7/6/20       
James Knowles

hello everyone

I am looking at Mirka and serfprep sanders that have that AC/DC conversion units.

For me these are single purpose sanders. I refinish existing cabinets in homes. Part of the process is sanding the old finish, both the flat and the profile. Never white wood. Years ago I purchased a serf prep and the cord between the conversion unit and the sander didn't last. I bought a new cord and it didn't last. So now I need to purchase new sanders as I am growing.

I would like to hear your preferences between surfprep and Mirka?? Looking for quality not price. Air power doesn't work on-site. To much air, to many sanders.

Thanks Jim

7/6/20       #2: advice comparing electric sanders ...
Shane

festool... done

7/6/20       #3: advice comparing electric sanders ...
Mastercabman

Festool?
Sure,if you don't mind spending money!!!!

I have a dts400
I like it but tired of having to spend so much money into it

I'm looking at Surf prep Sanders and Mirka
I used the surf prep and liked it very much

7/6/20       #4: advice comparing electric sanders ...
MarkB Member

Dont leave AirVantage off the list.

We are still running two of the Mirka Ceros sanders with separate transformers and love them which is why I continually look at the Surfprep and the Airvantage. The Mirka Deros comes highly recommended from another contributor here but for whatever reason I really love the dyndabrade envelope for what I do.

I have no idea about bad cords from the transformer to the sander but for one, pertaining to the OP's question, Mirka is out because they no longer offer that format. You are looking at a Surfprep or the AirVantage and thats pretty much it.

3M had the identical tools (likely all come from the same source) for a while but they dropped the electric dynabrade market a couple years ago.

I am in no way, shape, or form, a festool fan. Have had my hands on several and other than a Rotex or a Domino there will likely never be a koolaid tool in my shop and with the Bosch dual mode and the Makita dual mode there likely will never be a Rotex for 2.5x the price.

7/6/20       #5: advice comparing electric sanders ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

mark brings up a great point that both makita and bosh have some really good sanders, and matching dust vacs for less than the festool stuff.

7/6/20       #6: advice comparing electric sanders ...
david zaret

i have a bunch of festool sanders, and as of a few months ago a Mirka Deros and Ceros. both great machines - the Deros has become my favorite sander, even ahead of the festools.

7/7/20       #7: advice comparing electric sanders ...
Kevin Dunphy

Website: http://www.kdunphy.com

I have nerve damage to the hand from using air sanders .

I don't sand like I use to in the old days days but hands down Bosch ROS65VC

https://www.youtube.com/watch?v=cUqJ5QjowYk

Its the only tool manufacturer taken the long term vibration exposer seriosly

7/7/20       #8: advice comparing electric sanders ...
Daniel Berlin Member

Most of the good air sanders have less vibration than the equivalent electric sanders.

For example, the festool LEX3 air sanders have less vibration than the festool electrics.

The mirkas are similar. the electric DEROS 650CV is rated at 3.4m/s2.
The pneumatic PROS 650CV is rated at 3.2m/s2

Additionally the mirka's will give you the current vibration level and let you track daily vibration exposure automatically over bluetooth.

The bosch you are recommending is worse than the DEROS electric or PROS air sanders for the same orbit.

DEROS 625CV = 2.4m/s2
PROS 625CV = 2.3m/s2
ROS65VC-6 = 2.5m/s2

7/7/20       #9: advice comparing electric sanders ...
Kevin Dunphy

Website: http://www.kdunphy.com/

What makes the Bosh special is the motor is separated from the disk  kills most vibration.To my knowledge have not seen any other manufacturer come up with design or approach .Had one lasted 3 years died because I wet sanded 

The problem starts when a sander is used and gets dropped then the disk is out of balance then the vibration starts . A bluetooth app I have little faith

Daniel, have you used any of these sanders? 

7/7/20       #10: advice comparing electric sanders ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

Not sure how you guys afford all those expensive tool geek sanders. They dont necessarily do a better job. I am a believer in quality air sanders for the shop. I use hutchins and dynabrade. but for site work I couldnt imagine any kind of added benifit to using a festool over a bosch or makita.if youre worried about vibration nerve damage wear vibration gloves.

7/7/20       #11: advice comparing electric sanders ...
DannyB

I've actually used all but one for at least a few months each.
I didn't use the Deros, but i did use the 6" electric Ceros.

The vibration numbers are measured at the hand, so whatever effect Bosch's technology has is accounted for in that number ;)

7/8/20       #12: advice comparing electric sanders ...
the google

we just retired two, surfprep 6" electric sanders after 14 months of use. both just quit working. both were returned (one twice) for service under the one year warranty. getting them back from surfprep was semi-painful and easily took a several weeks each time for our three returns. this is why i'm going to trash them now instead of sending them back for repair. i don't know what it would cost us to get them repaired and the process wasn't fun. i'm also not sure how long they would last once we would get them back.

the sanders are pretty awesome when they are working properly. my guys tell me that they take off more material quicker than our air sanders and leave a better finish sanded surface. the elusive, win-win.

i just ordered an airvantage sanders. this sander looks exactly the same as the surfpreps, minus a different color scheme, and they are considerably less expensive. same one year warranty. it arrived today and sands the same as our surfpreps did when they were new. a real joy to use (or so i'm told).

at $350-$500/ea, i would hope to get years of trouble-free service from these, but the technology might just not be there. regardless, if we can sand faster, we're saving money on our labor costs (plus none of my guys really like to sand any longer than necessary). these savings with quickly eclipse the cost of the sanders, so if we have to purchase one a year, then it is still a good deal for the business. plus, it helps with sanding moral. not even pizza fridays help with this.

one the flip side, our dynabrades cost considerably less and have been trouble-free for many, many years. right now, they are enjoying a back-up role.

9/8/20       #13: advice comparing electric sanders ...
Denny J

SurfPrep has great support. I also started out with the older surge sanders and the cords were an issue but the new design is very good. We do cabinet refinishing as well as custom cabinets and we use both of our 3x4 sanders every single day. We also have the 6" orbital and it runs every day as well.

The team at SurfPrep is great and they are some of the better owners I have met. I wouldn't be able to do the things in my business the way I do without their products.

12/19/20       #14: advice comparing electric sanders ...
dave c

I want to do a youtube on my Graveyard of sanders over the past 15 years all-electric. And I have a 40 year old Rockwell flat that still works fine.

1) Festool 6 inch 13 years old.

still works but not on grind mode sent back a few times over the years, it sits.

2) Cervo 1st $600+ amazing just loved it. Worked great for a year then died electrically. Called the MFG had to do a complicated registration and was highly discouraged and insulted. It sits.

3) Cervo 2nd $600+ in a rush and no time for complicated frustrating return processes I bought another. Yes, I love it that much. It sits
4) Cervo flat $500 bought at the same time.
3 and 4) Both died about a year later same electrical issue. I only use them 30 minutes a week on average (hobby) they sit.

5) Bosh 5" $250ish solid does well but not a Cervo and heavy. It's a backup.
6) Festool 5" $600 like most of their tools now (I have most) cheaply made since my first sander and trax saw. It's OK not a Cervo but works. The pads burn out quickly and I'm afraid to drop it unlike my 1st) a tank.

Ranking:
1) Cervo buts disqualified due to poor quality
2) Festool but not as good as the old days
3) Bosh is always solid and I'm sure will figure out a way to beat the other two companies.
Summary: Go to air supplied or buy $70 units that can be replaced. 9 to 1 cost ratio not worth improved performance.

12/19/20       #15: advice comparing electric sanders ...
mastercabman Member

Well...I did it!
Got the 3 x4 surfprep
Black Friday weekend sale
15% off and free shipping
I got the starter kit(sander with dust control connector and whole bunch of sanding paper /pads)Under $500.00
So far I'm loving it.Good ergonomic,good dust control and those sponge sanding pads works great
Will keep you posted on it's performance


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!