Getting Dark Brown Stain

3/15/21       
Tony Member

I am doing some shaker cabinet doors where I want the Rails and Stiles to be a really deep brown like what you see on the edges of the attached image.
I am using red oak and am having difficulty finding a way to get the wood to go that dark a color. I have been working with combos of red mahogany, honey, espresso and Jacobean but can't seem to find a mix that even after several applications will go that dark. Any help is appreciated.

3/15/21       #2: Getting Dark Brown Stain ...
John Member

Attached image?

3/15/21       #4: Getting Dark Brown Stain ...
Tony Member

Hmm. I will try attaching again as well as posting a link.


View higher quality, full size image (640 X 640)

3/15/21       #5: Getting Dark Brown Stain ...
John Member

Get some Sherwin Williams BAC Wiping Stain. You can get almost black with one application on oak. They have several stock colors and will custom mix any color you want. Here's a photo of some rift sawn white oak I did with a custom BAC Wiping Stain.

3/15/21       #6: Getting Dark Brown Stain ...
John Member

Let's try that again.


View higher quality, full size image (2272 X 1704)

3/15/21       #8: Getting Dark Brown Stain ...
Tony Member

Ha. Glad to see I am not the only one having issues with getting an image to post. Thanks John for the tip. I will go over to my local SW and see what they can tell me.

I had another guy post me about using a combination of concentrated black tea to raise the tannin and then using a stain made from steel wool that had soaked in apple cider vinegar for a couple of days. I don't suppose you have tried that or had any thoughts?

3/16/21       #9: Getting Dark Brown Stain ...
Jim Clark

Use a lacquer stain where you can spray
as many coats as you want.

3/16/21       #10: Getting Dark Brown Stain ...
Nicko Member

You need to use a dye first then stain

Nicko.

3/16/21       #11: Getting Dark Brown Stain ...
The Staff at WOODWEB

Any time that you have problems posting images, be sure to let me know - I can help or I can post your image for you. Don't hesitate to contact me - webmaster@woodweb.com.

3/16/21       #12: Getting Dark Brown Stain ...
Scott

Like Tony said, you need to get a toner and spray that on first, then stain over the toner, and then your couple coats of clear over that:

3/16/21       #13: Getting Dark Brown Stain ...
Snaglpuss

I'm with Niko.
Try some aniline dye first maybe.

3/16/21       #14: Getting Dark Brown Stain ...
Scott

Sorry I meant to say I agree with Nicko, you need a toner or a dye to get a dark color.

3/18/21       #15: Getting Dark Brown Stain ...
Robert Member

You can also use a coarser sand paper than you would normally use.

3/19/21       #16: Getting Dark Brown Stain ...
John Member

Yes, you can dye it first and then stain it, or you can use something like SW's BAC Wiping Stain which has both dye and stain in it.

One coat on white oak.

3/19/21       #17: Getting Dark Brown Stain ...
John Member

OK, maybe now.


View higher quality, full size image (1600 X 1200)

3/19/21       #18: Getting Dark Brown Stain ...
Bart

The color you're doing is not much different than what I'm currently doing as far as depth of color. It's hard to get depth like that in one step. What I do is apply twice and sometimes follow up after sanding the first seal coat. Adding either full strength or diluted base color. Which you can also do initially. I'm currently doing a very dark cherry project using GF rtm stains where I diluted the base stain to 70% and apply it twice (wait for it to dry completely) which should give 140% of the base stain color and I'm color correcting after sanding the 2nd seal coat.

my 2cts

3/19/21       #19: Getting Dark Brown Stain ...
John Member

The OP asked how to get a dark brown on red oak. The BAC Wiping Stains will do that. If you want a lot of depth, too, then yes you need to go a different route. However, I'm not sure you can make that happen with red oak no matter what process you use. I'd like to see some photos if it is.

John

3/19/21       #20: Getting Dark Brown Stain ...
Tony Member

Hey everyone, thanks for the responses. I have decided to go the route of a wood dye as that seems to allow me to get the custom color I am looking for and for it to work with the finish. I wanted to ask a couple of additional questions based on the feedback above.
1. If red oak wouldn't work, would white oak be a better selection?
2. To up the game a bit, I am thinking about using an airbrush for applying the dye in order to get some really smooth transition. Thoughts on this?
3. This is for a kitchen so I want a finish that has some depth and will be easy to clean. I was thinking either a satin poly or shellac. OIl would be great but I just don't see it being practical for the kitchen.
Thanks again for all the thoughtful responses.

3/19/21       #21: Getting Dark Brown Stain ...
John Member

Airbrush? Use a spray gun if you want to finish this year. Choose a KCMA rated finish for the topcoat. Shellac would be a really poor choice except for someone who never cooks. And if you want to use an oil based product you could. Waterlox is very durable, but best applied by hand and not something I'd want to do for an entire kitchen's worth of cabinets..

Be sure to test any finish system of interest to make sure it's all compatible. When in doubt, stick with one manufacture's products. .

John

3/27/21       #22: Getting Dark Brown Stain ...
Petes

Saman stains are pretty intense, don't raise the grain, and water clean-up.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!