute. can spray a 4 x 8 sheet of material with clear finish thru the machine in 1 minute. only thing that limits capacity would be drying rack capacity for all the doors you want to spray. machine capable of spraying 200 or more doors per hour on 1 side

11/22/17       #5: Flat Line vs. Conventional ...
kevin

it takes 12 minutes to run the doors thru one time. one pass on one side.
then that coat has to dry before flipping them over (unless you have an IR drying system or an oven)
the same goes with each coat so you actually are limited only by your dry time.
Similar to your "conventional spraying". It only takes a minute to spray a door. Takes hours to dry.

11/22/17       #6: Flat Line vs. Conventional ...
Family Man

I appreciate the extra feedback. So tell me what I am missing here...I'm a simple minded fellow. Unless you have enough men to keep up with the staining, sanding, feeding and taking off the machine it is not speeding you up. Which to me to staining and the sanding are more time consuming when done right than the laying down of the finish.

Trying to wrap my mind around what you guys are saying. To me this things could INCREASE the amount of men needed because you have to keep up with it but only when it's running.

I will admit my complete ignorance now but I thought these had gotten to the point they applied the stain, sealer, hit a drying point, sanded and topcoated hit a drying point and somebody is catching it at the end. Like I said, I know nothing about these things as I never entertained in a million years it would be the way my shop would go. But my door guy is looking at possibly going this route and while he knows I know nada about them trusts my eye for what the end of each step and final result is.

As you guys explain it to me the only way it would work is if he batched up a complete days worth of clears, all same sheen and ran them (ran the next job while previous one dried). What I struggle with is the pigmented. I just can't see enough batch quantity size to make the pigmented worth the time. Enlighten me.

Thanks again and any input on the financial side about costs, and percentage of cost savings once you hit a certain door # per day would be helpful.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)