Waterborne help

3/6/23       
nicko

Hi
I am spraying some Target Coatings raven black pigmented lacquer.
I am happy with the product but the biggest needle/nozzle i have is 1.7. I have thinned it up to 10% with water and it runs about 45 seconds thru a Ford cup. I am spraying a box coat on some cabinet doors and when i lay down the product it looks great but when it dries i can see some tiger stripping. I am thinking that the product is a little too thick for the 1.7 but the instructions say to thin up to 10% so i don't want to thin more than that.
Would adjusting my spray width, Volume and pressure be the thing i want to do? I have just been spraying with the volume wide open and the width wide open at about 25 pounds of pressure.
The gun i am using is a CAT gravity with a HVLP and a CPR air cap.
I have been using the CPR. Would it be better to use the HVLP cap?
I am out of the lacquer right now and my delivery isn't due until Wednesday day the 8th so I was trying to get some info to think about until i get the product so i can experiment.

Thanks.......nickko

3/6/23       #2: Waterborne help ...
herb johnson

my guess is you are unders atomizing the coating or your lap stroke is off. i would starting increasing your pressure at ten 10 psi at a time on a piece of cardboard white preferrable and examine your results.

good luck herb j

3/6/23       #3: Waterborne help ...
Nicko

Thanks Herb
I’ll try when I get my finish on Wednesday. It’s definitely user error.

3/6/23       #4: Waterborne help ...
Mastercabman

I have sprayed target coating before
That CAT CPR shouldn't have any problems spraying it
Is it cold where you are?
Are you mixing the material thoroughly?
Either air cap should be just fine
Sorry I don't have much to say
Hope you resolve it

3/7/23       #5: Waterborne help ...
Adam

I did a 10 second look at your gun. It needs 11CFM @ 29psi with the CPR cap. I had a look because 25 is really really low. Do you have 11CFM? Where are you measuring the pressure? The biggest upgrade I ever made to my gravity HVLP guns was switching to a 3/8" air hose and having the air pressure adjustment/gauge on the gun. Instantly everything sprayed better.

3/7/23       #6: Waterborne help ...
Mastercabman

Adam makes a good point
CFM on a Compressor is something that many people overlook when using those type of guns
If your Compressor doesn't put out enough cfm,then psi drops and you end up with poor atomization
Just something to think about

3/7/23       #7: Waterborne help ...
nicko

My compressor puts out 15.1 scfm @ 40 psi and 13.5 scfm @ 90 psi
I check my pressure at the gun. I guess I need to do some test panels and play with the adjustments. I just opened things up and started spraying because that's how I spray my solvent based CV.

3/7/23       #8: Waterborne help ...
nicko

Just to add to my above post. I do use 3/8 hose and I have the larger high flow fittings on the hose and gun.

3/7/23       #9: Waterborne help ...
Adam

Sounds like your setup is good. You should use distilled water for reduction. Stir it in with a stick really well. Keep the pressure at whatever the max they rate the HVLP(40psi?). I would run everything wide open. The low pressure air caps don’t work with every product.

Target has great tech support, give them a call.

3/8/23       #10: Waterborne help ...
nicko

Thanks for all the help. I am waiting for my finish to arrive any time now so I will follow up later.

3/8/23       #11: Waterborne help ...
Nicko

Thanks for all the help. I turned my air pressure up to 30 from the 22 to 25 I was spraying at. I warmed the finish up some by just letting some heat blow on it for awhile and made sure I was more precise on my overlap. I did a box coat on all the cabinet doors and I’m super happy with the results.
Now if I could just keep dust particles from settling on the finish……..
But that’s a whole nother thread.

3/8/23       #12: Waterborne help ...
Mastercabman

Glad you got this figured out!
That CPR gun is pretty sweet!
I like to keep a fan at low speed blowing air across the top of the painted surfaces

3/8/23       #13: Waterborne help ...
herb johnson

glad my suggestion worked out, you even improved upon by increasing air pressure by only 5psi instead of the 10 psi i wrote about. good move!

good luck
herb j.

3/10/23       #14: Waterborne help ...
Craig Caughlan  Member

Website: https://www.instagram.com/craigcaughlan/

I use a Graco AirPro with 1.8 tip on my WB products (Milesi,Ilva, Solrac). I'm curious as to the opinions from someone who has used both guns.

3/10/23       #15: Waterborne help ...
Bill Colligan Member

I would suggest putting Target's clear urethane (EM9300) over it. I have used the raven black and the durability as a stand alone is poor. I did an entire bedroom set 2 years ago and there are many areas worn through to the primer. I plan on using the black again and top coating with the 9300. I did that on a pigmented bedroom set a few years ago and it has held up great.

3/10/23       #16: Waterborne help ...
Nicko

I have some Sherwin Williams water white solvent conversion varnish. Would it be safe to spray that over waterborne? I would light scuff with a maroon pad and do two thin coats. Thoughts.

Thanks.

3/11/23       #17: Waterborne help ...
nicko

This is a no go as per Jeff at Target.

4/5/23       #18: Waterborne help ...
Bart

I use a 2.2 in my FLG-4 for all my WB. Mostly GF including there white undercoat which is really thick. I just cut with leftover topcoats and pinch of water on cold days. BTW, for years I had 3/8 hose but then I realized the fitting from the tank to the output on my 5hp 220 Curtis-Toledo was 1/4".....doh. Puts out 13+ @ 90lbs. So switched my hose to 1/4" and didn't notice any difference.
And I haven't tripped over it once since switching...lol
PS you may want to consider a pressure pot system for more viscous material.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!