Oil primer not drying on stripped sash

11/20/20       
Tim  Member

Website: eastmanwoodworking.com

We are in the process of reworking sash from a library at UVA. Our company has been reworking sash for many years. The sash were built in the early 30’s out of pine and finished with lead paint. Our process is to steam the paint off, then when lead paint has been removed we do whatever restoration needs to be done. We use Sherwin Williams exterior oil primer.
Over the years we have reworked many thousands of windows. This batch is causing problems as the oil primer is not completely drying even after four days. On another project we have in the spray booth the same oil primer dries fine. That project is made from sapele. Moisture content and ph on the sash are good, leading us to wonder what is interfering with drying. We need to use oil paint as it is in the specs and also because the glazing we use has adhesion problems on latex.
Any thoughts would be welcomed; we have a job coming up soon with 700 sash so we need to figure this out.
Thanks

11/20/20       #2: Oil primer not drying on stripped s ...
rescraft

Could there be any residual moisture left after steaming? Any way to check w/moisture meter?

11/20/20       #3: Oil primer not drying on stripped s ...
Tim  Member

Website: eastmanwoodworking.com

Moisture content and ph on the sash are good,

11/20/20       #4: Oil primer not drying on stripped s ...
rich c

Temperature in your shop?

11/20/20       #5: Oil primer not drying on stripped s ...
JeffA

What does Sherwin Williams say?

11/20/20       #6: Oil primer not drying on stripped s ...
Mark B Member

I read a long while back about SW low VOC oils taking a very long time to dry and requiring thinner coats. Not sure if it applies to the primers as well. From memory the solution was heat and airflow. Would seem you'd done far and away enough to have the temp and application right. Any input from sherwin industrial?

11/21/20       #7: Oil primer not drying on stripped s ...
TonyF

Tim:

Are you sure that the wood is pine? Was it kiln dried to begin with? (I know, how would you know that?) Perhaps your steam process has brought resins to the surface that may have lain dormant for years, and if it was air dried lumber, the resins would not have been "set", as they may have been if kiln dried. Cedar might be even more of an issue than pine in that regard.

I've heard old wive's tales of finishers "baking" windows and doors to try to set the resin, but that sounds dubious at best to me.

As a practical matter, perhaps an exterior stain blocking primer like Zinsser might be more effective at sealing in whatever it is that is interfering with the Sherwin Williams primer.

Definitely talk to the rep, whichever product you use.

Good luck.
TonyF

11/21/20       #8: Oil primer not drying on stripped s ...
Chris

Hey, is the primer brand new or a bit older?
Could the driers in the primer have evaporated?

11/21/20       #9: Oil primer not drying on stripped s ...
Adam

Have you used epoxy resin under the paint?

11/22/20       #10: Oil primer not drying on stripped s ...
Adam

Have you used epoxy resin under the paint?

11/29/20       #11: Oil primer not drying on stripped s ...
mike

i previously did not even know this existed but i recently used Corotech oil base paint hardener from Benjamin Moore. It did as it says and dried faster and harder than regular oil base paint. It seems to be able to be used with any brand oil base paint. May be an option for a troublesome situation.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!