Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Kremlin 10-14 vs. "?"

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Kremlin 10-14 vs. "?"

5/17/21       
MHorrillo

Been running my 10-14 for the past 20 years. Second pump, third gun. Looking into a like and kind replacement to shoot "Cat's" and maybe WB. Yes I know this is like asking your preference between a blond or a brunette. We are a heavy use in shop and in field. I have had good luck with CA Tech equipment over the years. For a second unit, I also like the cost factor of a non-kremlin?

5/19/21       #4: Kremlin 10-14 vs. "?" ...
Scott

You say you are heavy use, so that tells me you are going to use the equipment all the time. If it was me and I was using it all the time I would want something top of the line.

If you are getting into some water base coatings that are thicker a 14:1 pump is not sufficient, if you talk to the experts the pump creates a shear effect on the fluid. Don’t get me wrong , people are still using these pumps. The shear effect changes the viscosity of the fluid. There are some good articles that explain this on the internet, check out the American coatings association, they have some good information.

Anyways back to the pump, I would recommend spending a little more and get the Kremlin 30:1 pump, the pump is simply amazing. I have 3 CAT 14:1 pumps and the Kremlin pump, I like it so much that I am in the process of trying to sell 2 of the CAT pumps. Don’t get me wrong, the CAT pumps are also great pumps, they have given me no problems, they are just a little weak for the heavier material.

At the end of the day I think all the companies that make these products have great equipment, so getting something that you have good service close by is also important.

5/19/21       #5: Kremlin 10-14 vs. "?" ...
MHorrillo

Thank you Scott. Fully understand the shear issue with WB. I also hate the WB finishes, but still are forced to use them at times. Will check into the heavier pump.

5/19/21       #6: Kremlin 10-14 vs. "?" ...
Jim Knowles

Scott where are you located? I am intrested in your pumps.

Thanks jim

5/20/21       #7: Kremlin 10-14 vs. "?" ...
mastercabman

Yes Scott!
Where are you?

5/20/21       #8: Kremlin 10-14 vs. "?" ...
MHorrillo

Dumb question Scott. How does the 30-1 spray Post Cats and C.V.'s?

5/20/21       #9: Kremlin 10-14 vs. "?" ...
herb johnson

the ratio is not creating the shear. the shear is created by the very small passages in the cat pump small fluid passages as would any pump made by graco, binks, etc. specifically the upper ball check area first then the lower ball check area. if you go to a higher flow rate pump say upwards of .8 to 1 gpm typically a 14-1 will handle most wb as most of the ones that i spray will atomize at approx 1000-1200 psi while it is certainly at the higher end of my pumps pressure rated it certainly is not anywhere near its flow capacity or max strokes per minute which is really what wears a pump out, which is strokes per minutes or the number of strokes the piston rubs against the upper fixed packing of the pump and cup packing on the piston rod. hope this gives a better explanation of wb shear to everyone related to pump shear for waterborne coatings

goodluck
herb j

5/21/21       #10: Kremlin 10-14 vs. "?" ...
Scott

I am located in the great white north, in Western Canada.
I think the Kremlin pumps are the best AAA pumps available as far as transfer rate. I also have fantastic service available for them.
I will also admit that they are expensive , I didn’t realize they had gone up as much as they have, so that could be a definite disadvantage for some. Having said that, I am not sure what the other manufacturers are as far as price point, maybe they have gone up as well and I am out of touch..

Equipment is all based on the opinion of the finisher, just like your favourite truck is a GMC and mine is a Ford, or vice versa. Like I mentioned earlier, I think all the pumps are good these days, that is the only way a company can stay in business.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!