Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Painted Cabinets

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Painted Cabinets

2/7/20       
scott brady

Met with customer about painted finish, we typically spray conversion varnish. She did not like the smooth feeling and said it looked to plasticly. Showed me some doors from another cabinet she had that was definitely finished with a brush, very light strokes. I talked to a painter friend that said in the old days they would brush oil, but latex was to much trouble.

Any suggestions to achieve this finish? Thanks

2/7/20       #2: Painted Cabinets ...
Leo G Member

Spray painting won't look like brushed.

Best you might be able to do is to spray your primer with lots of retarder and brush it to get the brush marks.

Then sand it with scotchbrite or other woven abrasive and then spray your finish. It's still going to feel smooth but you might get the brush marks showing through.

2/8/20       #3: Painted Cabinets ...
Eddie

We offer a finish with brush strokes (haven't done one in awhile), we prime with Clawlock, than spray Satin Impervo following with brush strokes, it takes time to brush and dry but we up charge for such a service.

2/8/20       #4: Painted Cabinets ...
mastercabman

Personally I think brushed painted cabinets looks cheap
But sometimes clients like to do an accent piece of furniture or maybe the island in the kitchen
I did such a job like that back in 2012
The perimeter cabinets were one color and the island another with brush strokes
I didn't finished the cabinets just installed
But I do know they used post cat finishing products to get the look and feel
I can try to touch base with the manufacturer and see if I can get the info on how they did it

2/8/20       #5: Painted Cabinets ...
Bart

I like what Leo is saying. General Finish has a WB brushable pigmented finish. You could brush the GF either on raw wood or the 2nd coat then topped with GF's pigmented Enduro line. Or you could possibly use GF's brushable clear line in the same manner to get the right look.
Charge em whatever you do because it won't be fun.

my2cts

2/8/20       #6: Painted Cabinets ...
dan shaf Member

We do some serious high end houses, the kind that you see in movies. Painted finishes are in, like it or not as finishers. I hate it.

The wood is sanded to 120 grit using a random orbit sander, peel and stick no vacuum holes pad. We feel that hook & loop is more like using a cushioned abrasive instead of like block sanding. MDF is sanded to 320, and I mean sanded, to the point where it's almost burnished. If the mdf soaks up the primer then it hasn't been sanded to our standards. A bad primer coat telegraphs through the topcoat. A poorly prepped substrate also telegraphs through the topcoat.
We do latex. We lay down a coat of oil based primer, thinned 25% with naphtha.

The primed surfaces are sanded with 320 grit, also random orbit sanders, peel & stick discs, usually 3M yellow bond (U-216?).

Then we lay down a latex topcoat, usually Benjamin Moore Satin Impervo, thinned 10% with water. For both oil base and the latex we use CAS (not HVLP, not LVLP, CAS = Conventional Air Supply). guns with 1.4mm fluid tips/needles. We boxcoat when possible, or do wet on almost-wet topcoats.

Then there's a 2nd topcoat. If it's going to be brushed on, that's done on site after installations by regular painting crews. They will scuff our sprayed latex with 320 or 400, either block sanding or ROS or both and brush on their topcoats, the same stuff that we sprayed in the shop.

If the spec is for a delivered latex, we do both topcoats in the shop, everything is sprayed. The first topcoat is scuffed with 3M's 600 grit wet/dry sandpaper by hand. The sandpaper clogs easily, but that's what we use because of the quality of the scratch pattern. The latex looks just like any other satin film-forming finish, minus any decent durability, of course.

We DON'T do latex over Clawlock to my objections. Our other finisher feels that the latex will peel, eventually. True or not, for sure, the best adhesion of the latex is over the oil based primer and because of our unique client base, we err on the4 side of caution as well as finish mythology (my opinion, not the other finisher's opinion).

We have a long and established track record for what we do and for whom we do it. These customers tell us their wants, what they want to pay for. We oblige.

We don't reinvent the wheel, even going back to using regular spray guns.

2/8/20       #7: Painted Cabinets ...
dan shaf Member

Regarding brushing a catalyzed or post catalyzed coating, you can do that, meaning it's possible, but here is a reason that you would not want to do that:

Wet and dry mil thicknesses, especially the dry mil thickness of a brush stroke. That thickness will likely exceed the 4-5 dry mils of thickness that is the tolerance level for many of the solvent based coatings that we use. Never mind durablity - a painted finish has no durability to begin with - but performance is different than durability. Performance of a coating relates to the way that the film survives as an intact film. Will it shatter or fracture? Will it lose adherence? It could. Likely? Probably not. Most likely not. I've done it, brushed on a post-cat, thick like pudding. Ok, not that thick, but you get my point.

My philosophy is that your customer askede for something that's currently popular in high end homes. Sell them what they want, not a facimile of what they want. A redhead dopesn't go to the hairdresser asking for a specific hairdo only to have the hairdresser bullying them to becoming a brunette.

2/9/20       #8: Painted Cabinets ...
Nick

Hollandlac from Fine Paints of Europe.
Very spendy but a top quality oil based brushing enamel. I've used it a number of times for exactly the purpose you describe and it worked perfectly. I always charge time and material for this work as it will take days to finish what you could do in hours with a spray gun and a fast dry finish. Your biggest problem might be finding a experienced brush man who knows use oil enamel.

2/9/20       #9: Painted Cabinets ...
Jim Clark  Member

I have brushed on automotive urethane
with great results.
that gives a good 2K durability finish.
You can even use a auto 2K urethane
primer beneath it when needing build.
It sands so nice and fills everything to
give a really flat surface.

2/9/20       #10: Painted Cabinets ...
mastercabman

Dan shaf

Spraying latex with conventional spray gun with a 1.4 tip and only thing with 10% water?

WOW! That's impressive!

2/9/20       #11: Painted Cabinets ...
mastercabman

Dan shaf

Spraying latex with conventional spray gun with a 1.4 tip and only thing with 10% water?
And getting good results?
WOW! That's impressive!

2/9/20       #12: Painted Cabinets ...
dan shaf Member

Water goes a long way to depress a thivk paint. What's my viscosity after adding 10% water? It's still thick. The fan pattern is still small, maybe 4" - 5". If you thin it more than that then you don't get the paint to cover and you risk serious drips, sags, & curtaining of the paint on any surface that's not flat. We spray so that the wet mil thickness is about 3 - 4 wet mils.

Latex wants to set up quickly. Spraying frames (rails & stiles) can sometimes be a challenge.

We aren't adverse to satinizing the finish after, a very light rub with Scotch-Brite. We don't hand rub brushed surfaces. No need. Brush strokes have texture.

Where or how did the brush stroke look enter the market to capture the eye of the designers and the customers? Most likely it's the shows from Public TV and maybe HGTV that influenced and corrupted/changed the culture of how to look at a finished cabinet.

2/9/20       #13: Painted Cabinets ...
Jim Clark  Member

If you're going to spray latex paint you really
need an airless sprayer.
That's what it's made for.

2/10/20       #14: Painted Cabinets ...
John Member

Dan, you might try BM's Extender instead of or as a portion of the water you are adding. 3% water plus 3% extender will cut the viscosity of BM Advance from 500 seconds #4 Ford cup to less than 300, and I can spray thinner coats with a wider fan pattern that flow out better and dry much faster.

John

2/12/20       #15: Painted Cabinets ...
Adam

First. Do not use latex house paint. Most of the usual suspects have Acrylic waterborne topcoats which are decent, but take too long to dry and reach hardness.

If you want to brush a waterborne finish on a pro grade cabinet. Use a pro grade product. MLC has Aqualente. It brushes really well.

We are located in New England. Painted cabinets have been a thing forever. Some people like it and request it.

I’ve seen a couple of kitchens done by other companies that tried to brush pigmented cv. It looked like some body dragged a hay broom across it.

2/13/20       #16: Painted Cabinets ...
dan shaf Member

We have 2 Devilbiss JGA-502 siphon feed guns, both with 1.4mm fluid sets. One is used for Zinsser oil based primer/sealer (thinned 25% with naphtha) and the other Devilbiss is used for latex topcoats (thinned 10% with water). The 1st coat of latex is cut down with 600 grit wet/dry sandpaper (used dry). The 2nd topcoat is laid out, off the gun. The surfaces have the look and feel of melamine after they dry. We have heated air makeup, plus we can also bake the finishes in the booth.

2/14/20       #17: Painted Cabinets ...
DannyB Member

The thing about spray guns, you can get them to do whatever you want if you learn enough about how they work.

You could just use a reduced pressure (but not conventional/HVLP) pressure feed gun and really, they don't have a lot of trouble with interior paints because they have high enough atomizing air pressure.

It's not a super effective way of spraying walls but it's fine for spraying cabinet doors.

But if you don't feel like going all the way to pressure feed or AAA:

I have a gravity feed gun, and I hook up a 3m PPS pressure cup, and spray latex easily if i need to.

The pressure feed takes care of ensuring good fluid flow.
The gun itself is a compliant (but not HVLP) gun so it has no trouble producing enough atomizing air.

As weird as it may sound, there is nothing that stops you from pressure feeding most gravity guns from a pressure cup. On some guns, doing this with too high a fluid pressure will cause leakage , but you don't need a lot of fluid pressure. Just a few PSI will push the latex along fine.

Most guns these days have fine enough tolerances and sealing that it's not an issue.

It's also nice in general if you like cup-on-top style.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!