Subject: Re: WB Coatings - successive layer orange peel texture

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

WB Coatings - successive layer orange peel texture

10/23/20       
Brent Member

I've been spraying clear and pigmented SW Kem Aqua+ for 2 years now on various casework/kitchens. My typical pigmented schedule is 1x coat of SW KA+ surfacer followed by 2x pigmented topcoats. I am using a good-quality Lemmer PP setup with a Lemmer conventional 1.4mm tip gun @ 42-45psi on the gun and 10psi fluid pressure. My surfacer coat lays fine. I apply my first topcoat for build at recommended mil thickness and it lays down wet, looks good, and dries good. My second coat is applied exactly the same way, looks good, but most always has a very "large texture" very slight orange peel texture to it. It is more pronounced in reflected light. The first topcoat always looks better than the second, it just lacks any build. The problem only becomes more pronounced the more topcoats I add to the system… as in, if I have to reshoot a door to repair a finish defect, the 3rd topcoat has this orange peel texture more pronounced. It has happened to me with the SW KA+ as well as MLC’s Agualente and Magnamax H2O.

My wife can see it when I point it out but I haven't had any clients complain. I'd love to get to the bottom of what causes it. I’ve tried several guns, tried higher and lower atomizing pressure, tried heavier wet mil applications, etc. Anyone have any thoughts?

10/23/20       #2: WB Coatings - successive layer oran ...
Pat

Yep, been liv\ing with this same problem forever. I don't have a good solution. Sometimes it seems to work fine, so I've always suspected that time between coats had something to do with it. Maddening when it happens.

10/23/20       #3: WB Coatings - successive layer oran ...
Shane Welch

The joys of waterborne.... since your already using sherwin products go ahead and switch over to the sayerlack side of sherwin for waterborne.... we tried for years to get the kem-aqua to behave predictably but never really had success.... We only use waterborne when forced to for specific green jobs... otherwise we spray the good stuff! when i do have to go waterborne the sayerlack does perform a little better for us. The trick is reduction and retarding... make sure your reducing with distilled water only at 10-20%.... we also retard with propylene glycol at 10%... Reducing and retarding these this way makes it lay out a ton smoother... Water always looks like crap until it shrinks back an hour later..

10/23/20       #4: WB Coatings - successive layer oran ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

they dont like to lay without a full sanding, you have to have a complete scratch to flow over the previous coat

10/24/20       #5: WB Coatings - successive layer oran ...
MarkB Member

Id argure that the water tends to look better the next day ;-). The shrink back is definitely better with time.

I find with water de-nibbing with a much higher grid than you'd normally use makes a huge difference in how the second coat lays out.

Ever more, the commercial jobs we are bidding spec' water so o'pyning(sp) over "the good stuff" seems a lost cause. If we want the job, and the paycheck, you just put up or shut up.

10/24/20       #7: WB Coatings - successive layer oran ...
Brent Member

Thanks for the responses folks.

Shane: are you suggesting to retard at 2 parts, reduce at 1 part, and have 7 parts waterborne finish? That sounds very runny... I did try and source Sayerlack, but it had to come to me through a SW product finishes department store (4 hours away) and it just isn't going to work for color matches etc. I would still like to try some of the clear though for drawer boxes and the like.

Jon: I do scuff sand between coats with 320gr. I was using 220gr but could see some of the scratches under the topcoat. What are others using for their scuff coat?

Mark: higher grit for scuff sanding as in go up past 320gr (600gr) or down to 220/180gr?

I do agree that the finish most ALWAYS looks better the next day. My rep keeps pushing me onto solvent borne solutions from MLC... but I like the water stuff, and my spray booth is not explosion-proof. I have made it work, and as said no complaints from customers. I'm just always trying to improve both my spray and finishing techniques - hence why I'd like to solve the orange peel look. In a way, it makes me feel slightly better that others are suffering too lol.

10/25/20       #8: WB Coatings - successive layer oran ...
Scott

First thing I would try is a bigger tip, 1.4 is more for an automotive finish. A problem with most guns that are decent quality , but not high end, and are available all over the place, even places like harbour freight, is they are built and sold with the person who is going to paint their vehicle in mind.
Wood working finishes require bigger tips, most water base products are thick, I would move up to at least a 1.8 tip. Thinning a material so it fits through your tip is not the solution, your finish will Have a proper thickness to be applied at. You check it with a viscosity cup and then your tip and air pressure are matched to the product.

10/25/20       #9: WB Coatings - successive layer oran ...
Adam

Your setup might be off.
1.7 n/n
40 psi at the gun with it pulled fan wide open
12-14 psi tank

You are putting a thick finish thru too small of a tip with not enough pressure.

I set the tank pressure with the beer piss method. Start at 10 and work your way up towards a max of 20(thick primer). When the stream has a nice long arcing stream like a beer piss you are golden

10/31/20       #10: WB Coatings - successive layer oran ...
John Member

I could never get KA+ to lay out well, even on the first coat, until I started adding extender/retarder to it. 3% of GF's Extender and it was a whole new world. I actually enjoyed spraying it after that. FWIW, I was using a 1.3 mm N/N set with 5 psi on the PPS cup and 29 psi inlet pressure.

Also, Lenmar's Duralaq-WB lays out beautifully for me straight from the can.

John

11/3/20       #11: WB Coatings - successive layer oran ...
Scott

John,
No offence , but that is why you had to add the retarder, there was not enough product for the material to flow out and flash with the small tip.
I am a firm believer that whatever works for a person is all good, but the retarder is just another thing to buy and add.

11/3/20       #12: WB Coatings - successive layer oran ...
John Member

No offense taken Scott. I guess I'm just not good enough to spray uniform coats w/o runs or pooling at inside corners with a larger N/N and higher flow.

John

11/21/20       #13: WB Coatings - successive layer oran ...
scott

John,
That is a valid point , having to much fluid is the flip side, definitely harder to spray when doing vertical surfaces and the insides of cabinets. To much fluid can cause solvent pop, runs and a different set of problems. The lesser of two evils is different for everyone.
Most days spraying is a pleasure, with fantastic results, some days you wish you would have stayed in bed.
Have a great day.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!