Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Milesi Waterbourne

10/12/19       
Tim Kroupa Member

Hi, wondering if anyone has used Milesi waterbourne finishes. I'm currently using their two component product with a Sata RP 5000, 2.0 tip, and just cannot get the product to flow well. I tried thinning, 5% and 10% and at 10% I had good results with the material laying down, but any time that I thin the product I get small pin holes all over my work piece.

Also, I have to be super close with very tight overlaps to get my material on the piece to flow out right. I feel like I'm using a detail sprayer.

Any help would be appreciated.

10/12/19       #2: Milesi Waterbourne ...
DannyB Member

Can you give more details on which product, and what you are spraying it on?

They have waterborne products that range from very thin to very thick.

Hard to help without more.

Also would be helpful to know what temperature and humidity are where you are.

10/13/19       #3: Milesi Waterbourne ...
Tim Kroupa Member

I'm using their 2K topcoat, paint. I'm spraying this in a 400 SF shop, humidity is low right now, temp around 70. Everything has been primed with their universal primer. I'm spraying maple and MDF plywood.

10/13/19       #4: Milesi Waterbourne ...
ron bryze

Most of the Milesi pigmented water base products require a 2.5 tip for best results. The larger tip reduces the need for over-reduction.
Try to limit your reduction to 5%.
Goes on like pudding, dries like glass.

ronb

10/13/19       #5: Milesi Waterbourne ...
Daniel Berlin

Tim,
If this is the HGA11-15 series, then.

A. they make a thinner (LZC97) that you could try.
You can't thin it more than 7% or it will have severe effects on the finish.

Thinning is done as a percent of *weight* of part A.

So if you are thinning based on mixed result volume or something, you are going to severely over-thin it.

B. LTC 5, which should improve flow-out, is also fairly available.

(It can only be used with the water based urethanes, not the solvent ones)

LTC 40 should be similarly available.

(You'd need to call them and ask them which they recommend here)

C. It is meant to be sprayed pretty thick - 4-5 mils. It is also fairly viscosity wise thick.

You probably need a 2.2 tip or to be using a AAA

10/13/19       #6: Milesi Waterbourne ...
ron bryze

If you are using the HKA114 or the HKR114 Milesi recommends a 2.1 to 2.5 tip. Max 5% reduction.

The HGA series is a clear topcoat and is not really intended to be tinted.

Ask your distributor for a copy of the Milesi Product Application Guide. A good read... I wrote it.

10/14/19       #7: Milesi Waterbourne ...
Timothy Kroupa Member

Thanks guys for the input. I'll give the larger tip a try and see what kind of results I get.

When I thinned it, I only thinned it on part A. When you used a larger tip, just curious, what did you have your air pressure set at?

When I spoke with my rep, they suggested 22 PSI. I did that, I was able to get good results at times, but I felt like the high air pressure was almost drying the material.

10/15/19       #8: Milesi Waterbourne ...
ron bryze

With a 2.5 tip I typically used 25 - 30 psi, but it really varies according to how high you hold the gun and how fast you move it. At this size you are capable of moving a lot of fluid thru the tip so you need a little extra air to increase atomization.

When I worked for Milesi I sprayed their water base products in literally hundreds of different shops all across North America and they were very forgiving. Followed the basic rules and the results were always the same...impressive.

ronb

10/15/19       #9: Milesi Waterbourne ...
Daniel Berlin

Note that being water based, temperature has a big effect on the viscosity here, especially towards the lower temps

I pulled out my certified ford 4 cup and the difference in material viscosity between 68 and 78 degrees temp is ~20%.

(which is amore than the viscosity difference for water at those temps)

Of course, it will also decrease pot life (but you can spray wet on wet so ...).

10/17/19       #10: Milesi Waterbourne ...
Timothy Kroupa Member

I spoke with a technical guy at Milesi. One of the issues it seems that I am having is my rep recommended a universal primer for the two component top coat. He let me know, I really should be using a two component primer as well. With my initial topcoat over primer, it is so porous, it forces the paint to dry very quickly, so you will undoubtedly need to add another topcoat. The second topcoat flows out much better. He also said that the HB1 catalyst is an extremely reactive catalyst, and needs to be added a little at a time when mixing into the paint, bc you can shock the product. I made that change, but didn't feel that it made a significant difference.

Ultimately, I was able to get good results on my smaller parts. One piece, a 5' wide x 5' tall x 13" deep locker, I took to my finisher (been in bus for 40 years) and he sprayed with his airless bc it was impossible to do with a cup gun. Ultimately, he felt that this piece was impossible to spray with this product. I've had great results spraying pieces like this with Milesi's single component top coat and conversion varnish as well, but I agree, I don't see how its possible to spray a piece like this with the two component. It dries too fast, by the time you get to the end, the product is dry and the overspray is all over the piece. I'm gonna end up rebuilding this section of my project bc it now has 6 coats of paint on it.

I'd be curious to know if anyone would ever consider spraying a piece this large with Milesi 2 component paint. I attached a picture of my design.


View higher quality, full size image (1540 X 1520)

10/19/19       #11: Milesi Waterbourne ...
Daniel Berlin

FWIW: I have sprayed (with HGA19) and rolled (with HSA6A457) objects larger and more complex than that with 2k Milesi stuff with no issue.

The HGA19 uses the HNB1 catalyst.

I have used their pigmented topcoats (HKR*) but not on objects that large. On smaller ones, drying speed has never given me any issue.

I normally use a pressure pot with a CAT H2O-CPR gun doing the above, but i'll pull out the merkur es when i spray very large flat objects, mainly just to get it done faster.

The only thing i'll note is that I use a precision scale to do the catalyst measurement, because it's very easy to overcatalyze it.

Given what you are saying about dry time, that's really the only thing i can think of that is different. I have the same temperature/humidity you are suggesting.

Note that if you can get it, they have a catalyst for HKR* that is unlimited pot life (HNB11).

HKR* can also be sprayed mono-component. You won't get the same chemical or physical resistance, but the datasheet specifically okays doing this.

That may be useful for you to track down what is going on here.

11/7/19       #12: Milesi Waterbourne ...
Denny J

For any if the two component euro WB coatings you can get better results going to a diaphragm pump. I run Titan 655 sprayers now after years of AAA and they lay it out perfectly. No microshear. Around 700 dollars

If you do high volume then look at the Wagner Cobra. 40:1 pump. Pricy.

7/26/23       #14: Milesi Waterbourne ...
John Member

I am new to spraying Milesi Waterbourne. I am using a 2.5 tip at 25 psi. I thin the product 5% add 10% hardner and 3% retarder. I am having problems with the product drying in the gun while spraying and also drying on the material quickly. The shop has hvac set at 76 degrees. Any suggestions of what I am doing wrong will be helpful.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!