Re - painting over Conversion Varnish

9/20/16       
D Brown

What products are available to paint over conversion varnish products . Talking about a kitchen that was painted but now they want to change the color or re paint.
Is there a special primer to get adhesion or do you have to strip the old paint off ?

Thank you

9/20/16       #2: Re - painting over Conversion Varni ...
RobertJ

How long to you plan to be in business?
Are you going to warranty the work for 12 or 24 months?

Lots of problems on 're-do's!

Clean and Prime with MLC Clawlock with fresh catalyst.

Mil thickness is your enemy.

Proceed with caution!

9/20/16       #3: Re - painting over Conversion Varni ...
Leo G

You can put almost anything over the CV finish. If you are putting more catalyzed finish over the top you need to be aware of mil thickness. If you are going for oil or latex all you need to do is a good clean and scuff. 220 grit would work well. Then go over it with a Scotchbrite pad or a Mirlon pad to make sure everything is deglazed.

9/20/16       #4: Re - painting over Conversion Varni ...
nick

I did this today on a kitchen island...like Leo said clean thoroughly. I use Dirtex (ammonia cleaner). Spray on, scrub with a Mirka maroon pad and wipe off.
Mask as necessary
Prime if necessary, I've been using bin pigmented shellac for this application 40 years and it works great, but it is flammable so take the necessary precautions if you use it. This job was very clean so I didn't need to prime...I just sprayed 4 medium to light coats of SW's Kem-Aqua Plus clear tinted to a medium grey right on top of the clean CV and It came out beautiful.

9/21/16       #5: Re - painting over Conversion Varni ...
nick

whoops, I left out a step...after masking I sanded with 320 grit using the little triangle festool sander.

9/22/16       #6: Re - painting over Conversion Varni ...
D Brown

RobertJ , Not sure why you ask " how long to you plan to be in business " ?
I have been in business for close to 40 years . My guess is you were not born yet . Do you know so much that you never ask a question ? How do you learn new things ? regards

9/22/16       #7: Re - painting over Conversion Varni ...
RobertJ

D. Brown,

From your question, " Is their a special primer.....etc," it would appear that you had never done this task before.

If so, I stand corrected.

Most shops warranty their work for 12 months, and many do lifetime.

In forty years you have not re-painted a set of cabinets that have CV on them?

9/22/16       #8: Re - painting over Conversion Varni ...
D Brown

You are correct I have never had to re coat CV painted cabinets . In fact I do not do re paints or refinishing . A friend who owns a shop is having a problem with adhesion on the re paint , thought I'd ask some experts for advice .regards

9/24/16       #9: Re - painting over Conversion Varni ...
DanShafner Member

Problems with intercoat adhesion? One cause might be an insufficient scuff giving your friend's finish a bad mechanical grip on the undercoat.

A thorough 320 grit sanding is usually all that's needed.

Mention was made of dry mil thickness. This is an important consideration. If you need to sand through the color coat because you need to deal with the existing dry mil thickness (so that you don't have a coating weight of over 5 dry mils with the new coatings) then you need to prime over those sand-throughs.

Spot priming prevents the new coating from seeping under the old coating which will cause wrinking. If you wrinkle, sand smooth and spot prime over that.

Clawlock is a great catalyzed primer, and it sands nicely.

You can assume what dry mil thickness you have or you can measure it with a dry mil thickness instrument. I would measure.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!