Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Finish for Outdoor Cedar

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Finish for Outdoor Cedar

7/18/21       
howard

Website: http://woodcontours.net

I've been commissioned to carve some cedar posts for an outdoor porch. I need a durable finish to keep the carvings intact. I've heard about marine varnish or clear penetrating epoxy. I'm very experienced with indoor finishes, but outdoors is another thing. I would appreciate suggestions and brand recommendations. Thanks

7/18/21       #2: Finish for Outdoor Cedar ...
Adam

Epoxy is not an outdoor finish. It gets hammered by the uv.

Marine varnish is high maintenance. Somebody needs to coat it once a year.

There are penetrating/thin build products made by Sikkens. Do not listen to negative people who used it 20 years ago. They have 6 different products all excellent. When it was first introduced to the US back in the 90’s it was marketed to the boating industry as a teak finish. It didn’t look good back then on teak. Products are different and cedar is a perfect wood.

7/19/21       #3: Finish for Outdoor Cedar ...
matt

Understand what you're going to be dealing with on exterior grade finishes. You have two basic options, NEITHER of which will ever stand up to the brutality of UV exposure, extreme temp fluctuations, and rain/humidity/freezing. All of in time will need TLC.

1) Thick film finishes. They all vary in their durability, and you can spend as much money as you want here. If you require high gloss, this is your only option. Expect the sheen to last maybe a year, regardless of the initial sheen. Old school SPAR varnish is reasonably decent and also not too difficult for the customer to rescuff and brush on a maintenance coat. There are post-cat products available but I honestly doubt their value in most case.

2) Thin film and oil finishes. Sikkens, mentioned by Adam, is a reasonable option. I've used a little of it here and there and always liked it. It looks like an oil finish.

Thin films and oils don't ever really have that "deep" look that thick varnishes have. But thick varnishes flake, peel, and look wretched after a few years if they don't get maintenance coats.

Personally in your shoes I'd punt this to the customer and see what they expect. Either way, I would not warranty the finish the way I would an interior product. Put everything in writing and make sure all options spell out specifically that exterior finishes WILL take a beating.

7/21/21       #4: Finish for Outdoor Cedar ...
Bart

Actually epoxy (West systems) is used as a stabilizer in the marine/boat finishing. They use it to build film thickness and keep the wood from moving as little as possible and then a couple of topcoats with a good marine varnish (Petit marine) . It's called bright work and has to be maintained on a minimum 2yr schedule.
I've done live edge wood tables this way and it's time consuming but it looks great.

The problem I see with the soak in types such as Sikkens or TWP is if you let it past its recoat window you're in a world of hurt having to strip/sand it off.

If it were on my porch I'd just throw an exterior grade oil like Watco on it. If it's in the shade you could maybe get 2 years. Just clean it or pressure wash with a small home unit, let it dry and reapply. Much more user friendly.

my2cts
cheers

7/23/21       #5: Finish for Outdoor Cedar ...
Adam

Bart,

I’m a brightwork/ boat guy. You are technically correct in the way epoxy is used outside. However, no one with any experience does it. We do use the epoxy, varnish on things inside the boats like the sole(floor) to build quickly.

The problem outside is epoxy gets trashed by the uv big time(west system makes an additive that temporarily helps). On the boats the wood gets damaged frequently. Now you have bare wood, some epoxy , and some varnish at the ding site. How do you fix it? It looks terrible after recoating. Whereas with just varnish, you simply sand it and coat it.

12/14/22       #6: Finish for Outdoor Cedar ...
Jack Ducan Member

Website: https://www.ridetheducksofseattle.com/

This TotalBoat varnish is hands down the easiest varnish I have ever used. I used to use Petit Flagship on my brightwork, and it took forever to get any kind of buildup. With Lust, you really can get 4 coats in on the same day. The shine is excellent and the only advice I would give you is to thin it a bit to get it to flow out better.

12/21/22       #7: Finish for Outdoor Cedar ...
Jack Ducan Member

By following the manufacturer’s instructions, I’m able to get the desired finish. Thanks to its classic spar formula with a modern twist. It’s ideal for exterior and interior wooden parts and brightwork on boats. It is the best marine varnish for me as it keeps my boats looking good.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!