Hydrocote Amber Additive with Sayerlack?

4/21/21       
Pdub Member

We are trying to slowly make the full conversion to WB finishes and get good systems in place before we are forced to. After trying a few different products, we are very happy with Sayerlack and have been spraying a fair amount of it for a over a year now. While I actually prefer the "WB look" on lighter woods (maple, beech, white oak, etc), it still looks pretty dead to me on the darker woods (walnut, cherry, etc). Maybe I'm just used to the old solvent look and can't get past it, but my clients are saying the same thing when I show them samples of each. So, it doesn't really matter what my opinion is anyway.
We have been discussing coming up with different "formulas" of dye additive (UTC's, transtint) for each wood, but my finisher recalled using the Hydrocote Amber Additive in WB's awhile ago and achieving the look more or less universally.
So, anyone used the Amber Additive with Sayerlack and had any luck? or any problems?...

4/21/21       #2: Hydrocote Amber Additive with Sayer ...
Bart

I don't know about hydrocotes amber but I've been adding orange dye to my GF wb clears for years. And I won't even show a client a straight "clear" on cherry or walnut. I always throw on a diluted GF light brown dye stain for a "clear" topped with the ever so slightly orange tinted wb clear. Otherwise you get the plastic-y look of wb.

my 2cts

4/21/21       #3: Hydrocote Amber Additive with Sayer ...
david zaret Member

i love sayerlack, and completely agree with your assessment of it on lighter and darker woods. not sure that my approach will work for you, but what i do with darker woods is use seal-a-cell to pop the wood, then shoot sayerlack over it. yes, you need to let it dry, but it absolutely sticks, and looks amazing. seal-a-cell will pop like oil, but cure and soak in. and, you can dry it faster with forced air, so a good fan and a little patience and you'll get great results.

4/22/21       #4: Hydrocote Amber Additive with Sayer ...
nicko

i have used a light coat of dewaxed shellac to get a solvent look under WB. It drys fast and sands nice.

nicko

4/22/21       #5: Hydrocote Amber Additive with Sayer ...
david zaret Member

yeah the key here is "light." i had a nightmare of a time with a job once where i put too much shellac on under the sayerlack, and it crazed horribly. i think with a light spit coat you'd be fine, and it's certainly faster than seal-a-cell, but for me, after that experience, i'll stick with what i know works.

4/22/21       #6: Hydrocote Amber Additive with Sayer ...
Nicko Member

Did you use shellac from flakes or seal coat shellac? I’ve done it successfully with both but it’s my understanding that the preservatives in seal coat could cause crazing. That said I never had a problem with a spit coat of seal coat.

Nicko

4/22/21       #7: Hydrocote Amber Additive with Sayer ...
Pdub

Yes David, your thread about the crazing problem made me pretty nervous. Our initial plan was to use the Sealcoat first, but there's some healthy debate on that thread about whether that's a good idea or not.

4/22/21       #8: Hydrocote Amber Additive with Sayer ...
david zaret Member

i used sealcoat when i had the crazing issue. and, i called them and talked to a chemist, and he told me that there's absolutely nothing added, no preservatives, etc. and that the formula hasn't changed for decades. said that the sayerlack was just too strong for the shellac... when i went heavy. just go light, and you'll be fine. or, use seal-a-cell and give it a few days to dry, and you'll absolutely be fine.

4/22/21       #9: Hydrocote Amber Additive with Sayer ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

The shellac will more than likely cause crazing if you actually put enough on to get any color. amber dye will work. the best product ive seen for color enhancement is magnamax H2O. Still never the same as oil...

4/22/21       #10: Hydrocote Amber Additive with Sayer ...
david zaret Member

jonathan - good point, the magnamax is very amber. it's like GF endurovar. personally, i don't like it as much as the sayerlack - i think the sayerlack has a more refined look. but you're right, it's definitely an option, and that stuff is very, very tough.

4/23/21       #11: Hydrocote Amber Additive with Sayer ...
Phil Member

Are you guys using Sayerlack or Magnamax h20 on kitchens? How do they compare to Target Em7000? I've noticed that the Em7000, even with the crosslinker, softens significantly when exposed to alcohol or cleaners like 409. Do Sayerlack and or Magnamax have similar issues?

4/24/21       #12: Hydrocote Amber Additive with Sayer ...
david zaret Member

phil, i'm yet to use magnamax on any casework - my partner used it on some a while back, and i didn't love the look, so i'm sticking with sayerlack. on the number of kitchens i've done with sayerlack, i've never heard of, or seen any issues at all with the finish.

4/27/21       #13: Hydrocote Amber Additive with Sayer ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

Ive used enduovar the magnamax H2O a few times. as David mentioned its tough stuff, ambers heavily,even more so than endurovar, or hybrivar from target, but doesn't necessarily dazzle the eye. It also has no "hang" so spraying vertically is a pain. the recommendation for sayerlac is a good one, but I cant get it in my area. Chemcraft Aqualux uniclear has been a really good choice for me. Has the clarity of the newer style sayerlac and some others. makes Target and GF look a little lifeless in comparison and it is pre catalyzed. tough stuff. Has an AWI TR3 rating. I get it through Wurth. They also sell the Magnamaxh20 and Milesi 2K

4/27/21       #14: Hydrocote Amber Additive with Sayer ...
david zaret Member

hey jonathan, thanks for this. i'm looking at the chemcraft site - which waterborne topcoat specifically would you recommend trying as a test? they have quite a few.

thanks!

--- dz

4/28/21       #15: Hydrocote Amber Additive with Sayer ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

The Uniclear is what I use. I haven't even tried the other clears, and I think you will find that many suppliers wont stock many of the others. The Aquaprime and Aquaset are really tough products also, but they dont have great flow, so AA or Airless are best with those.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!