4/7/20       
Jenny

I plan to spray some kitchen cabinets. They have solid wood frame and MDF center panel. The result I want is low-luster solid-color cabinets.

I want everybody here to rank or at least point out the worst and the best schedules. It would be helpful to know the reason behind your worst and best pick.

Below are 6 finishing schedules I have observed from multiple professionals.

Schedule 1
2 coats of Vinyl Sealer 1K
2 coats of Topcoat 2K (tinted to exact color by paint supplier)

Schedule 2
Same as Option 1, but with the Vinyl Sealer also 2K

Schedule 3
2 coats of 2K Poly Primer
2 coats of 2K Poly Topcoat
- both primer and topcoat tinted to the same color

Schedule 4
1 coat of transparent Poly Primer
2 coats of white or grey Poly Primer (White for light cabinet colors, grey for darker cabinet colors)
1 coat of 2K Poly Topcoat (tinted to the exact final color)

Schedule 5
Same as Schedule 4, but with every layer 2K

Schedule 6
2 coats of 1K Poly Primer
1 final coat of 2K Poly colored topcoat

When defining what’s best, I generally think about which one will look the best and which one will be the most durable.


View higher quality, full size image (1125 X 1519)


View higher quality, full size image (1030 X 1011)


View higher quality, full size image (1000 X 1295)

4/8/20       #2: Rank multiple 2K poly finishing sch ...
Jenny

I actually asked the professional who did Schedule #4 why he used the clear Poly primer as first coat. He told me that he was trying to “seal the fuzz.” After talking to him, I am wondering why he didn’t just skip the clear primer and head straight to the pigmented primer from his second step. Do pigments in primer decrease the primer’s performance as a sealer?

What do you guys think?

4/8/20       #3: Rank multiple 2K poly finishing sch ...
Jenny

For interior kitchen cabinets, should we use 1K or 2K Poly primer?

I am wondering why we need to harden the primer layer when we usually catalyze the topcoat.

Can we get away with using just a 1K Poly primer? Why or why not?

4/8/20       #4: Rank multiple 2K poly finishing sch ...
Jenny

Does the color of the primer matter that much?

Should primer be white or grey or clear? Or should it be tinted exactly to the color the client picked from the fan deck?

4/8/20       #5: Rank multiple 2K poly finishing sch ...
Jenny

Some professionals only spray 1 layer of 2K poly topcoat. Some spray 2 layers of 2K poly topcoat.

Are the 1-layer sprayers under-cautious or are the 2-layer sprayers over-cautious?

4/8/20       #6: Rank multiple 2K poly finishing sch ...
Leo G Member

1st thing I noticed is you had a schedule with 2 coats of vinyl sealer. As far as I know you aren't suppose to do that. Might just be an MLC thing though.

You are suppose to use a special sealer/primer underneath 2K products. I don't think a vinyl sealer is appropriate. Again, MLC products.

The sealer/primer is a 2 part for MLC, it is catalyzed.

I would do 1 coat of the appropriate poly primer, tinted if you'd like. Then 2 coats of 2K poly. You can do three for durability as most 2Ks don't have a 5 mil limit. MLC Polarion has an 8 mil limit I believe.

4/8/20       #7: Rank multiple 2K poly finishing sch ...
CraigM

I usually spray Schedule 3, I find I get the best finish with 2 topcoats vs 1. I echo the warning of spraying 2k poly over vinyl sealer, pretty good chance it will wrinkle. Anything that's not white/ off white I spray over tinted primer. If you're spraying 2k poly be sure to use an air fed mask and tyvek suit.

4/10/20       #8: Rank multiple 2K poly finishing sch ...
mauricio poli

Answering your questions :
1 - a pigmented primer has the same performance as a transparent sealer. You can use transparent sealer in MDF edges to help avoid absorcion of the finishing with years gone by. 2 coates of primer it ok.
2 - Use 2 K only. Never use 1K under a 2K topcoat, it will wrinkle as time goes by.
3 - Use white primer for white or off-white colors. All the other colors is better to use primer with the same color. It is interisting because if you have a damage in the furniture one will see the same color under. And some colors as orange is very difficult to hide and then using the same color as primer will help.
4 - if the furniture is low gloss one coat of final top coat is ok. if it is high gloss you will need to coats to polish.
Always buy good stuff, in the end it will pay, good material has more quality, hiding power etc.
Good luck!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!