Spraying 30 kitchen cabinet doors in spraybooth with Fuji stage 4 non-bleeder. Spraying color matched off white precat lacquer. Was thinking of a gravity feed but didn't know if the cups hold enough material to be practical for this type of job. If a standard gun is better what would be best. I have the fuji gun that comes with the turbine, but would like to update to a new one. Thanks

12/7/19       #2: Spray Gun Recommendation ...
dar

spraying color with a turbine and getting a nice finish is difficult, i have a kremlin, but i dont use it for pigmented color sprays, I bought a harbor freight gun called the black widow its about 150$ its a sata knock off, is it built as good no does it spray as good yes.they make 2 models hvlp or htf, buy the htf model

12/7/19       #3: Spray Gun Recommendation ...
mastercabman

I would look into a pressure pot or a pump if you can afford it

12/11/19       #4: Spray Gun Recommendation ...
Matt

If all you are spraying is 30 kitchen doors and you won't be spraying much the rest of the year, then even a Campbell Hausefield gravity feed from somewhere like Lowes or Auto-Zone can get the job done for $50-100.

I've owned 3, and still own/use 2 of them for personal stuff. You'll want a 1.0 to 1.5 tip and just dial your fluid flow to whatever gives you good results.

I cannot speak to a Turbine gun, I've neither owned nor needed one, I always have plenty of compressed air to run a gun off of.

HOWEVER.

If you're going to be spraying stuff on a regular basis you really want to get either a 1-gallon pressure pot, or even better an air-assisted airless.

Our shop runs 3 AAA pumps (2 CA Tech and 1 brand new Kremlin).

Having sprayed pressure pots, quart pots, gravity feed....... you simply get a better return on investment with an AAA system and it's not even a close comparison.

The AAA just atomizes better. A pressure pot can spray "just as fast" but you're going to be thinning the paint more, using more atomization air cap pressure, and wasting more material, and possibly spraying more coats.

12/28/19       #5: Spray Gun Recommendation ...
MartyFromKingston Member

As others have already mentioned, if this is a rare volume job, then your existing turbine and HVLP gun should suffice... but as you're already aware, you'll be stopping every 5 or so doors and reloading your cup.
If however such volume finishing jobs will be the norm for you, you have two options as far as I'm concerned:

1. If you're happy with your present Fuji Spray equipment, you can add their 2 Qt. Pressure Pot Assembly Kit #5432, which will reduce the number of times you'll have to stop to refil your gun, but perhaps more important, you'll no longer be carrying around the weight of the finish, as the fluid line coming from the pressure pot weighs very little; your arm will thank you! Another option is to buy Fuji Spray's
compressor-driven 2.5 Gallon Pressure Pot #5470 and use it... that is, assuming your turbine as at least a 4-stage model and you have the technical abilities (it's not that difficult...) to swap out the pressure pot's fittings to fit your turbine hose. The same issue for the fittings will be needed regardless of the make of compressor-driven pressure pot you purchase - be it from Fuji Spray or some other manufacturer.
2. If you want to wean yourself off HVLP and move "up" to slightly higher pressure and improved atomization, Fuji Spray is now offering a suite of reduced pressure, or RP guns (they use the term mid-pressure). I have extensively used their MPX-30 gravity feed gun with my compressor and find that it atomizes extremely well. I also have that same gun with connections to their 2.5 Gallon Pressure Pot #5470, which I use whenever I have a volume finishing job (such as the kitchen cabinet job you described) to do.

If you will be doing such high-volume spry finishing jobs as a rule of thumb in your shop,and if you're willing to make the significant financial investment then perhaps you could consider moving to an entirely different technology such as AAA. I owned a Kremlin AAA system when I was into high-volume spray finishing and can well vouch for its ability to lay down an exceptional finish. CA Technologies has a reputation for their AAA system, at a less steep price point from what I understand, but I can't vouch for them, as they weren't around when I purchased my Kremlin system.

I hope this rather lengthy post helps you with your decision.

1/10/23       #6: Spray Gun Recommendation ...
Eddie Williams Member

For speed and quality of finish air assist, airless is the way to go as it also gives you a fine finish like the paint spray guns or pressure pots. Or if you have an airless you could run with that and a fine finish airless tip, its close to the AAA finish but not quite as good.

Air assist airless sprayers


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!