Blushing troubles

7/13/25       
Keith Farr

Im a cabinet shop owner with a finishing department relying on a employee who has much experience in finishing but is having Blushing issues. He shoots AMARIUM precat conversion lacquer over our lacqeur painted cabinets and our stained cabinets. We have a knotty Alder job that was stained , sealed , glaze applied , then sealed and fished that started blushing about 10-14 days after it was shot.( cabinets are allready installed ) It has been very humid here in Texas for last month. We installed a 14 x24 Colmat spray booth about a year ago. For years we just spryed in a large room with exausht fans and such with no problems. and we never have problems except with stained cabinets. We have been bringing doors back to shop and trying Mohawk blush remover in a rattle can with limited success Any suggestions?

7/13/25       #3: Blushing troubles ...
Leo G Member

Are you staying within your brand system or are you mixing different products to get your final outcome.

Using oil based stains under modern finishes can cause issues. Usually you'd use the recommended stains so you stay within the system.

I'm just noticing you said you coated with lacquer and then overcoated with precat. Nitrocellulose lacquer is know to blush while most modern pre and post cat lacquers won't even under extreme humid conditions.

7/15/25       #4: Blushing troubles ...
FM

I would not call it blushing if it’s doing weeks afterwards. Blushing is immediate. My experiences guess? You have separation between two coats. Have you blue taped a section that is effected, cut a grid pattern in with a razor blade and pulled the blue tape to check for adhesion?

7/17/25       #5: Blushing troubles ...
Jim Kolar

Is your stain solvent or water base? We currently sent a job out unfinished, and the painter used old masters stained and then top coated with evo water base clear. Having issues now with the finish. The dry time was 48 hours.

Tough spot to be in feel your pain.

7/18/25       #6: Blushing troubles ...
Pete

My guess is the conversion lacquer is reacting to the coat below it. Can you tint the proper sealer to go under the conversion?

7/26/25       #7: Blushing troubles ...
Keith Farr

I think we have isolated the problem. These are alder cabinets with Sherwin Williams oil stain on some units and then Old masrters oil stain on other rooms ( we get the problem on both stains so we dont think its the stain) we seal with laquer sanding seal then GLAZE with oil glaze , Wipe most of the glaze off , then several coats of final laquer . We have done some test pieces where we glazed and sealed within an hour and also pieces that were allowed to set overnight before finishing over the glaze. Both pieces failed . We have done many jobs WITHOUT the glaze with same process with no problems ( various woods). Oddly we have done this stain, glaze seal process for years with no problems. My own personal home has gray stained alder with so much glaze it looks like it was brushed on. Did it four years ago no problems . My former inhouse finisher of tweenty years has been coming in trying to help us figure it out and he swears the Amarium laquer smells and feels different than it use to. Of course Wood finisher depot rep says nothing has changed. Its definately not adhering because you can scrape some areas off( not all areas) with hard fingernail pushing. currently we are stripping down to the sanding sealer with laquer thinner thru the glaze as much as possbile and then recoating and hopeing for the best. Any suggestions would help Thanks (NO MORE GLAZE OFFERED FROM MY SHOP FORESURE! )

7/26/25       #8: Blushing troubles ...
Leo G Member

I use MLC products and with the older glazes they require you to sandwich it in between a coat of vinyl sealer. So stain, vinyl sealer, glaze, vinyl sealer then top coats.

The have a product called Amazing Glaze that is sprayed on and dries to a powder consistency. You can spray that on a conversion varnish and wipe of to get the look you want and spray your clear. But you can't use weaker products like precats or straight nitro. It'll eat into it and you won't be able to removed it.

7/26/25       #9: Blushing troubles ...
FM

It is hard to offer solutions without a full finish schedule/recipe including products used. Without that information its wild a** guesses at best.

Are you sanding before you glaze? My best guess is you have no bite between your glaze and the coat underneath it or the coat on top of it. With most products that are catalyzed you are going to have to sand on one side of glazing. Without out that sanding you'd have trouble even without throwing a weak point in (the glaze). I have very rarely ran into this but with the right products time between the coat underneath the glaze and on top of the glaze might be an issue also. You have to get some bite on the glaze. If you wait overnight on the glaze and don't topcoat it can you scratch it off easily?

9/9/25       #10: Blushing troubles ...
NJ Furniture Mart  Member

Website: https://www.njfurnituremart.com/

Generally speaking, blushing indicates trapped moisture, particularly when the humidity is high. Controlling the humidity, ventilation, and temperature is essential even in a booth. To slow drying and let moisture to escape, try warming the lacquer, adding a retarder, or dehumidifying the booth. Professional blush retarder spraying is more effective than rattling cans for installed cabinets.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!