Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: RE: Lacquer Finishes & Alternatives

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

RE: Lacquer Finishes & Alternatives

11/23/19       
Tommy

For hardwood cabinets or table tops, is lacquer considered the best of the finishes?

Or, are there other easier finishes that will produce the same end result looking highly professional as well?

11/23/19       #2: RE: Lacquer Finishes & Alternat ...
Adam

We are in the year 2019. Straight laquer was replaced by precatalyzed laquer back in the early 2000’s(?) Then conversion varnish(CV) took over in the late 2000’s(?). 2 part Urethane has always been a speciality product until 2010(?) they reformulated the toxicity, so some people use it almost exclusively.

I wrote that in order of increasing cost, durability, chemical resistance. Lacquer is at the bottom. Not a good finish for a tabletop.

11/23/19       #3: RE: Lacquer Finishes & Alternat ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

Lacquer still does have its place in the finishing world as well as do all the other cross-linked or 2k products.
We do custom finishing and refinishing. Nitro has its place in the antique refinishing world.
Also lots of the very hi end home furnishings have nitro on them.
Many of the musical instrument manufacturers use it along with several big name piano manufacturers.
Pre-cats and Post-cats have their place also along with Conversion Varnish. It just depends on the performance you need for your finishing application.
We also use lots of 2k Urethanes and also Polyester when needed.
So is Nitro dead? Not at all. Just make sure it is the right coating for your application.
As for table tops I like 2k urethanes for the flexibility and durability. Cabinets I also tend to lean towards 2k urethanes as I need a non yellowing coating most of the time.

11/23/19       #4: RE: Lacquer Finishes & Alternat ...
rich c.

I'd really question that high end furniture has straight lacquer on it. Unless we are talking about the imported furniture from Viet Nam. If it's sprayed in North America, water based is climbing the charts very quickly. Lacquer is a very poor choice for kitchen cabinets and table tops, and not the greatest water resistance either. It has a very low chemical and heat resistance. I was spraying gallons of ML Campbells precat in the late 1990s. I have cold checked dining room chairs and water damaged kitchen cabinets in my home to prove it. I've never been quick to work on my own home. Finally remodeled the original 1957 bathroom! Still not completed though.

11/24/19       #5: RE: Lacquer Finishes & Alternat ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

We do lots of touch up on many hi end brands of furniture and yes we see lots of NC. Yes some are switching to water, but those finishes are easy to spot.
Yes, believe it or not lacquer is still used.
On a kitchen? never.
I love to hear about all that checked precat. We see tons of it. Most of it is not from cold checking. It is from poor flexibility of the dry film that can not move with the wood. Same thing with CV. Some of it just gets to brittle.
Yes imported stuff does have NC on it but lots of those factories also use hi tech finishing systems. I know as I spent plenty of time in Vietnam consulting at these factories.

11/24/19       #6: RE: Lacquer Finishes & Alternat ...
Daniel Berlin

FWIW: Most musical instrument manufacturers have moved on to 2k urethane (for non-vintage instruments).

Smaller ones still use lacquer for sure, but the larger ones do not.

11/29/19       #7: RE: Lacquer Finishes & Alternat ...
dan shaf Member

The furniture industry, names like Hooker, Ethan Allan, Baker, Century, Thomasville, Henredon, etc., still use lacquer. Pianos are still being done with lacquer, and though Steinway has moved to polyester, a lacquer hand-rubbed finish is still available from them, same with Mason & Hamlin.

Currently, I do my OEM lacquer finishing using ML Campbell's DesignRClassic Furniture Lacquer. It has great flow out. It's harder and more durable than Sherwin-Williams NC lacquer. It has a silky-smooth feel and tactile properties are always important. If I'm doing a Steinway, I prefer to use the same NC lacquer that Steinway uses, sort of. Steinway uses a hot spray lacquer. The lacquer mfg will make it for me in a regualr-spray format, and they will also formulate it to be less soft and more scratch resistant than its usual mix.

11/30/19       #8: RE: Lacquer Finishes & Alternat ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

dan shaf, We have a custom made NC. We worked over a year with the manufacturer to get the formula just right.
Like you said, flow, feel and hardness or flexibility is everything.
We ran many tests on it to get the best performance possible.
Also many other little tweaks that the long time experienced finisher would want in a product.
Need the same Polyester Steinway uses? I can get that for you. :-)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)