Mdf shaker doors

8/13/24       
Jonathan Mahnken

Ive been making mdf( Weyurhauser/plum creek brand only) doors for a little over 2 years now, and Im struggling to perfect the process of pre sanding, coating and final finish. I am spraying all WB primer and topcoat by ESC coatings. I rout both sides of the doors so I dont have to worry about cupping. the routed centers are then presanded with 150 grit on a dynabrade 2/3 sheet rectangular sander. At this point I have tried several different combinations of how many primer coats and sandings between coats, followed by two topcoats with a light to moderate sanding in between. My issue is that on medium to dark colors I struggle to stay under 4-5 coats of material and at least two sandings before I get what I consider to be a good finish. At this point paint buildup in the corners is also an issue. I would like to drop the number of coats to a consistent 3-4 coats, or less if someone knows something I dont... Any Ideas?? Also, switching to solvent primer is not an option for me

8/13/24       #2: Mdf shaker doors ...
mauricio poli

You can apply one or two coats of a 2K PU high solids transparent sealer only in the routed/edges. With high viscosity, without thinning, with a 1.8 or 2.0 tip.
After dried, you can sand it and continue with your WB process.

8/14/24       #3: Mdf shaker doors ...
JM

I know you said you didnt want to hear it, but 2K poly is the solution. We sand routed panels and profiles with 320, then 1 prime coat , 1 top coat, then add a 2nd topcoat just on the faces just for a slightly improved finish. 2nd topcoat would be optional depending on your finish standards.

8/14/24       #4: Mdf shaker doors ...
Jonathan Mahnken

Thanks its just that the area of california that im in doesnt allow solvent finishes. Looking for Ideas about sanding into square corners. grit process...
I think there are a couple of wb 2k primers out there I could try. Over all just trying to make fewer steps out of what seems to be a many step porcess.

8/14/24       #5: Mdf shaker doors ...
JM

Also options for 2 piece mdf where a 1/4" panel gets inserted into the frame. Drastically reduces finish time on a flat panel.

8/14/24       #6: Mdf shaker doors ...
Jonathan Mahnken

JM do you have an example of how this is done? I havent tried this because ive been trying to reduce the amount of handling and steps involved because I am a 1.5 man operation

8/14/24       #7: Mdf shaker doors ...
JM

We do it with our shaker doors. We route a pocket on the back thats just a little over 3/8inch deep (same as you would to insert glass). We then insert a 3/8 panel that is basically press fit. It eliminates warping from single side machining and is a breeze to finish. Obviously more machine time and some assembly time, but the finish is amazing, and no warping.

No experience with other methods, but here is a youtube for an option for another way to do it.

https://www.youtube.com/watch?v=dmEbKOq1mgc

8/15/24       #8: Mdf shaker doors ...
CraigM

I spray tons of routed mdf doors (2k solvent though). I sand the raw MDF center panel to 320 until it's almost burnished and use a high solids 2k primer, wet on wet. It does a great job filling pitting and no grain raise. I know a lot of the WB guys prefer to use a wb 2k primer because they find it helps lock down the grain. Look into Sivam, Renner, Envirolak, Icro ect, I hear good things about all their WB 2k primers. A lot of california guys are using it so it should be pretty easy to source.

8/17/24       #9: Mdf shaker doors ...
Jonathan Mahnken

Craig, what type of sander are using and what is you grit process?

8/19/24       #10: Mdf shaker doors ...
CraigM

Jonathan, I usually receive the doors finished sanded to 180. Most of the shops I spray for use good quality mdf for their routed doors, so they aren't terrible for pitting and fibers. I use a mirka 3x5 to sand the center panels 240/320 and almost burnish it. Then 2 coats of solvent 2k primer (Sivam) wet on wet and that locks everything down and fills the majority of the pitting. I've talked to a few guys that use wb primer and they get better results if they sand between first and second coat if primer

8/28/24       #11: Mdf shaker doors ...
Frank Garrido  Member

Website: http://www.cabinethero.com

Are using the ESC prime master? Also the pre sanding of 150 is to rough ,
Should be done at least 220.
MDF first coat of primer should not be heavy , a light coat is best. Can either sand this to remove some of initial
Rough texture after 30 to 45 minutes blow off sanding powder . Apply 2nd coat , even wet coat , wait at least
1 hour before sanding 70 degree temp,.
Apply top coat ESC Spray master or ConVar .
You can also contact Rick or Zack at Colorama paint store in San Diego , Rick is a biochemist who is designed these coatings knowledable and will def take time to guide you through this .
Hope this helps you

8/28/24       #12: Mdf shaker doors ...
Jonathan Mahnken

Frank, yes. Using the primemaster. Im beginning to see that the 150 is too rough. In the beginning of making cnc shaker doors, my machining was a little rough, and required heavy sanding. Im not sure how familiar you are with ESC products, but over the last two years ive witnessed a chemistry change in the lineup. The topcoats, including the clears, seem to be drying much slower than previously. I was able to compare with older product that I still had in stock. I've also had issues with colorant overload on dark colors. This resulting in even longer cure times and on a couple of occasions cratering. Positively, the primemaster blocks stain better than any of the other WB primers that I use, and sands well too. It doesnt seem to isolate, or lock down the grain as well as some others that Ive used, namely chemcraft aquaprime and mlc agualente. Ive had good service from ESC and they have an extremely complete line which is very attractive for me, but product consistency has been a little off with the topcoats. Another positive is that once cured all of their topcoats are super durable. More so than many WBs that ive used


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!