Subject: Re: Milesi questions

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Milesi questions

5/7/24       
Pete

Website: http://cherrybrookwoodworks.com

Looking for some feed back/advice. I've been a custom furniture maker for close to 30 years. My finishes will range from a traditional French polish to spraying solvent lacquers. Every piece is custom color or color matched. I am used to and comfortable with colors/products- Lockwood water stains, Mohawk dyes, pigments stains and glazes. I spray with a 5 stage Apollo turbine which works great for “one off” pieces of furniture. Im not spraying cabinets or large quantities of pieces. I'm starting to look into Milesi solvent products. Has anyone used the mohawk product line with the milesi solvent products? I know the companies say to use their own products but I have too much $ in stains/dyes etc to switch to and that goes for water based too.

The last job I did- mahogany table, water stains for color, lacquer mist coat of sealer, added NGR dye to sealer to adjust color, lacquer top coat. Usually there may be a glaze/pigment color application in the process as well.

I am currently waiting on some info, particularly a PDS sheet, on the milesi line to start doing some samples for myself. Just wondering if anyone is using these products together without issues.

Thanks.

5/7/24       #2: Milesi questions ...
mauricio poli

In my opinion there is no problem.
All you have to do is first to check in scrap panels searching bad adhesion, pin holes, craters, some kind of bad compatibility with your stains and Milesi material. If everything is ok you could finish your furniture with more confidence.
Hugs!

5/13/24       #3: Milesi questions ...
Al

Pete,
I can’t answer your question. I thought regular lacquer was done away with. When I first started I would spray lacquer sealer 50/50 with thinner and then 2 topcoats lacquer 50/50 with thinner. Sanding between coats was easy and quick but not required as next coat burned into previous coat. Does Mohawk still sell products like this? In my opinion still the easiest system to use.
Very nice work that you do.
Al

5/13/24       #4: Milesi questions ...
Pete

Al,

Lacquer is still very much available. But what about a hi gloss, closed poor, durable finish? Regular nitro lacquer is time consuming, even with a grain filler. A more durable finish now has mil limit thickness. Im just wondering what I can and can not do with the milesi solvent vs lacquer.

5/19/24       #5: Milesi questions ...
Chris

I’ve been using Ilva products for past 10 years from camgercoating in Ma. They are very similar to milesi products For a full fill finish I use polyester followed by acrylic urethane I can normally get a full fill with just one coat of poly which gets sanded flat through a wide belt sander benefit is a very durable finish which can be buffed to high gloss The downside is it is harder to repair

6/6/24       #6: Milesi questions ...
Adam Member

Website: https://virmer.com/

Given your extensive experience in custom furniture making and finishing techniques, transitioning to Milesi solvent products could be a promising step. While both Mohawk and Milesi recommend using their own products, mixing and matching can be successful with proper testing. Waiting for the Milesi PDS is wise, and seeking advice from other professionals can offer valuable insights. With your expertise, you're well-positioned to navigate this transition effectively.

6/6/24       #7: Milesi questions ...
George Member

Website: https://wattsan.com/

Experiment with small test pieces to see how Mohawk and Milesi products work together. Check with both suppliers for compatibility advice. Keep detailed records of your experiments, and seek feedback from peers. Aim for consistent, high-quality results that meet your clients' expectations.

8/24/24       #8: Milesi questions ...
Dan

We typically spray Resisitant , it’s a post cat , but recently we have been using some Milesi water Bourne it takes a bit getting used to but seems to be a nice finish product

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!