Rubbing out a lacquer finish

5/16/25       
Rick Hensley

I am refinishing a fine coffee table. I have many coats of lacquer (low voc gloss). I have sanded dry 320grit then wet sanded from 400, 600, 1000, 1500, 2000, 2500, 3000. Then wet apply 2f and 4f pumice and last rotten stone. The finish is slick as glass but I can still see my hand strokes. Many applications of rotten stone still see strokes. Help don’t know what to do.

5/17/25       #2: Rubbing out a lacquer finish ...
Leo G Member

Possible that the lower grits weren't sanded out enough to remove the scratches. If that's the case you may need to go back to the grit above what wasn't removed.

5/17/25       #3: Rubbing out a lacquer finish ...
Chemmy

Your mistake is using the 2F pumice which in use, (as compared to or with 600 grit w/d sandpaper) is coarser..!! Even 4F pumice is coarser than than all of the finer grit papers you used.!! All you've done or accomplished is reintroducing larger deeper scratches to your 3000 grit sanded surface, a surface that at that point, could have been easily polished with auto compounds available at any automotive paint supply store across the country, best used with a buffer ( electric or pneumatic) to buff out the finish after applying the polishing compounds to the finished surface or to the buffing pad itself. You can polish by hand, but it is very difficult to achieve a truly polished glass like surface that is uniformly stunning as a piece of glass would be or is.! If further info is needed just reply.
Chemmy

5/19/25       #4: Rubbing out a lacquer finish ...
shenendoa


Rick,

Leo has a valid point. What I learned to do to avoid not fully removing previously made scratch patterns was to sand the next higher grade of paper perpendicular. or at right angles, to the lower grade just used. One can then visually confirm that the preceding scratch pattern is removed. I found this most valuable with polyester finishes.

Also, Chemmy is correct.

5/19/25       #5: Rubbing out a lacquer finish ...
RichC

Move from the 1950s methods up to current times. Go to an autobody supplier and get current on how to polish. Mirka Abralon is a great place to start.

5/19/25       #6: Rubbing out a lacquer finish ...
Leo G Member

You mean "traditional" methods.

5/19/25       #7: Rubbing out a lacquer finish ...
Chemmy

"LOL"..... 😂😂😂
MIRKA has great products, but they can't polish everything.!
For example, heavily carved furniture, or other ornate surfaces.
This requires a lot of hand polishing with various soft to hard felts and other specialty cloth and tools, together with compounds ranging from course to sub micron polishing attributes. But for flat and not to curved surfaces, MIRKA works fine, so does micro-mesh, and a few others.

5/20/25       #8: Rubbing out a lacquer finish ...
RichC

What the hell Chemmy. Where did the OP say his coffee table was heavily carved and ornate? I suggested he just start with Mirka. No where did I say it's the only way to polish lacquer.

5/20/25       #9: Rubbing out a lacquer finish ...
Chemmy

???...that was an opinion, my opinion on polishing any or all surfaces...it sure wasn't a comment on your suggestion, I've used MIRKA for a couple of decades along with Micro-Mesh, and a couple of others that use fine grit sheets and disc. I will try in the future to be more " specific" as to my comments so as to not unintentionally offend you or anyone else, or maybe not even posting anything else ever. I'm not tied to this forum to the extent I feel I have to be cussed out over a post. So enjoy your stay with woodweb, I only came back here because of a particular post that no-one was answering. I don't need any information or help from anyone on this site, I can let everyone struggle on their own or have others here give their two cents. I will keep my two cents to myself and just continue to help those who contact me for help.
Have a good life..!

5/21/25       #10: Rubbing out a lacquer finish ...
starbucks

Settle down everyone. No one needs to get their panties in a bunch over a woodworking forum.

5/21/25       #11: Rubbing out a lacquer finish ...
RichC

I really just took a guess at what this meant. You have to admit it's open to personal interpretation.

"LOL"..... 😂😂😂

6/9/25       #12: Rubbing out a lacquer finish ...
Charles

" I don't need any information or help from anyone on this site, "

I've never met anyone that knows everything and never needs help on a subject, I feel blessed to have read this post


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!