Subject: Re: Exterior grade finish for Teak

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Exterior grade finish for Teak

10/9/21       
Mike

Hello everyone. As long as I have been a pro, for 27 years, I rarely have ever used Teak. I have a project where my customer wants me to make a two person glider and two rocking chairs. We are in Chicagoland, so the brutal snow winters are inevitable. I am looking for a finish that will be strong enough to hold up to the Chicago climate. I need something that will allow snow to literally sit on the Teak and not break down/ruin the finish. Is there such an animal? I have reached out to my supplier to find out if I use 2K isolante, along with a 2K acrylic urethane by ilva, will be strong enough to hold up for the long term. (He is going to reach out to the manufacturers rep to see what they suggest.)He is going to reach out to the manufacturers rep to see what they suggest)

I spoke to one other professional recently who suggested tung oil and Naptha (3 coats until it turns out like honey)or mineral spirits as a cut with tung oil. He claimed that combination would do what I am looking for. To me, tung oil has always been an interior finish.

Thoughts? Ty

10/9/21       #2: Exterior grade finish for Teak ...
RichC

Any film finish I have used is doomed on exterior wood because of wood movement. The seasonal or daily movement will sooner or latter crack the finish. Then water gets in the crack and the film completely fails then. Don't use any organic oils as they are susceptible to allowing mold and mildew to grow. Sorry, but I don't have a current preference for outdoor. You can caution the customer that oil needs a renewable nearly every year, and film finishes need to be stripped and redone around every 5 years. I can't understand why they won't store it away in the winter. Who sits outside in Chicago in Jan and Feb at the least! Or do they plan on using it to reserve parking places?

10/9/21       #3: Exterior grade finish for Teak ...
Mike

What are your or anyone’s thoughts on typical teak oil And needing to do that say twice a year.

They live in an area where I don’t believe they have a garage that is going to be big enough to store a double person glider and two rocking chairs. I don’t know what the inside of their home is like, so I don’t know if they would even have room for there either.

10/9/21       #4: Exterior grade finish for Teak ...
RichC

The only difference between teak oil and danish oil is that teak oil has more flatting agent in it and dries to a flat sheen. The difficult part of a glider is it is usually made of slats. And there is no more difficult construction to refinish often. Today's teak is not the teak we used decades ago. Plantation teak does not have the rot resistance of old growth teak. I have no experience with teak or danish oil for outdoors. This article may help you.

https://www.popularwoodworking.com/flexner-on-finishing-woodworking-blogs/teak-oil-what-is-it/

10/9/21       #5: Exterior grade finish for Teak ...
Mike

What are your or anyone’s thoughts on typical teak oil And needing to do that say twice a year.

They live in an area where I don’t believe they have a garage that is going to be big enough to store a double person glider and two rocking chairs. I don’t know what the inside of their home is like, so I don’t know if they would even have room for there either.

10/9/21       #6: Exterior grade finish for Teak ...
Adam

Film finishes are useless in a harsh climate. Especially horizontal surfaces where you will have ice, snow, water sitting on it for long periods of time. It doesn’t matter what type of film. Once it gets scratched the water will get under the finish and will delaminate/ discolour. Very high maintenance. Every year or two depending on the damage you will have to “wood” the finish and grind it all back.

The other issue with film finishes is UV protection. I have no idea about the 2K’s you mentioned, but the best marine varnishes need to be recoated annually. Those have the highest UV protection available and still get trashed on boats from the sun.

I would look at using a penatrating finish. Checkout Penofin. It’s used on Ipe decking. Sikkens makes many different products. You need to research them and test some one teak specifically. They look different on all woods. The older versions looked a bit orange on teak. They have better products now.

Tung oil is not rated for exterior use.

No matter what you do it will be an annual maintenance problem. On the real high end houses in CT is common for them to put covers on the nice outdoor furniture.

I’m an architectural woodworking & boat guy. No good solutions for this problem.

10/9/21       #7: Exterior grade finish for Teak ...
Mike

Thank you Adam. Makes total sense. So, when it comes to putting a finish on teak for a boat, what do you recommend? I also strongly advised the customer to put custom-made slip covers with an exterior material on top of them send it to bring them inside from the elements as possible during the winter

10/9/21       #8: Exterior grade finish for Teak ...
Mike

Adam, what do u think about teak oil? I know it may need to be coated a few times a year. Will a product like teak oil be OK for the spring/summer and fall rain storms?

10/9/21       #9: Exterior grade finish for Teak ...
Adam

We still do versions of varnish on boats. They have the typical oil based, poly. and high build epoxy like.

Teak oil is a high maintenance chose. There are numerous products. I’ve never liked the look. It’s for people who don’t know how to or want to spend the time varnishing , or don’t like the glossy look.

Like, I mentioned before look at Penofin or Sikkens. Teak oil is cheap rubbish in my opinion. Any of the penetrating finishing will get you thru your stormy weather. There is also aesthetics. Plus, Once a year should be enough or find another product.

10/9/21       #10: Exterior grade finish for Teak ...
Mike

K. Could you pls provide me model numbers/names to those you recommend? Ty

10/10/21       #11: Exterior grade finish for Teak ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

Mike, We are not far from you(more north) and we do our share of Teak Patio furniture.
I have been finishing for 41 years and so far this is the best I have found so far. Epifanes Teak Oil Sealer. Every type of finish has its pros and cons. Every product will have maintenance.
I Suggest buy a liter and make samples. Epifanes is easy to recoat and works well.

Epifanes Teak Oil Sealer

10/10/21       #12: Exterior grade finish for Teak ...
Nick

I live in a more mild climate than Chicago & north of there (thank god) and there is no answer to this question only compromises. I agree with the Epiphanies plus a maintainice contract or if that's not what you do suggest it.

10/10/21       #13: Exterior grade finish for Teak ...
Nick

PS; of course there is a reason teak is used outside in the harshest of climates. It's silica content enables it to do so without damage even without any finish at all. If your clients don't mind it silvering and are willing to move it indoors during winter...no finish might be the best finish.

10/13/21       #14: Exterior grade finish for Teak ...
David Sochar

Website: http://www.acornwoodworks.com

Zackly. Teak is used when wood is desired, but endless refinishing is not. The current crop of buyers that want Teak do not want it for its extreme weatherability, but for its quiet cachet of class. Go to England and dit on a 100 yr old Luytens teak bench that has never had a finish, and suggest to them they really should get with the program.

10/19/21       #15: Exterior grade finish for Teak ...
John Member

I'm near Niagara Falls so the weather is fairly similar to Chicago. There are several Pentofin products; the Hardwood Oil one doesn't hold up on Ipe' worth a damn. Nor does Ipe' Oil or Armstrong Clark's product. I'm fairly optimistic a product called One Time is going to work fairly well, but won't know for sure until next Spring.

Covers are your best option if you use a film finish, or any finish actually. Once I started covering my Epifanes Marine Varnish finished black locust bench with one I've done zero additional maintenance. Prior to that it would crack/peal just as Adam described.

John

10/23/21       #16: Exterior grade finish for Teak ...
Bart

In the early 2000's I helped out my neighbor selling teak furniture on weekends. Over the course of 3yrs I acquired a fair bit teak furniture mostly exterior stuff. Being a "pro finisher" and wanting my teak to look good I used Semco. It's a penetrating solvent sealer. Almost watery. Easy to use and if you catch it before it fails easy to re-seal. Just light power wash, light scrub brush, let it dry real good and re-seal. It has a kind of dead look in the tinted versions but I thought it looked better than weathered gray. But when you got 8 chairs and a10ft table it's still kind a of pain in the rear. About 10yrs ago I finally just let it all fade out and just hit it with some 220gr on wear areas and tabletop once or so a year. I'm over it.

cheers
my2cts

http://www.semcoteakproducts.com/

10/23/21       #17: Exterior grade finish for Teak ...
Bart

BTW, If you do go with any type of finish invest in covers. Not cheap but they will definitely stretch out your maintenance schedule.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!