Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: 2 quart pressure pot

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

2 quart pressure pot

10/21/22       
Scott

I have never used one of these, so I have a couple questions, they range from $70 to $500 plus. Like a Harbour freight one compared to a name brand. Is there really a big difference in quality? I am not looking for a gun as I have lots of those.
I am planning on spraying some viscous coatings, just small batches on an extra door or filler or a screwup.
I am looking at the Kremlin gravity gun with a pressurized cup, but they want $920 for that? Wowzer! Maybe it is worth it?
Not sure if anyone has some other ideas, I have 4 air assisted pump, Kremlin and CA Technologies, I have big pressure pots, I have an airless pump. I have sata and lemmer and 3M gravity guns.
I just need a system to get some really good finishes without reducing this heavy material and throwing a bunch away when I prime a pump.
Thanks for any ideas?

10/21/22       #2: 2 quart pressure pot ...
herb johnson

how much are you mixing up at time? and do you need stainless steel? so for options, how about putting a one gallon can in a two gallon pressure tank that most people have laying around? buy a new set of hoses shorter the better that will still work for you, there you go alternatives expensive, one qt pressure cups, heavy and expensive, cheap two 2 remote cups, usually fluid air pressure regulators are of poor quality.......

me, shorter hoses, one gallon can in a 2 gallon pot, good to go, less expense, works well, easier on the wrist........, sometimes have to shorten the pick up tube on the pot but they are cheap and easy as crap to replace

good luck
herb j

10/21/22       #3: 2 quart pressure pot ...
Scott

Herb,
Thanks for the info, I didn’t even think of putting a smaller pot in the bigger pressure pot.

I usually spray a set of cabinet doors with my Kremlin air assist, I will mix about a 1/3 of a gallon and that primes the pump and sprays one side of the doors as I spray everything flat unless on site.

I am looking for a set up to spray just a few ounces for say a door or two.

10/21/22       #4: 2 quart pressure pot ...
herb johnson

how thick is the material, most of the time a decent gravity gun with a 1.8 tip or 2.0 tip. not even hvlp gun just a air spray hvlp, with that little material, you are looking for convenience, not paint savings......i wouldn't even full around with a tank and hoses with that small amount, blow it on with an air spray gravity gun, so what if loose 35percent of your material cost, you will get killed with time cleaning and solvent cost messing with a p pot with that small amount of material??????? just my two cents, in bidens world i don't want to think of its true value anymore................maybe just the copper

10/21/22       #5: 2 quart pressure pot ...
Scott

Herb,
Everything you said is bang on. The product I have been spraying lately is Envirolak, I just hate mixing a 1/4-1/3 of a gallon to prime a pump to spray say 1 door that was dropped and needed to be rebuilt as an example. I tried a sata gravity gun with a 1.8 tip, I had to thin the material and it changed the sheen. It doesn’t happen very often, but I hate wasting material when it is $100 a gallon..

10/22/22       #6: 2 quart pressure pot ...
Mastercabman

Scott
What's the viscosity of Envirolak?
If it's like most waterborne it should be fine with a gravity feed gun
For small jobs like you described I wouldn't bother with a pressure pot
You still need material to bleed the line
And clean up can be a b&$# at time
I use CA Technologies J100 gravity spray gun with PPS cup
You could also look into a turbine sprayer
The cup gets pressurized to help pushing material out
But they can get expensive
Good luck

10/24/22       #7: 2 quart pressure pot ...
chris

you can get the PPS with a pressurized cup. i use it to spray small amounts of polyester. works fine. easy to clean

10/31/22       #8: 2 quart pressure pot ...
Adam

I would be amazed if you can't get a wb topcoat out of a Sata gravity gun with a 1.8n/n. I'm assuming it's the high transfer HVLP type that runs on 40psi.

Like others have suggested, we would use a gravity gun. Regardless if you have the 3m cleanup system or not. You waste hardly any material or solvent cleaning a gravity gun.

If you are seriously interested in getting a 2qt pot setup for any other project, I highly reccommend the Starr brand gear. It used to be available under the Astro Pneumatic brand as well. Great HVLP guns & there 2qt setups are perfect out of the box. I used to spray tons of heavy bodied wb MLC primer out of my 2qt. The gallon was a waste of time and material to clean.

10/31/22       #9: 2 quart pressure pot ...
Svott

Thanks for all the good information.
I ordered the cartridge and the pressure cup for the 3m gun. I will give it a try.

I could get a good finish with the sata gun, but I had to add at least 5% thinner to the material. The thinner changes the sheen, it doesn’t look good if you have the odd door that is different.

10/31/22       #10: 2 quart pressure pot ...
duster

The 2.0 tip works well for heavier coatings with the 3M pps gun.

12/21/22       #11: 2 quart pressure pot ...
Nick Sinderson

I have every imaginable paint application system in my shop ( from AAA, pressure pots & cups, diaphragm pumps, airless, turbine and gravity guns.) The 2 most used set-ups are the AAA pumps and gravity guns. Occasionally l'll use the airless fir very viscous material or pressure pot/gun set-up for spraying stain.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!