Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: How hard/resistant should precat be?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

How hard/resistant should precat be?

11/21/19       
Pascal Member

Hello

I know my question may be hard to answer but I will try my best to describe it how I test hardness/resistance

My product of comparison is a floor polyurethane varnish (non catalysed, hardware store type). Now even if the look may have been "ok" the resistance was phenomenal! To scratch to the finish bare wood I would need a penny and press real hard. I suppose this is what you would expect for a floor polyurethane

I have now switched to a precat lacquer(duracoat precat from mohawk). I knew it would be less scratch resistant that poly but I am confused as to whether is supposed to be THAT MUCH less resistant.

I first tried self sealing (all products are from mohawk) :

-dye
-precat Washcoat (5% solid)
-pigment stain
-precat sealcoat (5%)
-Full coat (18% not reduced)
-Grain filler
-Sand 320-600 to get smooth)
- Precat coat (10-12% solid)

this has left me a fantastic look but a light scratch with my nail(without denting the wood) would remove all the finish up to the dye/first washcoat easily. Some people have pointed to me that the pigment stain could be the problem as self sealing on natural has given me better result.

So I decided to go with the recommended vinyl sealer :

-dye
-Vinyl 5%
-sand
-Pigment stain
-Unreduced vinyl coat (17-18%)
-Grain Filler

(Havent completed the next steps but they will go as follow)

-Sand
-Vinyl sealer(tinted or not)
-Precat coat ( 18%)

Up to the grain filler step I got a big improvement on resistance. In order to lift the vinyl sealer I must scratch to the point where I dent the wood and if the wood is too hard then I won't be able to lift the vinyl without scratching a lot. I estimate I must use about 100% more pressure to damage the vinyl. I am now waiting for the grain filler to dry (oïl) before applying the lacquer coats. I went ''by the book" using the recommended products on the tech sheets.

For those who have experience with precat "how" would you describe it's resistance/hardness. Whats considered acceptable. How can I stain wood if finish can't stick to it. Does mineral spirits/solvent from grain filler damage the vinyl?

11/21/19       #2: How hard/resistant should precat be ...
Daniel Berlin

This is standardized as taber abrasion.

see https://www.taberindustries.com/taber-rotary-abraser

It's not always published but all the manufacturers test it and should know it.

The short answer is: Pre-cat is usually pretty horrible, even after final cure time (IE 30 days).

This is compared to what you compare it to - polyurethane.
It's not even a close contest.

(post-cat CV/etc is much better)

This isn't me being judgey - only you can decide where the tradeoff is for your customers.

But pre-cat is very much meant as a time/cost saver, not as an ideal finish.

11/21/19       #3: How hard/resistant should precat be ...
pascal stgelais

thanks a lot daniel.

I think this answer my question very well fortunatly my work is mostly decorative light use furniture. up to now the resistance I have is as you describe not horrible but not fantastic either. for decorwtive woodworking it fits the bill.

But Ill probable switch to CV if I ever need to do a heavy duty furniture(i.e. customers with kids :))

11/22/19       #4: How hard/resistant should precat be ...
Pat

Did you try your finish schedule without the pigment stain? You don't say if it's oil-based, but if it is, it's a likely culprit. Oil-based stains require days to dry fully and the problem is worsened if you don't wipe it off aggressively.

Cheers,
Pat

11/22/19       #5: How hard/resistant should precat be ...
Pascal Member

Thanks Pat

The stain is Indeed Something I will try. I use mohawk wiping stain which is supposed to be ready to top coat after 30min but I suppose this is in summer heat

I also Apply it after a washcoat to minimize blotching but I have limited experience with them. Is it how pros usually do it? Do I need to Apply it to bare wood (over the dye)? Should I scuff sand it to remove the binder and help the vinyl sealer stick to the wood/wascoat?

UPDATE ALSO:

So I have completed the test pieces. THe grain filler has cured and put on another full coat of vinyl sealer than full coat of precat. It's been now 24+ hours and the pieces seems to have become more fragile (same as selfsealing precat) but some spots are more resistant than others wich raises the Following question:

-Have I applied too thick of a finish (Vinyl washcoat + vinyl full coat + grain fille + vinyl full coat + lacquer full coat + sometimes even toners)? I Don't have specialized equipement to measure but since it seems the more coats I Added the more fragile it became maybe I applied the finish too thick (4-5 tho is damn thin if you look at a feeler gauge and it's easy to go overboard). I know about the crazing and all but could this be an early symptom?

- Have I recoated too soon or too late? My vinyl spec sheets ask for a 45min dry time than scuff sand but isn't catalysed and mention no recoat window. I may wait a few hours to a full 48h depending on my Schedule. Since It need sanding I also assume that sealers don't "burn in".

My bets are on the finish being too thick. I have a test piece wich I did not liked the color so ended up stopping spraying after only 1 vinyl coat and guess what...they were damn hard to scratch

11/22/19       #6: How hard/resistant should precat be ...
Daniel Berlin

To tack on to what i said earlier:
I think what you are describing is worse than the pre-cat should be, but it's not gonna be amazing, and it will have issues like you are facing in schedules.

Scratching is a resistance issue, but it could also be adhesion.

If you want to know if you have adhesion issues, do cross-hatch testing of various schedules and thicknesses.

That will give you a clear and concrete answer as to whether it's adhesion or fragileness or something else, and is easy to do with tape and a box cutter ;)

11/22/19       #7: How hard/resistant should precat be ...
Pascal Member

Thanks for your answer Daniel,

Remade 2 test pieces from ash. Since the wiping stain (or the stain being over a washcoat) is likely the culprit I will try 2 Schedule.

-Both will have a black dye stain (wich is in fact really dark redish)

I stained directly over the Dye on the first one. Blotched a bit but the also hid the red tint of the dye quite well. Hope it did note lift too much of the dye (acetone based)

The second one was stained after a washcoat. It was very uniform but kept a black redish tint (will need a green toner).

Althout this wiping stain is supposed to be ready to topcoat in 30min (well according to the spec sheet) i will give it 72h to dry.

as of now the only difference I see is that the stain over the wascoat still ooze oil from ash pores and the smell scream mineral spirits. As for the stain on bare wood the smell is already almost gone.

Although is is not specified in the spec sheets I suspected the 30min dry time may be for an application over bare closed pore wood.

Anyway I will take these at home for 72h and continue the Schedule. If the wiping stain did not cure over the washcoat after that I gess I will have to trade a bit of blotchiness for a more durable finish.

11/22/19       #8: How hard/resistant should precat be ...
rich c.

You must stay in the manufacturers specification for film thickness. It's as simple as getting a wet film thickness "comb". Less than $2.

11/23/19       #9: How hard/resistant should precat be ...
Adam

Your comparison is not really fair. You used a floor poly. Designed to be tough. It can be put on pretty thick. It’s a durable(soft) finish. You are comparing it to a thin film hard(brittle) cabinet finish. Not really apples to apples.

You’ve compounded the issue by putting down various other products under it. The one thing that stood out was your sanding schedule. It should be 240grit after grain filler. 320 between topcoats. If you are looking for max durability you would do 3 topcoats. 600grit is a no go with solvent based products.

11/23/19       #10: How hard/resistant should precat be ...
Pascal Member

Adam you pointed Something I may have overlooked. I come from a waterbased finish background and, unfortunatly, had to learn all by myself.

My reasonning behind using such high grit was to prevent sanding trought the top coat and since lacquer burn in it would not cause trouble. Right know I Don't think intercoat adhesion is my problem since the finish seems to lift up to the wiping stain but I will try using no higher than 320 on my last 2 samples in order to maxime adhesion.

As for the comparison yeah I know it's a bit unfair. I knew lacquer wood be less resitant but I was a bit skeptical that it would be that much fragile. I mean I can lift it after a week using only a finger nail.

I had sprayed regular nitro on a decorative box (bare wood) a year ago (first time) and in my memory, the regular nitro, although less resistant than poly, still needed a bit of effort to lift from the wood. As it is know, I can wash my pieces with water without problem but using a penny I can remove the finish just like a lottery ticket.

11/24/19       #11: How hard/resistant should precat be ...
Adam

Typical sanding:
150 bare wood
240 primer/sealer
320 between topcoats

You can see 240 scratches in white paint and clear topcoats. 320 is invisible. No reason to go higher because you will potentially lose adhesion.

You should ask your rep if their precat actually has burnin. That’s an old school laquer thing. The reality is you are sanding to remove defects, dust, runs between coats not simply for adhesion.

12/8/19       #12: How hard/resistant should precat be ...
Greg Aanes  Member

Website: gregaanesfurniture.com

we started using milesi 2k poly on tabletops and found it so nice to use we put it on everything now, no mo lacquer. it doubled our Finishing material costs but saves work, improves throughput and best of all the shop is happier, less headache. we thin it more than recommended because we don't want a built up look but that takes some of its strength away.

1/11/20       #13: How hard/resistant should precat be ...
Pascal Member

resurecting and old thread but to help other I think have solved my problem.

After dozen of test pieces I have figured that I was spraying my coats too dry and also too thin. I got a wet coat gauge (man it's hard to mesure a non colored finish!) and found out that I was spraying coats that were barely 1mil thick whereas the manufacturer recommand 3-4mil thick coats.They seemed wet in look but hazed in about 30 sec whereas now they dry in about 5-10 min to the touch like the pds sheet states.

I also switched to a "post-cat" (not your typical post-cat since you add the catalyser to the whole gallon which last for 6 month) lacquer (mohawk versalac) wich is supposed to be more durable than a precat.

Although I know It won't beat CV or the brushing floor poly I was used to, I am really satisfied since I use it for decorative furnitures that won't see a lot of abuse.

Hope This can help anyone reading the thread

2/19/22       #14: How hard/resistant should precat be ...
Mark Rogan

You’ve compounded the issue by putting down various other products under it. The one thing that stood out was your sanding schedule.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!