Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: brand of caulking

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

brand of caulking

11/26/19       
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

looking for opinions for the best brand of caulking when caulking the center panel of doors to the stiles and rails. Ive been using the fast dry version DAP, just wondering if theres something more awesome

11/26/19       #2: brand of caulking ...
Leo G Member

Bolt White Lightning.

For door panels I like to get the toothpaste type tube. I use my edge sander to make the tip a pointed 90º angle and as small as I can, usually a 1/32" hole. I use a pc of hanging wire to keep the hole clean. It's a little stiffer than DAP and I use a toothpaste tube key to get it out of the tube. A tube will do a couple hundred doors because of the small hole.

Bolt Caulk

11/27/19       #3: brand of caulking ...
Bart

I use Vista Paints brand of latex acrylic 25yr caulking. It's less than $2 a tube in a box. I let it dry overnight ALWAYS. The only time I had problem with caulk popping was when I caulked and shot finish over it in the same day. I use the fast dry for cabinet joints or a one off door here and there. But I'm very leary of putting finish over caulk that isn't bone dry.

11/27/19       #4: brand of caulking ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

Thanks guys. Ive recently noiced a few hairline cracks on a couple of jobs, and Im thinking that ive just been pushing the dry times way too much. I was caulking and priming in the same day, then letting all that sit over night before sanding and topcoating. Ive heard some guys say they put the caulk between primer coats. Ive always caulked before priming and it seemed to be ok... I think either way I need to go back to letting the caulk dry over night before I coat over it.

Heres my basic schedule

caulk(dap quick dry)
prime(chemcraft aquaprime)
sand
prime
sand
topcoat(General Finishes Enduro White Poly)

11/27/19       #5: brand of caulking ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

I should also add that the cracks are not showing up immediately. In this particular instance the paint job is about 5 months old.
AND the doors that have this issue were facing afternoon sun(large windows across the room with no treatments) in a house that has yet to be lived in (climate controlled) Te doors are poplar with mdf raised panel

11/27/19       #6: brand of caulking ...
Bart

My schedule:
Prime with Zinnser bin shellac tinted gray so I can see the caulking.
sand-caulk, let sit overnight.
quick sand the raised MDF grain from wiping the caulk with wet rag.
prime the front of the door again with bin shellac.
sand
prime with General Finish white undercoat cut 60-40 with whatever GF white or off white poly I have sitting around.
sand
two topcoats of tinted GF white poly.
Total of 5 coats on the fronts and 3 on the backs.
Lots of work but they come out really plush.

We use Alder frames with mdf panels which can vary in quality quite a bit from Decorative Specialties door MFG. We quit using poplar years ago because of movement issues/cracking.

11/28/19       #7: brand of caulking ...
mastercabman

Personally I never understood why would someone caulk the center panel to the rails and stiles
Every cabinet manufacturer that I know does not do it
Beside the panel needs to move freely
Probably why some of you get hairline cracks

11/28/19       #8: brand of caulking ...
Bart

The reason mastercabman is because if I don't I get spider webs between the panel and the stile/rails. Not a good look to have a clean gap in the middle of the door/drawer and then spider webs leading to a finish sealed look in the corners. It would be nice if the MFG didn't have such a tight gap between the panel and stile/rails. And now my main clients want the caulked look. Trust me I would love not to do it.

Happy Tanxsgiving

11/28/19       #9: brand of caulking ...
Adam

We glue our mdf/plywood panels into the stiles and rails. No cracks.

11/28/19       #10: brand of caulking ...
mastercabman

Bart
Sorry if this is a dumb question but what is
Spider web?

And happy Thanksgiving

11/28/19       #11: brand of caulking ...
Jonathan Mahnken

I, like Bart, caulk in order to prevent the paint bridging between the panel and the rail. Yes you can skate by doing thin coats ect..., but what if you get one a little thick, or you have to do a respray? I see how you can do this with solvent based products, but with waterbased I see this being problematic. Those building their own doors I guess are glueing instead of caulking, but the act is similar in theory?

11/28/19       #12: brand of caulking ...
Dv Member

As a painter, we do not know how the doors are constructed so we do not know when panels are glued in place. I will say that jobs with solid solvent lacquer finishes always seem to crack over caulk eventually on house trim. And, most solid color cabinet doors or room crack if caulked. When we paint cabinet doors, we keep that panel to rail/stile open and open it up between coats if needed. It seems to only look good in the short term, caulk often pulls from these areas even if the finish doesn’t not crack. Not saying it can’t be done, but it rarely looks good at least on all wood doors.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)