Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: MLC Magnamax H2O Precat Water Borne Poly

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

MLC Magnamax H2O Precat Water Borne Poly

4/24/18       
JoeW Member

I have sprayed with waterborne finishes for over 10 years. I currently use MLC Agualente Plus products. My supplier has now started to push the MLC Magnamax H2O Precat Water Borne Poly. I have ordered some to try. Hoping it will provide a much harder surface than the Agualente plus.

Has anyone tried this product yet? It does cost more and I'd like to know what you think of it. Any suggestions on it's application. I spray with a CATech AAA.

5/16/18       #2: MLC Magnamax H2O Precat Water Borne ...
Marc P

My supplier gave me a sample quart to try and I used it yesterday. It looks good, and feels good. It is VERY thin unlike any other waterborne I’ve sprayed before. The PDS says to lay it down at I believe 4-5 wet mills, but I can tell you there is no way you could spray that thick on a vertical surface and not have run or sags.

I sprayed it through a 4 stage hvlp turbine because I just had two shelves to spray. I would like to try it through my AAA with a
4-09 tip though.

5/16/18       #3: MLC Magnamax H2O Precat Water Borne ...
JoeW Member

Thanks Marc, I have received mine , but have not used it yet. Hope to try it today. I'll be using it in my AAA with the 409F tip.

5/30/18       #4: MLC Magnamax H2O Precat Water Borne ...
JoeW Member

I Finally had a chance to spray this on a job. It does lay down great. It feels great. It looks great. And It gives an immediate amber appearance.

But. It is very thin right out of the can. I found on vertical surfaces multiple very thin coats is the way to go. I think like all waterborne products it takes a lot of practice to get used to it. And Patience, Patience, and more Patience.

Will see.

Joe

6/23/18       #5: MLC Magnamax H2O Precat Water Borne ...
SK Member

My MLC rep told me Magnamax H20 was put out in response to complaints that water bornes are crystal clear. It gives the Amber tint that comes with some oil based pre cats or Polyurethanes. Worked well for me.

6/26/18       #6: MLC Magnamax H2O Precat Water Borne ...
Greg Larson Member

Website: http://www.nesaw.com

I just finished a large job with MagnaMax H20 and learned a lot. I used both Aqualente and Sherwin Williams Kem-Acqua for the past 10 years. I love the feel and the look of it. I used to spray a first coat of de-waxed shellac to get the color, but the MagnaMax gives me that color without needing the shellac. I also like the way it scuffs; it powders up perfectly after about 20-30 minutes and doesn't clog the paper like the other products did.

As everyone else mentions, it is super thin. I was using the same 1.3 tip with my CA Technologies CPR gun, but it didn't seem to be atomizing well and a ton of material was coming out no matter what I did with the gun settings. It was getting a bit of orange peel and a lot of bubble pops and nibs. For fun, this morning, I switched to the only smaller tip I had which was 0.8; I was amazed that it even sprayed at all, but because it's so thin, it not only worked, but laid down perfectly. I had to slow down a lot to get enough material, but it worked very well.

I have contacted my rep to see what tip and settings are recommended by CA Technologies and ML Campbell. I had a horrible problem with drips on vertical surfaces with the 1.3 tip, so I'm curious what they recommend. I agree that 4-5 wet mils couldn't possibly hold on vertical surfaces, so several light coats seem to be the ticket.

I'm really happy with the coating so far and am looking forward to figuring it out. Practice, practice, practice, for sure...

6/27/18       #8: MLC Magnamax H2O Precat Water Borne ...
JoeW Member

Greg,
I think your on to something there. I have tried a number of things so far that just do not help the sagging.

I cannot turn my AAA pump fluid down any more and still get it to prime. I already use a 409F tip, which is pretty small.

I'm gonna order a 407F tip and experiment with it.

If I can get the sagging under control, I will be very happy with this product.

9/7/18       #9: MLC Magnamax H2O Precat Water Borne ...
JoeW Member

I have now sprayed 10 Gallons thru my Cat 14:1 AAA. The last seven with a 407F tip.

The 407F made everything much easier. I was able to control the spray in every way. I have found that several thin coats virtually stopped the sagging and runs.

9/8/18       #10: MLC Magnamax H2O Precat Water Borne ...
Chris  Member

Website: srhardwoods.com

what fluid pressure are you set at? and air?

9/9/18       #11: MLC Magnamax H2O Precat Water Borne ...
JoeW Member

Fluid pressure is 350. The air pressure I have found best at 19 to 20.

9/10/18       #12: MLC Magnamax H2O Precat Water Borne ...
Greg Larson Member

Website: http://www.nesaw.com

Hi Joe,

It's great to hear you had success with the smaller tip. I finally did get a 1.0 tip for my gun and it worked great. I still haven't had the opportunity to spray much vertical stuff and I'm a little worried about doing that successfully without runs, but I guess I'll just have to be careful and use multiple light coats.

9/10/18       #13: MLC Magnamax H2O Precat Water Borne ...
JoeW Member

Greg,

I sprayed a lot of drawers, I only had to be extra careful in the corners. Light coats did it for me there.

On locations where gun/ hand control is not so restricted, runs were easily controlled with regular coats.

5/6/19       #14: MLC Magnamax H2O Precat Water Borne ...
banjod Member

This product is amazing in comparison to any other water based products I've tried. It sprays and looks almost identical to current solvent based products.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)