Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Western Red Cedar Solvent Soluble Extractives??

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Western Red Cedar Solvent Soluble Extractives??

10/26/18       
John L Member

I’m having a bit of difficulty finishing exterior WRC. The house is 4 years old and is being stripped and repainted for the third time now due to blistering paint. Exterior construction materials include mixed species, the vertical siding being clear vertical grain WRC, and the facia and soffits being clear vertical grain WRC as well. The window and doors are FEQ genuine mahogany, and the balance of exterior trim/millwork is Sapele. All the above were painted according to architectural specifications which included an oil primer and two finish coats of B&M Aura exterior low luster paint. The color is Kendall Charcoal, being very dark, with a light reflectance value of 13. The surfaces get extremely hot in direct sunlight due to the dark color. The paint is fine on both the Sapele & Mahogany, but is blistering on the cedar, and only on the south elevations. The cedar was primed all sides, as well as every end-grain cut being primed during assembly. I took numerous moisture content readings and none are greater than 6% so I’ve ruled out moisture. The blistering is isolated to individual boards, the blisters occurring across the entire lengths and widths of boards. 10% -20% of the boards are experiencing finish failure. Being that the blistering is isolated to individual boards I’m ruling out solvent blisters as well. Where one board failed, the adjoining board is fine. The primer is releasing from the cedar only when top coated, or on locations where a second coat of primer is necessary. Both wet and dry film thickness are spot on to manufacturer’s specs. There is no visible evidence of moisture or solvent within the blisters, however, what I did notice was a sticky pitch or sap-like residue beneath the blisters. This substance appears to be exuding through the oil based primer, actually causing the primer to darken and turn gummy. The exuding substance doesn’t have any dimension to it, and is more like a sticky film. I’ve included a picture to illustrate, the arrow in the photo illustrates a bleeding board and the effect it has on the color of the primer after being intercoat sanded, and ready for finish. I’ve also included a photo of the stripped siding, thinking the coloring of the cedar was a bit odd, many of the boards having the appearance of being sapwood, but at 4” wide/vertical grain, I don’t think sapwood rarely exceeds 45mm. I’m suspecting that the cedar is immature new growth. Finish failure is occurring randomly without any correlation to a particular board color. Are there essential oils, sap, or pitch in newer or quick growth cedar that could be volatizing due to the heat and solvent based primer? The cedar was stripped mechanically and orbital sanded to #120 to provide plenty of tooth. It was then vacuumed and wiped down with acetone. No boards were left exposed to the elements and were primed within hours after initial stripping. There was no visible evidence of an extractive of sorts before priming. I’m hoping someone here might be able to share some knowledge as to the chemical properties of Western Red Cedar that might be causing this, and provide a possible solution rather that a tear-off/re-side and re-trim which the client is willing to do as a last resort. A breathable finish such as an acrylic semi-solid stain is not an option due to the variegation in color of the boards.
The primers used on all three re-paints were B&M 100, 094, and 366. The 366 is the same as 094, yet comes in a deep base to allow it to be tinted to the finish color without compromising the performance of the primer. All primers were tinted to the finish color.
I’m really at a loss on this!


View higher quality, full size image (750 X 1334)


View higher quality, full size image (4032 X 3024)

10/26/18       #2: Western Red Cedar Solvent Soluble E ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

This is a good one for Gene Wengert to look at. He is the guru of wood knowledge.
Also he has a forum here on Woodweb.
I believe it is under Kiln Drying

10/27/18       #3: Western Red Cedar Solvent Soluble E ...
Steven

If the blistering is due to sap bleed through you could try spot priming with BIN shellac based primer to seal it in.

10/27/18       #4: Western Red Cedar Solvent Soluble E ...
Gene Wengert-WoodDoc

In your case, without being there, I can only guess, but I think I know the answer. When an old growth tree is growing, there is an anaerobic bacteria that often gets into the tree. It is in small compartments running vertically in the tree and in the bottom log. While alive, it creates fatty acids that turn rancid with time. Did you or the homeowner mention any funny smell? The bacteria also create some slime that tends to plug the moisture movement. The bacteria also somehow create very high moistures in the tree, as they are anaerobic. Finally, the bacteria create enzymes like pectinase that destroy some of the wood’s strength. I have seen discoloration in plastic overlaid molding...it comes through the plastic. The infected area is sometimes called wetwood or sinker stock. It often has a darker color.

10/27/18       #5: Western Red Cedar Solvent Soluble E ...
John L Member

Thanks for the responses. Doctor Gene I think nailed it. After initially posting this I noticed making an error, the boards appear to be old/slow growth, not new growth. I needed to correct myself after counting growth rings. The prior painter appeared to have masked off problematic boards, coating them with Bin, but they still popped. I did notice the ring separation on the right board and the dark vertical streaks on others which are indicative of bacterial wetwood. The fatty acids would account for the solvent soluble bleed, fatty acids being an oil. Thinking the mineral spirts and heat activated the slime. That would also account for the primer turning gummy and not drying for weeks. It all makes sense now. Thanks again.

10/30/18       #6: Western Red Cedar Solvent Soluble E ...
robert johnston

FWIW: I was told that 'Bin' shellac is not to be used on any exterior wood product. Correct me if I am wrong. I did try using it to fix a chronic 'sap' problem on a painted pine exterior door, and it always came back within one season.....oozing all the time.

Each year, for 5 years I painted that door!

I think you have to replace the board!

10/30/18       #7: Western Red Cedar Solvent Soluble E ...
Adam

I wrote this on one of the other threads last week. BIN is an exterior spot primer. What area a spot covers I have no idea.

Shellac used to be used as a glue on wooden boats. BIN is rated as a spot exterior primer. I primed some cedar flower boxes I built inside and out. They were on my own house for about 5 years full of flowers. dirt and water. My wife was supposed to topcoat, but never got around to it(how surprising). Zero peeling inside or out. BIN is an excellent product. I honestly do not know of another product that would have performed in those extreme conditions. I did it when I had no time and little kids. Interesting accidental experiment.

10/30/18       #8: Western Red Cedar Solvent Soluble E ...
Gene Wengert-WoodDoc

The bleeding or oozing of sap or pitch in pine is a different issue than the WRC issue. The pitch is made up of many different chemicals, some of which are liquid at room temperature. When drying pine, it is recommended that the wood be heated 160 to 180 F. This evaporates the chemicals that are liquid at 100 F or cooler The sap left in the wood can be softened with heat or rarely some chemicals in finishes. Every piece of pine and most other softwoods like WRC have a potential sap issue so needs to be heat treated., which is common in kiln drying indeed,

The bacterial issues I mentioned in an earlier post are a totally different. Hemical. are not too common, and. Annoy be stopped with heat or various chemical coatings. I have seen the bzcterial chemicals also move through plastic overlays. I have seen it move through gymnasium flooring finishes. The foul odor is not fixable with a finish but requires total replacement. Be happy that few of you have encountered the bacterial issue, as such wood almost always has shake and would be eliminated in processing.

10/30/18       #9: Western Red Cedar Solvent Soluble E ...
Gene Wengert-WoodDoc

Correction:
The bleeding or oozing of sap or pitch in pine is a different issue than the WRC issue. The pitch is made up of many different chemicals, some of which are liquid at room temperature. When drying pine, it is recommended that the wood be heated 160 to 180 F. This evaporates the chemicals that are liquid at 100 F or cooler The sap left in the wood after het treating can be softened with heat (including heat from sanding or a finishing oven) or rarely by some chemicals in finishes. Every piece of pine and most other softwoods like WRC have a potential sap issue so needs to be heat treated., which is common in kiln drying indeed,

The bacterial issues I mentioned above in this post are caused by a totally different. chemical. are not too common, and. cannot be stopped with heat or various chemical coatings. I have even seen the bacterial chemicals also move through plastic overlays. I have seen them move through gymnasium flooring finishes. The foul odor is not fixable with a finish but requires total replacement. Be happy that few of you have encountered the bacterial issue. Most bacterial infected wood almost always has shake and would be eliminated in processing.

10/31/18       #10: Western Red Cedar Solvent Soluble E ...
John L

Correction:
I incorrectly stated that fatty acids are oils, which they aren’t. My conclusion that the solvent in the primer was activating the bleed is likely questionable. What I’ve gathered, as Gene mentioned, the fatty acids plug up the water transport system in isolated regions of the tree, some being pencil thin, and moisture is trapped under extreme pressure which many times won’t escape during the kiln drying process. When checking moisture contents as I did, there is a strong likelihood that unless I probed those exact locations where pockets of moisture were trapped, that I might be getting low readings. I noticed that many of the problematic boards have a bright yellow to orange discoloration. The staining of the primer starts as a small dark wet looking spot, and just keeps growing, turning entire board faces dark and gummy. I’ve never seen this condition before.
I’ve been seeing a lot of white oak sourced from wetwood infested trees, with flooring and veneers blowing apart during processing and finishing, including ring separation across entire rift-sawn veneers.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)