Subject: Re: using pre-finished plywood vs raw/unfinished

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

using pre-finished plywood vs raw/unfinished

1/21/22       
michael aufiero Member

As with most cabinet shops today many of the jobs that I undertake are solid color finishes. Given the state of the quality of plywood as the preferred substrate with voids below the top sheet of veneer, separation of the veneer at the seams, many variations in grain, extremely thin veneers themselves...etc , I have been using pre-finished clear maple ply as the substrate to spray all of my color jobs. This gives me a super smooth substrate with none of the problems that I have mentioned above.
My schedule is I sand the pe-finished plywood with 220 grit to help with the mechanical bond of the primer ....1 coat primer.....2 coats of the pigmented topcoat with 320 sanding in-between. I use Kem Aqua "Surfacer "Primer with 2 coats of Sivam waterbase color.
I do worry somewhat with the adhesion of the Primer to pre-finished maple ply. So far so good.........................anyone else using this method?.........and with what results. thanks for any response on this

1/21/22       #3: using pre-finished plywood vs raw/u ...
Mark B

Ive done the same thing numerous times with no issue mainly because we bring in UV clear prefinished one side domestic ply for cabs cheaper than we can buy raw and far cheaper than veneer core melamine. The pre-finished is about the best veneer substrate Ive found for pigmented work and the domestic stuff is flat so your 90% of the way there over any raw material (grain raise, warpage, etc).

We cut for another shop who insists on raw ply for carcass material that they spray in house and it drives them nuts that the pre-finished ply we run is most always a few bucks cheaper than their raw material but they continue to run it.

1/22/22       #4: using pre-finished plywood vs raw/u ...
Chemmy  Member

I guess I don't understand.?? In Fl. back in the early 2000's, We were using the pre finished maple ply as a selling point, it was always used for the interiors of all cabinets, and being a UV cured urethane, we guaranteed it's performance as to chemicals etc. It was a great interior finish and cut down on the over all finishing cost drastically. Our kitchen jobs usually ran in the 50- 85, thousand range, for the finest homes in south Florida, how could a water base finish out perform a UV Urethane.??
For our exterior finishes, yes we did both painted and natural wood finishes, multi step glazes etc.
With only the face edges of the boxes being painted, never the already finished interiors.
Is it now the case that your customers are demanding color matched painted interiors or what.?? Help me understand what's going on please.??

1/22/22       #5: using pre-finished plywood vs raw/u ...
Mark B

The point is regardless of your 50-80k FLA mc mansions (florida is the dog sh$t of construction standards... an utter hell hole) uv cured prefinished ply is sold in such quantities that it is in fact one of the best substrates for any subsequent pigmented finish regardless of solvent or water. You have a pretty much dead flat, smooth, starting point thats cheaper than even veneer core melamine.

I would not be steering my offering based on anything produced in the FLA market. That can be some of the worse of the worse. I know theres quality there (forgive me harold et al) but FLA is not known for anything quality on mass

1/22/22       #6: using pre-finished plywood vs raw/u ...
Leo G Member

I do the same thing except I'm using a solvent based finish on top of the UV.

Sand 150, prime, 320, pigmented coat, 320, top coat.

1/22/22       #7: using pre-finished plywood vs raw/u ...
Matt Calnen

Mark B, What brand of one sided UV are you using that stays dead flat? The Roseburg and Columbia I get from my supplier never seems to be, or stay flat. I assumed it was because it was only finished on one side, so it had unbalanced moisture in it. Is the stuff your using the what the call combi core? It has mdf as the ply directly under the face veneer.

Also, I sure would not lump all of Florida’s quality of work into one basket. I live in northern Michigan, and I have several customers that have their main homes in Naples. The level of work in a lot of those homes is superb. A lot of them have much more expensive kitchens than $85,000.

1/23/22       #8: using pre-finished plywood vs raw/u ...
shenendoah

Chemmy started his post writing that in the " early 2000's " his kitchens were 50-85 k. That would be today 85 - 100 k +.

And I share his confusion re is this a trend? We don't see it and our designers/decorators have an awareness of what's going on in 2 of our country's very higher end and trend setting markets.

So, along with Chemmy I ask: What's going on guys?

1/23/22       #9: using pre-finished plywood vs raw/u ...
Bill

Have you tried something like this?

HDF ply

1/24/22       #10: using pre-finished plywood vs raw/u ...
Bill  Member

Website: canadianacabinets.com

Guys it has been our experience that pigmented solvent base lacquer will not adhere to the us coated plywood. Thoughts?

1/24/22       #11: using pre-finished plywood vs raw/u ...
Mark B

Matt,
First, I will agree that my broad brush of the FLA market is a stereotype. That said, I have known personally many who have operated in that market as well as people who have owned in that market and I think anyone whether its maker or owner who is speaking honestly would say its a "peculiar" market to say the least. Spin peculiar any way you want but transient, quick, in-and-out, partial use so good enough is good enough, whatever. Its not a viewpoint of FLA that is unique to me. But yes, broad brush stereotype not good on my part.

The Columbia, RockShield, even a States to an extent, for me at a least, has been exceptionally flat. I have never had a single complaint about Columbia other than at the moment the cost, and most generally in my area the availability. I havent had much bad experience at all with 1/2" and 3/4" prefin 1 side North American core period. But what you consider flat and what I consider flat may be completely different animals. Flat to me is something that lays down on the CNC without opposing corners up in the air that require being held down for the vac to pickup and your hoping once you start cutting the tension out it stays put. That scenario is junk in my world. Ive never had a sheet of Columbia behave like that. Now if we are in some sort of "fine furniture" flat I would have no idea how to qualify that.

All the pf1 and pf2 domestic Ive had in the shop is more than acceptable for anything we've run and when top coating it with pigmented, as I mentioned, youve got a pretty much dead smooth starting point.

The times when I miss it is when the customer wants some grain showing through the finish and you have to start from raw. More work.

1/25/22       #12: using pre-finished plywood vs raw/u ...
shenendoah

Bill,
20 + years ago approached painting prefinished ply having not done so before. We sanded with 120 grit thoroughly( never would I use 220 - gets burnished in a heartbeat as the uv is too hard, so the scratch pattern is iffy and not deep enough!) and cv primed until fully white. Waited a week and did cross hatch and abrasion tests. No issues, none. Other than had to sand to level, etc. Waste of time. Easier to skin mdf/hdf to 1 sided prefinish ply - prefinish interior side, mdf/hdf flat panel exterior for painting. Edge band. Done.
Now your suggestion re hdf is good re assembly screws/ splitting etc., yet doesn't solve the prefin for the interior on a 3/4" frameless job which I think is where the whole conversation started. I am honestly not sure as the questioner didn't specify whether this was all about finished flat fronts, end panels, interiors or both. Nor did the "first responders." I assume they are referencing painting flat finished end panels and fronts and were on the same page. Not so Chemmy nor I were on that page.
If that is the case, I have spent hours dumping on primer and then leveling plywood prefinished or not. Plywood is not flat. Prefinished plywood is not flat- much better yet not flat. Typically, grain and manufacturing waves that need to be leveled. Too much paint and too much labor. Of course, it depends what your gloss is - dead flat, 10, maybe 20, certainly not 35+ - and what your expectations are.

And Bill, I haven't used poplar core in ages - 15 years? - back then lots of voids and other issues. I assume it has improved? Post please.

2/2/22       #13: using pre-finished plywood vs raw/u ...
Nick Sinderson

In my experience, l've found that better adhesion to uv cured prefinished plywood is achieved by a finer scratch, 320 grit is my grit of choice before priming.

4/6/22       #14: using pre-finished plywood vs raw/u ...
Mastercabman

I have a job coming up that I will be building and finishing with a solid color
I've been thinking of trying out this idea of using UV finished plywood instead of MDF
I primarily use MLC product
My go to primer is white vinyl primer and then Turino as my finish coat
Should I look at a different primer?
Or is the WVP good enough?

4/6/22       #15: using pre-finished plywood vs raw/u ...
Leo G Member

Never used it before on the UV coated. But that stuff sticks to everything. Still scuff the UV coating before priming.

4/6/22       #16: using pre-finished plywood vs raw/u ...
Mastercabman

Leo
Thanks
Yes you're right about that WVP
And yes I am planning on scuffing the UV surface

8/3/24       #17: using pre-finished plywood vs raw/u ...
nobapula Member

I have also worked with pre-finished maple ply for my cabinet projects and found it to be a game changer. Like many of you, I sand with 220 grit to ensure a good bond before applying primer. The smoothness and consistency of pre-finished ply significantly reduce prep time and eliminate issues like grain raise and veneer separation. I have used both water-based and solvent-based finishes with excellent results, but I make sure to use high-quality primers to ensure proper adhesion. Overall, the benefits of using pre-finished ply far outweigh the drawbacks, especially for achieving high-quality, solid color finishes. You can check here https://mjklosscarpentry.co.uk/ for more ideas.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!