Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Infared/heated curing

6/12/23       
Jim Knowles

I would like to make my own infared or heated batch oven for curing cabinet doors on a door rack. I want to place it in an 8' wide trailer and take it on site.

Any of you make your own? Any experience with rapidly curing the finish? I know systeams that I can buy. But they are pretty expensive.

Right now with my solvent CV doing doors is a 3 day job....waiting for the cure to be dry enough to flip over and handle....

Thanks for your input!!

6/12/23       #2: Infared/heated curing ...
Jonathan Mahnken

infratech makes all different size and configurations of lamps that you could hang or put on a rack inside your trailer

6/12/23       #3: Infared/heated curing ...
RichC

You want to transport doors down the highway on thin steel cantilevered support wires? Could you please put a go pro camera in there for the first trip? I'd love to see a video when the driver has to slam on the brakes!

6/12/23       #4: Infared/heated curing ...
Jim Knowles

Thank you Johnathan, I will check it out!

RichC. Yes that sounds pretty sad..!!

No, I want to cure them in their(clients) driveway. That's the whole point of the onsite trailer. I would love to do the doors both sides and rehang them in the same day.....

That's what dreams are made of....

Thank you! Always looking for a better way! Love all of your help.....!

6/12/23       #5: Infared/heated curing ...
Bill

We have many IR heaters.
Infratech makes 110V IR heaters, to find them easily search body shop supplies. They come on a stand, they are not terribly expensive.

To get a large surface area of heat you need 220V, higher amperage, multiple units. That is not a system that would work onsite.

If you are going to set up a large high voltage system call Infratech and deal with them directly. They will baulk because they don't want them to be in a paint booth.

Good luck!

6/12/23       #6: Infared/heated curing ...
Leo G Member

Never had a marking problem with CV. 2 coats on the rear and one on the front, wait overnight and 2nd coat on the front (back-front-back then front).

They have infrared heater panels that go into a ceiling grid system that usually run about 750W each. You could box them to get them closer to your doors. Most CVs don't like more than 110ºF for curing. And you wouldn't put the wet door under the heat. Wait until it fully flashes and then you can heat cure it.

6/12/23       #7: Infared/heated curing ...
Jim Knowles

Leo G
Thank you for this response and the many you have made over time.

So very interesting you are spraying the back and then on the same day....they are dry enough to roll over "with out marks" spray the front..then 2nd coat the back....

So how much time does the back cure before you roll do the front? And do use uv lights or heat with fans??

Thank you Leo! This is great information!
After you second coat the the fronts, how long before you reinstall?

Much appreciation

Jim

6/12/23       #8: Infared/heated curing ...
RichC

I wonder what the neighbors will think as you vent the conversion varnish 75' from their front door? Or even closer by their kid's bedroom windows.

6/13/23       #9: Infared/heated curing ...
Leo G Member

I use MLC Krystal. I spray the back and wait about 45-60 minutes depending on temp. I flip over and spray the front and wait the same time. I scuff the back with 320 and then spray it again.

Usually I'm doing this with 15-30 doors so by the time I finish the last side I'm ready to to start on the next round.

The next day I scuff the door front and spray the 2nd coat. I usually put it on 6-7 mil and 2 coats is pretty close to getting 5 mil dry.

I almost always consider the back of the door a B quality side. I always try for perfection but if there is a slight imperfection on the rear of the door I don't worry too much about it.
6/13/23       #10: Infared/heated curing ...
gary

There are some hanging systems available. With them you can spray both sides at once and cut the dry time in half and not worry about marks from the drying racks.

6/14/23       #11: Infared/heated curing ...
Mastercabman

I have the same set up
6X12 trailer as my on-site spray booth
When I used CV I would do what Leo G said
CV dries pretty quick
On the other hand if you're talking about precat then I can understand why you would want to speed up cure time!
I now use waterborne and I'm still trying to adjust!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!