Chemcraft Conversion Varnish

2/24/19       
Garen Pletzer

I sprayed SW conversion varnish for a bunch of years. Then picked up a distributor with chemcraft. Always wanted to try them. I have been using the conversion varnish and I dont seam to think it has the same hardness as the SW water white CV. Any thoughts on this? I have been using the correct cat and the correct ratio for mixing. I had to switch back for this job i am working on. I needed that harder finish. I also have tried Chemcrafts poly finish. was alright but more expensive. I am doing something wrong?

2/24/19       #2: Chemcraft Conversion Varnish ...
Tyler

That doesn't sound right . Which CV are you using? We use plasticolor, and plastofix light it is a really hard and resilient finish.

2/24/19       #3: Chemcraft Conversion Varnish ...
Garen Pleter

using the chem24 sealer and top coat.

2/25/19       #4: Chemcraft Conversion Varnish ...
Tyler

The chem24, as is in its name, takes longer to cure than a conventional CV, while also giving you a full 24 hour potlife. If you try the plastofix light you will not see the initial softness you're dealing with right now, but will go back to a more conventional 8-12 hour potlife

2/25/19       #5: Chemcraft Conversion Varnish ...
Gerry

We use the Chemlife 24 and don't find it soft at all. Are you insuring the drying room is at 70 degrees. If it is not warm enough it will never get hard.

Also I would recheck your cat mixture. Chemlife 24 is a very durable product.

2/25/19       #6: Chemcraft Conversion Varnish ...
dub

I spray SW Kemvar CV and also tried Chemcraft's CV for a couple of projects and found it to be less durable. I actually have two identical cabinets in my house with one topcoated with SW and one with Chemcraft. They are in different locations and may be subject to different amounts of wear, but the Chemcraft one shows the dings/chips, etc. more than the SW.

I also think the SW pigmented conversion is more durable when self sealed rather than using a primer/surfacer.

dub

2/26/19       #7: Chemcraft Conversion Varnish ...
Garen Pletzer

I have checked the amount of cat and room temp is above 70. Have air makeup and spray booth. I have samples here from over a year ago and it still not as hard as my desk that has the SW. I will try the plastofix. The chemcraft seams to lay down great but if i dont get a hard finish it doesn't mater. Thanks for the tips.

2/26/19       #8: Chemcraft Conversion Varnish ...
Jim Clark  Member

Sounds like bad activator or not enough
added.

2/27/19       #9: Chemcraft Conversion Varnish ...
mauricio poli Member

Hello !
The best way to compare those materials is to prepare a big panel, and apply side by side both products at the same time, same viscosity,same coats, same temperature
Wait 3 day and make the coin test.
Wait 30 days and make the test again
Hugs

12/11/23       #10: Chemcraft Conversion Varnish ...
Walter Kerr

Try the E-Var Conversion Varnish 421-80xx from Chemcraft. 8-hour pot life with 10% catalyst 873-0870. We have sold and used this for many years.
Ther is a vinyl sealer that goes with it, or it can be used as a self-seal 2 coat system. Water clear and extremely durable.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!