SAYERLACK Hydroplus AF71 VS Valspar WB C.V

4/2/18       
Robert Member

Has any of you guys tried both SAYERLACK Hydroplus and VALSPAR Zenith WB Conv. vanish and can honestly with no bias give a "clear" comparison diff !?
Thks, Robert

4/2/18       #2: SAYERLACK Hydroplus AF71 VS Valspar ...
MarkB Member

We ran close to a hundred gallons of AF72. Never saw AF71 but this was a couple years back. Liked the metal pails with locking bands. Still have them around the shop.

4/3/18       #3: SAYERLACK Hydroplus AF71 VS Valspar ...
JM

Never heard of or sprayed the AF71, but did spray AF72 and I have sprayed Valspar Zenith. No comparison between the valspar and the AF72. While the Valspar is a pretty good product, the Sayerlack AF72 is a superior product in every way. Sprays out better, sands better, better scratch resistance, better moisture resistance.

The only negative I can say about the AF72 is a minor issue we had when spraying over light colours and using a 2P-10 glue. The glue activator would cause the finish to discolour after a few weeks.

A quick look on the sayerlack website doesnt show an AF71, but does show AFL71 but it says its for flow coating. So not really sure what you are planning to do, but if spraying, I would go with the AF72.

4/3/18       #4: SAYERLACK Hydroplus AF71 VS Valspar ...
Robert Member

First thing.... I believe before going further it's quite important to clear this skepticism on the existing of the SAYERLACK Hydroplus AF71.
Nothing like a credible sheet & data back ground check !
Since there is & will never be absoluteness in life, I'll steer you guys to see the attached PDF so we can go ahead and enjoy further exchanges with out doubt nor though I may have done some mistake in typo or else.
BTW....The attache PDF is an "official" Tech Data Sheet from SAYERLACK.

Now, that's said & cleared.....
TO more direct concern on why I'm seeking info here .....then to know what the pail is made of, .....( no attack, but, let's stick to what is the post all about !!)

TO JM ; I must thank you for this very valuable info you took time to share.
Very much appreciate !
I've been using Valspar and...well, although I've never used this SAYERLACK, but have tried many other, even a few other Italian ones, Valspar to me has been a good choice !!
Now, I've been ask to try this SAYERLACK Hydroplus ( AF71 to me....but maybe same to you as a AF72??....not important for now!!)....witch to this day, never had the curiosety to try !!

I was quite curious to read before hand on ACTUAL SAYERLACK Hydroplus users feed back, as I'm a strong believer on what this WOODWOEB and many other "so-call" pro web forum are here for.....exchanging actual info, experience, knowledge & pertinent data from our work, ( nor in what the pail looks like !!....)

With all respect to all, nothing personal nor attacks intended, just clearing and re-steering the....goal, target !
Sincerely, Robert

Click the link below to download the file included with this post.

Sherwin_williams_SAYERLACK_Hydroplus__AF71_TDS_English.pdf

4/4/18       #5: SAYERLACK Hydroplus AF71 VS Valspar ...
Mark B Member

"Now, I've been ask to try this SAYERLACK Hydroplus ( AF71 to me....but maybe same to you as a AF72??....not important for now!!"

That seems to make no sense. If AF71 is a different formula than the AF72 its crucially important hence two people saying they havent seen AF71. Beyond that the Sayerlack line as offered by SW is still somewhat new in the US and its unclear (but assumed by your grammar) that you may either be outside the US or from outside the US (both of which are wonderful). But if your outside the US or in Europe, you may have access to a lot more of the Sayerlack line that most who post here do.

When you go to Sherwins site, all but a couple PDF requests on their own Hydroplus page return a clear page warning that "no information has been retrieved and if you are in an emergency please call such and such a number". Meaning if your employee drank a pint of material or the material was accidentally sprayed in someones eyes, you have no MSDS.

I really have no idea what your issue is? Tell your supplier to float you a couple gallons for free, bring it in house, and run some tests? Asking for input is great but if you dont get much, well, do your own testing. We were happy with the AF72 for a single part WB clear. We never ran a modifier (which left us uneasy), it was a fine single part finish. Our vendor gave us a few gallons we sprayed it, abused it in house, and went from there. It was touted to us as a single part waterborne suitable (and being used by) flooring manufacturers which immediately launched red flags but that may well have been in EU not in the US.

4/4/18       #6: SAYERLACK Hydroplus AF71 VS Valspar ...
Paul O in Ontario Member

Robert, in the last 6 months I have sprayed both the Sayerlak AF71 and the Valspar WB CV (7702) and my vote definitely goes to the Sayerlak.
Both were sprayed with an old Kremlin 10.14 and MX gun, and although both laid down well, I found the Valspar to need a second coat to get it to flow ot evenly.
I also found the Valspar turned really white with the thicker coat, but it dried out clear, although I had lots of problems scuffing it as it corned, smudged and generally was difficult to work with. I gave it lots of time to dry btw. It reminded me of the old style waterbased finishes that were around about 18 yrs ago. Although it always dried out clear, I always felt it was slightly hazy when looked at in direct sunlight when compared to the Sayerlak.
To put my observations into perspective, I used the Sayerlak on some Birch ply which I was using for cabinets for a washer and dryer. I didn't do much in prep, just sand to 180, dilute first coat 30% with water and then scuff with 320 and a final coat. Came up great, no blemishes, no haze and gave a nice smooth coat. The clear Valspar was sprayed over a tinted version of the 7702 as a walnut shading lacquer by my supplier. It definitely didn't spray as nice, cover as well or look as good and when I talked to my supplier he said they had had too many complaints about it and were going back to the 7500 line as their main Valspar WB clear coat.
It's only a very limited sample I know, but hope my observations help you out.
Good luck
Paul

4/6/18       #7: SAYERLACK Hydroplus AF71 VS Valspar ...
Robert Member

Yes PAUL, this helps very much !
Thanks alot taking time to share this valuable info.
Wishing you all the best

4/6/18       #8: SAYERLACK Hydroplus AF71 VS Valspar ...
DannyB Member

AF71 info:

http://oem.sherwin-williams.com/products/wood/clear-wood-finishes/water/s
ayerlack-hydroplus-af71/

Staring at the SDS/PDS for AF71 and AF72, there are differences (but they don't appear huge at a glance)

4/6/18       #9: SAYERLACK Hydroplus AF71 VS Valspar ...
Jonathan Mahnken

The Zenith line was just purchased by Axalta coatings. Some of the products were recalled at this time. I cant even get it right now. I wouldnt go making zenith products my standard until the transition is complete

4/7/18       #10: SAYERLACK Hydroplus AF71 VS Valspar ...
DannyB Member

Yeah, when Sherwin Williams acquired Valspar, it was required to divest itself of the wood coatings line.

The products are (so far) identical

4/12/18       #11: SAYERLACK Hydroplus AF71 VS Valspar ...
Scott

I have sprayed the sayerlack waterbase solid color, I thought the rep who started me with the product said it was the 71. When I looked at one of the pails the other day it said it was AT99. I will have to ask him about that. The product is fantastic to work with, however he said you may get shear with a smaller pump. I use a kremlin 30:1 and it is great.

4/24/18       #12: SAYERLACK Hydroplus AF71 VS Valspar ...
Gary Member

I spray Sayerlack on a daily basis through an automated spray line, and also out of pressure pots and gravity fed cup guns.

When we switched to a water base, we tried lots of different finishes, and ended up using the Sayerlack. I have found it to be as good if not better then solvent base finishes.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!