Kitchen and bathroom cabinet/ vanity finishs

7/18/15       
JP Member

I am a electrician by trade and I make cabinets as a separate business. I picked up a whole house recently.

Tongue and groove blue pine or cedar on all of the walls and ceilings.

I would have tried to pre-finish the wood for the walls and ceilings but there wasn't the space to lay it out.

I have already made the cabinet boxes.

The face frames and doors are red oak and they want them dark.( almost black )

I made a few sample boards with transtint dark walnut mixed with water as the base color and used Java gel stain over it because of the grain not taking color well.

On other test board I tried Charles Neil prestain conditioner and just used the water based transtint dye.

Both turned out good.The non conditioned oak with dye and then gel stain turned with the least amount of messing around.

What should I use as a clear? I'm thinking pre cat lacquer for everything. I want a repairable surface.

Sealer? Shellac?

The local Sherwin Williams only has nitro laquer ( I keep some around )
and pre cat ( which I have never used ).

I am going to spray it on with a Fuji turbine unit on site.

I also need a recommendation on what to spray on western red cedar ( interior ). Some of it is in sun catching windows. I don't think they want it turning grey.

The local ACE told the home owner to use Thompsons water seal. All of the wood is interior.

I'm thinking on renting a airless for spraying the walls.

Thanks for your help.

7/18/15       #2: Kitchen and bathroom cabinet/ vanit ...
rich c.

Precat will not last around the sink, dishwasher, and range hood. It cracks at the joints, then water and steam leak in. The finish then fails at those cracks. I did mine 20 years ago when I first tried precat. It was a mess in around 5 years. Nitro is worse, shellac is horrible if any moisture around. Use conversion varnish on the cabinets, or a professional water based product from General Finishes. I've never used shellac under precat. If you insist on using precat, be really careful with film thickness. It also likes to cold check if sprayed too heavy or with too many coats. You are really going to spray nitro or precat onsite? That's not healthy for anyone! Expect a visit from the neighbors, or the city inspector, when you put the fan in the window! That house is going to stink for days! Oh yeah, the tongue and groove is going to shrink this winter so they will see a line of unfinished wood on all the tongues. I always pre finish tongue and groove, and raised panels for that reason.

7/19/15       #3: Kitchen and bathroom cabinet/ vanit ...
Leo G

In bathrooms you want to use a conversion varnish. It's a post catalyzed product. Do you have a booth to evacuate the fumes?

Other then that, use a waterborne polyurethane. It's much safer to use and it is still a tough finish. Dry times will be slower.

7/19/15       #4: Kitchen and bathroom cabinet/ vanit ...
rich c.

Leo is right, BUT, it's the time of year for tough application temps and humidity for water based in certain areas around the United States. Dew points in the 70s around here lately, with temps in the low 90s. It's like Florida is sending it's air to Central IL.

7/19/15       #5: Kitchen and bathroom cabinet/ vanit ...
RobertJ

Look at "TARGET" coatings for waterborne lacquers. Lots to choose from.....they have their own website discussion forum too.

Go with their polyurethane clear for the kitchen.

Next coating would be waterborne by Valspar of MLC.

I would never spray CV onsite without total house ventilation....protect your eyes and lungs!

7/19/15       #6: Kitchen and bathroom cabinet/ vanit ...
JP Member

Thanks for the advice.

I should mention that the house is a new build ( no peoples inside ) and there are no neighbors within 200 yards. The heat and A/C is on.

I usually brush on poly or spray paint or lacquer at my shop for things I build. But I usually build smaller things like a pantry or a stand alone cabinet or two. Or just add pull out shelves.
This is my first complete kitchen.

I have seen unfinished cabinets installed on jobs where they spray them with lacquer ( The fumes ran all of the other crews out of the building ) after they are hung. I was thinking on going that way.

I just need a clear coat though, I will stain my faceframe pieces before I install them.

That and I want to put the boxes up and build large one piece face frames so there aren't all of those mating lines you see in individual box assemblies.

I will look into CV. I will probably have to order a qt online to try out.
How is CV to repair.
I know poly isn't easy like lacquer.

I don't like poly on cabinet doors so much.

The doors I will build and spray at my shop.
It's just the faceframes I want to spray once they are hung.
I have a supplied air respirator that hooks to a air compressor. Set it outside and run the hose in. I was going to set my turbine outside as well or at least outside of my plasticed off area.

7/19/15       #7: Kitchen and bathroom cabinet/ vanit ...
RobertJ

JP

First, Target's waterborne poly is not like convention 'household' poly. They also manufacture a CV waterborne lacquer.

Next, solvent borne CV is available in gallons.

Spraying on site with CV is a non-stopper for me. I spray with a Kremlin 10-14 AAA pump for all on site work. Extremely low overspray. But would never consider solvent CV as a coating that is safe to spray indoors without alot of ventilation.

You have to turn off heat and AC, close all vents and duct work and return supply vents, etc.

Take the time and effort to use a Waterborne Lacquer. If you have an ICA coatings dealer near you, have him give you a sample of their waterborne.

7/19/15       #8: Kitchen and bathroom cabinet/ vanit ...
JP Member

How about this?
http://targetcoatings.com/products/interior-top-coats/em8000-series/
I'm thinking about order a bit of each to try it on some sample.

I don't have to spray lacquer and I want to do a good and long lasting job. I'm willing to change a few things to make that happen.

7/19/15       #9: Kitchen and bathroom cabinet/ vanit ...
JP Member

Oops I posted the wrong link.

How nasty is the CV? I'm going to buy some of each just to try.
Everything is available in QTs by the way.

Do you use the crosslink additive?

I also need something suitable to seal the walls and ceilings. Some walls are blue pine and some walls are western red cedar.
I'll need quite a bit of that.

7/19/15       #10: Kitchen and bathroom cabinet/ vanit ...
JP Member

I also found this.
http://oem.sherwin-williams.com/products/wood/clear-wood-finishes/solvent/catalyze
d/sher-wood-f3-kemvar-varnish

I asked a the local Sherwin Williams saturday and they didn't mention this.

7/24/15       #11: Kitchen and bathroom cabinet/ vanit ...
Henry Member

Try ML Campbell waterborne lacquer, Its a good finish that won't kill you on the jobsite..

Yes I have also seen many paint crews spray lacquer in homes with no ventilation, wouldn't recommend it but it happens every day

11/2/15       #12: Kitchen and bathroom cabinet/ vanit ...
JP Member

I ended up using GF Enduro-var on everything.
Low odor, sprayed a little different but it turned out really well.

I looked into the CV finishes, but I just don't have what it takes to safely spray them.

5/17/19       #13: Kitchen and bathroom cabinet/ vanit ...
Robin Khan Member

Website: https://www.kitchenwarehouseltd.com/

Thanks for the discussion. Actually, I think you have good knowledge about to make the kitchen cabinets. Am I right? But, If you ever want to buy the best kitchen cabinets, doors, and other accessories then no problem. I can help you.

2/23/22       #14: Kitchen and bathroom cabinet/ vanit ...
John Salida

You are really going to spray nitro or precat onsite? That's not healthy for anyone! Expect a visit from the neighbors, or the city inspector, when you put the fan in the window!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!