Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Pre-cat VS CV for kitchen re-sprays

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Pre-cat VS CV for kitchen re-sprays

3/11/21       
Joel

Hello, I am thinking about going after residential re-sprays. Just the thought of all that light good paying work is getting me excited, To be honest I have only done two. One fifteen years ago, one eight. I know the people. Both were sprayed with pre-cat and still look good. No moisture problems even around the dishwasher.
I plan on marketing myself as a pro and charging accordingly. I feel I owe it to the people to use the best finish. I have sprayed a ton of pre-cat but never CV. I believe any decent pre-cat is going to be functional and look good for 20 plus years based on my limited experience. It is easy to spray, cheap, and durable. Why should I switch to conversion varnish? Thanks

3/11/21       #2: Pre-cat VS CV for kitchen re-sprays ...
rich c

I had just the opposite result with Precat when I did my own kitchen. Glad I used conversion varnish on the other kitchens I built. It's going to be a rare customer than doesn't mind the out gassing of either of those finishes in their homes.

3/11/21       #3: Pre-cat VS CV for kitchen re-sprays ...
rich c

I was thinking only solvent based when I made the comment about off gassing. Maybe you are referring to water based.

3/12/21       #4: Pre-cat VS CV for kitchen re-sprays ...
Daniel Berlin Member

Hey Joel,

I 100% would not use pre-cat for this purpose.

I have personally seen many mid to high end kitchen totally ruined by using pre-cat, even "decent" ones.

I've pretty much only had the opposite experience of you - most kitchens i've seen redone were originally done with "good" pre-cats, and rarely done with "good" CV.

Despite what you say, there is often a ton of cracking/peeling around high moisture areas pretty quickly.

A number of these kitchens have no-overhang + inset cabinets. For these, every pre-cat install i've seen started having issues pretty quickly.

I can believe that in a full-overhang, non-inset, low moisture, kitchen that pre-cat can survive quite a while.

Overall, i'd offer that if your view on pre-cat (fast enough, cheap enough, durable enough) was correct, the industry would not have moved on :)

3/12/21       #5: Pre-cat VS CV for kitchen re-sprays ...
Joel

Thanks for the responses. I guess it's time to switch at least for kitchens. One more question though..have you had any problems with CV sticking in a re-finish situation? Thanks

3/13/21       #6: Pre-cat VS CV for kitchen re-sprays ...
mastercabman

Joel
I refinish kitchen cabinets
I use a white vinyl primer then use a CV like the MLC Turino
I catalyze the WVP like the instructions suggest

"WVP,I put that $#!& On everything!"

3/13/21       #7: Pre-cat VS CV for kitchen re-sprays ...
mastercabman

As far as pre-cat vs post cat
I think it depends on the product you use and if it is applied correctly
I get calls sometimes when a homeowner needs their cabinets touched up
I recently visited one that I personally installed the cabinets about 10 years ago
Cabinets are from Kraftmaid
Lots of paint peeling/rubbing off
Mainly on the sink base
Other areas not as bad but rubbing through on doors near the knob/pull
I know for a fact that Kraftmaid uses a CV but I'm not sure what brand
But that's not the only time I've seen this with Kraftmaid
I've used pre-cat on kitchens before many times
I used MLC Magnamax or Magnaklear
I never had a problem
As I stated before, when refinishing cabinets and not sure what's on it
I always use white vinyl primer

3/14/21       #8: Pre-cat VS CV for kitchen re-sprays ...
jOEL

Thanks mastercabman! Good tip.

3/14/21       #9: Pre-cat VS CV for kitchen re-sprays ...
Jeff

What is an equivalent water based product to white vinyl sealer?

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!