CV to selfseal or not to (sealer)

2/15/20       
pascal stgelais

Hello

I know I wont get a definitive answer but was looking more of a pros/cons of using CV as a self sealing or with a sealer.

I am currently using mohawk conversion sealer and conversion varnish (both post catalyzed).

I tried both selfsealing and with sealer and got about the same results. I have been digging the forums and both methods seems to have their followers but could not really find a kind of pros/cons of both. Some claim that self sealing is the best way to get the hardest finish and that sealers weaken the finish while others claim that to properly seal you need a sealer otherwise you wont get 100% performance.

I already asked the manufacturers opinions but there might be conflict of interest here since by advertising sealers he can sell 2 products rather than one. but would that be pointless to sell products that weakens topcoats.

Thanks for your answers

2/15/20       #2: CV to selfseal or not to (sealer) ...
Leo G Member

My take on it is the sealer is a weaker finish than the finish is. It is designed to be softer so you can sand it easier.

Pros for using it are usually the sealer cost less than the finish. It usually dries quicker. It usually sands easier.

Pros for self seal are you don't need to have two products available in the shop. You don't have to swap over from sealer to finish. I think it gives a harder finish because you don't have the softer finish under the harder topcoat.

2/15/20       #3: CV to selfseal or not to (sealer) ...
DannyB Member

Leo nailed it.
For self-sealing CV, it's basically cost of finish/energy to sand.

It provides no performance benefit.

There are types of not-self-sealing finishes that require sealer to operate at 100% performance. In these cases, the sealer is often closer to a clear primer, and promotes adhesion.

2/15/20       #4: CV to selfseal or not to (sealer) ...
pascal stgelais

thanks to both of you.

I also had the impression that the selfsealing was harder than the sealer. the first coat of CV was almost unscratchable using my fingernails while the sealer was a bit easier to scratch and lift

2/15/20       #5: CV to selfseal or not to (sealer) ...
Leo G Member

You should be able to scratch the sealer but not lift it. If it's dry-dry and you can still lift it you have adhesion problems. If you are pushing the time and the sealer is still a bit rubbery and you can lift it you should be waiting a bit longer for it to dry.

2/16/20       #6: CV to selfseal or not to (sealer) ...
Jim Clark  Member

The sealer gets a lot harder later on down the road.

2/16/20       #7: CV to selfseal or not to (sealer) ...
Leo G Member

It's still full of stearates to make it sand easy.

2/16/20       #8: CV to selfseal or not to (sealer) ...
dan shaf Member

I would invite everyone to read this pdf document "The Importance of Sealing".

The author of the article was a finish formulator, a consultant to the big factories, and he had many other distinctive titles.

The Importance of Sealing

2/17/20       #9: CV to selfseal or not to (sealer) ...
DannyB Member

The article was written at a time that lacquer was still super popular, and conversion varnishes were just coming into vogue.

It literally doesn't disagree with anything said here.

I bet if you emailed the author this thread, he would agree with every word written :)

2/26/20       #10: CV to selfseal or not to (sealer) ...
G Member

Do you spray a full wet coat then or reduce as the say if using as a sealer? I spray with a AAA graco and was told not to reduce with my unit.

2/26/20       #11: CV to selfseal or not to (sealer) ...
Leo G Member

For the most part I put in a reducer at about 2.5%. I find if I don't I get solvent pop. But that's just me using MLC Krystal.

But that's how I spray all my coats.

2/29/20       #12: CV to selfseal or not to (sealer) ...
Dan drb woodworks

Only time that I can think of using a sealer is if we use the level sealer under Krystal . Otherwise we just use Krystal . We add the flow enhancer in the summer months to prevent any solvent pop

3/4/20       #13: CV to selfseal or not to (sealer) ...
Matt

Always self-sealing. Always.

Invariably, I've found sanding sealers to be inferior to the actual topcoat in every respect except that it kicks over quicker and powders easier than CV topcoat.

Find a good clear CV that cures fast enough for your taste and skip the sanding sealer.

Also consider the benefit of having only 1 product that will take you start to finish. 1 product to order, 1 to inventory, 1 to train people how to spray, and I almost always spray the exact same mix for all coats. I find a thinner amount that works (usually 5-10% with a medium speed thinner) and leave it at that.

I've done this with several brands and have yet to regret it for any reason.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!