Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Spray gun for Dyes and Toners

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Spray gun for Dyes and Toners

5/14/18       
John Member

Up front, I spray less than 5 gal per month. Much of the work I do involves WB dyes and shellac based toners to color match existing work. Shellac is the only solvent based product I use; all my topcoats are WB.

My current Qualspray gun, which draws around 8 cfm at 29 psi, is pretty versatile but I get some pulsing when spraying dyes and toners and that gives mottled color. I compensate by spraying at least two coats but that does not completely eliminate the non-uniform look. I had similar issues with the low end gravity feed HVLP gun I first used, which makes me wonder if the problem might be in my air line and/or filter or regulators.

I'm interested in what you folks recommend for spraying dyes and toners on furniture and cabinets with the most important characteristic being uniformity. For info., my compressor can handle 11 cfm at 40 psi. What should the piping size be for this flow? Thanks very much.

John

5/14/18       #2: Spray gun for Dyes and Toners ...
John Member

Another piece of info., my compressor, regulated at 90 psi outlet, is about 50 feet from the secondary regulator, and that is typically set at 29 psi. I use a 20 foot 3/8" hose from there to my spray gun.

John

5/14/18       #3: Spray gun for Dyes and Toners ...
mastercabman Member

John
When you say pulsing,is it like spitting?
Or it's spraying a little more or less?
Are you using gravity gun?
Is it set up with PPS cup.
Check your air cap and make sure no holes are clogged up
Also I like to use mini regulator at the gun

5/14/18       #4: Spray gun for Dyes and Toners ...
John Member

A little more, a little less, not spitting. I had this problem first with a low end gravity feed HVLP conversion gun, and now with my mid range gun with a pressurized 3M PPS cup. I first thought it only happened when the internal liner approached empty but I realize now that it happens even when the liner is full.

The air cap is clean. I used a mini regulator on the inlet of the gravity feed gun. The PPS cup on my newer gun has it's pressure regulator at the gun, so I have the gun air regulator 20 ft upstream.

Thanks,

John

5/14/18       #5: Spray gun for Dyes and Toners ...
nick

have you cleaned the fluid passage and nozzle lately (both inside and out)? One dried piece of crud at the tip on the outside or anywhere on the inside of the nozzle can even make a Sata spray like a $50.00 spray gun.
When it comes to spraying dye (SW universal dye thinned with DNA) I use a Devilbiss compact gravity gun with a 1.0.
For WB toners (1 to 1 finish to water) I use the same set-up as the dye.
For solvent based toners (1 to 1 finish to butyl acetate); I use a Sata 2000B with a 1.4 but I crank in the needle until the fluid volume is where I want it. For spraying toner I'm looking for the a gun with fine atomization and even particle distribution and then spray it at the lowest air pressure where the gun can maintain those attributes especially if the piece has any depth or profiles.

5/16/18       #6: Spray gun for Dyes and Toners ...
Herb johnnson

Buy an Iwata gun with the tulip tip stain will look like a spray and wipe not cheap but worth the money

Good luck herb j

5/16/18       #7: Spray gun for Dyes and Toners ...
John Member

Thanks for the feedback, all. I'm doing a complete soak and cleanout on the gun. I don't see anything in it, but I'll know it's clean when I'm done and if the problem continues then I'll know it's with the air delivery system. I'm suspecting the problem might be with my step down regulator, 20 feet before the gun. I had a similar problem with the last regulator when it developed a leak. This one seems fine, but the problem is back, so ....

I will look into the guns you all recommended, too. I start to choke when it goes North of $500, considering I used to get pretty darned good results with a $20 throw away gun, but I'm willing to spend the money if the results justify it. Anyone use a CA Tech. FE Line HVLP gun? Their literature says it's made specifically for dyes and toners.

John

5/16/18       #8: Spray gun for Dyes and Toners ...
John Member

As I was disassembling the gun more fully to soak it this morning I found the packing nut behind the trigger was completely loose. I think I've found the source of the problem.

The gun was pretty clean inside when I looked inside it after disassembly. It's really clean now.

John

5/16/18       #9: Spray gun for Dyes and Toners ...
mastercabman Member

John
Hopefully that was the problem
If something is loose it could bring air into the nozzle and can make it pulsing as you described
As for the FE LCFM spray gun
You can spray all kind of coating
You just need to get whatever size nozzle/needle for the task
I have one and sprays very nice
Also it runs on low CFM

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)