3/13/18       
Mike Member

I'm new to Kremlin and I like to know the extent of clean up from other Kremlin owners. This is what I have. 15C25 with paint filter and the one pass pain heater.
Lately I been spraying solving based white pigment lacquer. My clean up cost me 2-1/2 gallons of lacquer thinner to clean my Kremlin unit as described above. My main question is, do I really need to pump lacquer thinner through the system until the lacquer thinner comes out crystal clear or can I stop when the lacquer thinner is just a little smoky clear?

I just have the above unit and I'm really not into buying other pumps for other colored products. I want to use my Kremlin for white and other color pigment lacquers along with clear lacquers. At times I will be spraying clear lacquers. So I want to clean my unit as best I can and not worry about when changing colors.

Thank you!


View higher quality, full size image (3264 X 1836)

3/13/18       #2: Cleaning my new Kremlin 15C25 ...
cletus joness

so a couple of things

are you running the heater, if not, disconnect the fluid lines from it, that is taking a lot of thinner

also how long are your fluid lines that can also help reduce the solvent usage a little bit

are you using a high quality thinner to clean out your pump, the price typically is tied to its cleaning ability

i use thinner that i have used before if i am using the same catalyst then i pickup the siphon tube and run virgin solvent

just a couple of things that might help

good luck herb j

3/13/18       #3: Cleaning my new Kremlin 15C25 ...
Leo G Member

I have a 10-14 so I'm not sure how different your machine is.

Generally clean up for me is about 1 qt of thinner. Usually I use the thinner from the last cleaning to start the process, get the thicker stuff out of the lines and the pump.

Then run the pump just about dry and fill up the qt container again with new fresh thinner. I've been using MLC Wash thinner which is their least expensive thinner, probably recycled.

Then I run that through the system emptying into another container (which will be next 1st stage cleaning thinner) until I get to a point before the thinner goes below the pickup tube. Then I'll circulate that thinner through the pump for a minute or so. I actually like to introduce a bit of air into the system to induce cavitation which helps clean the walls of the lines and pump. I keep that in the pump/lines until the next use.

3/13/18       #4: Cleaning my new Kremlin 15C25 ...
Jon Member

I have a CAT pump and bobcat gun that I am running with a fluid line heater. I keep thinner in the pump/heater and lines when not in use. When I get ready to spray, I pump the thinner into a quart cup until all the thinner is out chasing the last of it out with the new finish.

When I get done, I pump the finish out, chasing it with the thinner that was in the system previously. I cycle it through for a couple minutes, discard that thinner, then put a quart or so of new thinner in the cup and cycle it through. Stop the pump with the rod down, and leave thinner in the system. That thinner will be used to flush out the next time.

So I get by with a quart or maybe a little less of thinner each time I clean up. The thinner may be a little milky, and more so after sitting overnight. If I feel it is too bad, I will pull some clean thinner in the system before pulling in the new finish if I am shooting clear.

My lines are 25' long and 1/8" dia. I am spraying CV, both pigmented and clear. I have a little trouble with white specs when shooting clear after a pigmented job, but not much. I try to shoot a few parts like backs or drawer boxes first to get rid of any little pesky specs that may come out.

3/14/18       #5: Cleaning my new Kremlin 15C25 ...
Mike Member

Well it seems like I'm doing the cleaning process properly according to what you guys are saying. By the way I have 25 foot line and I use a low quality thinner. Actually last time I used 1-1/2 gallons of settled/recycled thinner finishing up with a gallon of new thinner. Do you guys keep running the new thinner through until it's crystal clear or just a little bit smoky? Recently I seen cheap quality lacquer thinner at Lowe's for about $13 dollars a gallon if you buy the 5 gallon.


View higher quality, full size image (3264 X 1836)

3/14/18       #6: Cleaning my new Kremlin 15C25 ...
Shane

Acetone is much cheaper and flushes the lines just fine..... My operation runs about 20+ kremlin pumps in our manufacturing and we flush between material changes... clear and pigmented with Acetone.... We do as others out of a gallon sized plastic container..... flush with the previous last clean flush until it has circulated through the system well.... then we flush with virgin acetone... of course we are buying in large bulk so acetone for us is about $4 a gallon... Still a big step up from the old days of scrubbing pressure pots when done for the day...

3/14/18       #7: Cleaning my new Kremlin 15C25 ...
JM

Talk to your paint supplier to see if they have gunwash. Its basically just a really crappy and cheap lacquer thinner. Dont use it for your paints, just for cleanup.

We keep two pails below our pump and this is how we clean....
- purge paint till empty into waste drum
- siphon from thinner bucket 1 and spray maybe a half quart into waste drum
- continue siphoning from thinner bucket 1 and spraying back into itself to flush for about 45 seconds
- pull tube from thinner bucket 1 and purge till empty into bucket 1
- put tube into thinner bucket 2 (this is much cleaner thinner) and spray about 1/2qt into bucket 1
- continue spraying thinner2 back into thinner 2 bucket for about 45 seconds.
- leave thinner in pump and lines until next use

This leaves bucket 1 being fairly dirty and just used for an initial pre-rinse and keeps bucket 2 fairly clean. When the thinner starts looking pretty gross, bucket 1 goes into the waste, bucket 2 becomes 1, and a fresh bucket becomes 2.

Been doing it like this for about 10 years with no issues and only takes about 2 minutes. We now have 2 pumps. One for clear, and one for pigmented, but when we were running a single pump, we would just flush about a qt of virgin thinner when switching from pigment to clear.

3/14/18       #8: Cleaning my new Kremlin 15C25 ...
Mike Member

JM, your last line item "leave thinner in pump and lines until next use." Would you say the thinner you left in the pump and lines is crystal clear or smoky but somewhat clear?
Also do you have pump filter and or the one past paint heater?

Thank you for the Kremlin cleanup instructions. I will definitely give it a try

3/14/18       #9: Cleaning my new Kremlin 15C25 ...
Leo G Member

The only time my thinner is clear is when I swap over from conversion varnish to 2K poly. Other than that it's a bit cloudy.

3/14/18       #10: Cleaning my new Kremlin 15C25 ...
JM

Its a little cloudy, some might even say its dirty :)

3/14/18       #11: Cleaning my new Kremlin 15C25 ...
Mike Member

JM, if the lacquer thinner in your pump and lines is cloudy and you been doing it like that for 10 years without any problems at all, then that is good enough for me. That is the information I've been trying to find out and thanks to you I feel safe leaving it a little cloudy in my pump and lines. Great information. Thank you very much!!!

3/14/18       #12: Cleaning my new Kremlin 15C25 ...
JeffD

I use a similar system on my CAT AAA to the rest of the guys, and yeah, the thinner can stay a little murky.... your not spraying it on anything.

Also FWIW I spray out the first pump of new finish into a "garbage" pail. Then I circulate the new finish back into it's pail for 10 or 12 pumps to make sure there's no excess thinner in the finish.

Lastly, as another poster mentioned, when you switch between pigmented and clears your probably going to get some contamination in the lines. The pigmented always seems to leave residue no matter how much I flush the lines. I think the catalyzed lacquer is so aggressive that it actually bonds to the inside of the lines while spraying. After I've been spraying pigmented and switch back to clear I have to make sure I flush the lines again before spraying and then clean the in gun filter to remove the gunk.

good luck,
JeffD

3/14/18       #13: Cleaning my new Kremlin 15C25 ...
Leo G Member

That's the reason I cavitate the thinner, to get bubbles into it which tend to dislodge the finish better in the lines.

3/15/18       #14: Cleaning my new Kremlin 15C25 ...
Mike Member

Thank you JeffD, JM and LeoG for your further replies. All great information!

LeoG, I like your cavitation ideas. Cavitation is what I did the other day but I didn't realize it was practiced. I ran a few quarts of recycled thinner through. I then pump it out until I have air throughout the system. I then re-energize the system with virgin lacquer thinner. While it was cycling through and pumping out the air and filling the lines with new thinner it felt and sounded like a washer machine agitating, if I can put it that way. I just felt it was cleaning in the system better but now that you enlighten me concerning cavitation I can now see in my mind what is going on in the system. I'm going to comprise everyone's notes together and come up with a plan that will shorten my lacquer thinner and time. Thank you!

3/15/18       #15: Cleaning my new Kremlin 15C25 ...
Leo G Member

I use a qt cup to clean. I'll bring the level down to about 10-15 oz and then I shoot the stream from the gun into the lacquer making is spin around. This introduces air into the system pretty consistently.

3/15/18       #16: Cleaning my new Kremlin 15C25 ...
Mike Member

Leo G, that makes sense using 10 to 15 ounces. Leo, does your pump run very fast when cleaning out with lacquer thinner and and using the cavitating method?

3/15/18       #17: Cleaning my new Kremlin 15C25 ...
Leo G Member

I operate the pump around 3psi when cleaning like that.

3/16/18       #18: Cleaning my new Kremlin 15C25 ...
Mike Member

I found myself doing the same thing. About three PSI.

3/18/18       #19: Cleaning my new Kremlin 15C25 ...
Mike Member

Has anyone had better results cleaning the pump with a higher quality lacquer thinner opposed to a cheaper thinner due to VOC ratings?

4/23/21       #21: Cleaning my new Kremlin 15C25 ...
Fergall Member

I remember when I periodically changed my place of residence, often came to order the help of children to transport things, in new houses to constantly make major repairs, because there were no elementary conditions for living. I'm not saying that everything is like this, but it was quite difficult for me to adapt. It is good that there are companies that do this, calculate the weight of garbage, help to make repairs, even make estimates. I can imagine how much the equipment for mixing cement or a mixture for plastering walls costs.

4/23/21       #22: Cleaning my new Kremlin 15C25 ...
Leo G Member

I've been getting my wash thinner from the NAPA paint store. About $37 for a fiver.

4/27/21       #24: Cleaning my new Kremlin 15C25 ...
Fergall Member

Covering pigment 2K-polyurethane primer or solvent-based intermediate coating is not only used for coating or painting. Aliphatic polyisocyanate acts as a hardener. High-performance insulation of wood components is achieved at the expense of small components, but it can be very difficult to remove it from the surface afterwards. It strengthens the wood and has a strong water-repellent effect. I used the services https://www.airconservicingsingapore.com/chemical-overhaul/, everything is described in detail there. You can use it for wooden elements.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!