Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Clear Coating Maple without Yellowing

12/12/25       
Michael R

What preparation must I follow in order to clear coat bright hard rock maple without changing its original color? Whenever I use for a sealer under my clear coat, I get a little bit of yellowing. Is there a way to keep the original unfinished wood color? Thank you.

12/12/25       #2: Clear Coating Maple without Yellowi ...
Chemmy

Use Acrylic coatings, SW, Delta, or others that are acrylic/cab coatings for indefinite non yellowing.!!

12/12/25       #3: Clear Coating Maple without Yellowi ...
Michael R Member

Thanks Chemmy!

I have been using Sherwin Williams Gallery clear coat, which is an acrylic and I still get a slight yellowing after spraying. Just to be clear, I'm not concerned about it yellowing over time because I am using an acrylic, I'm just trying to keep the bright Maple bear wood color using a clear coat. Are the products that you are recommending (solvent-based) designed to completely stop any yellowing? I know in your first reply to me, you used the words "indefinite non-yellowing. Should I expect a slight transformation after three coats, or should I see through it as if it were glass?

12/12/25       #4: Clear Coating Maple without Yellowi ...
cris

Whitewash then clear. you will have to experiment with it. We did this years ago and it worked great.

12/17/25       #5: Clear Coating Maple without Yellowi ...
Michael R Member

Cris, you nailed it! I did a test and the results are exactly what I was looking for. I got a quart of Zar Beach House #139 and applied to the maple let it dry, then two coats SW Gallery series acrylic. The Maple did not lose its bright white natural color and you can't even notice that there is a white wash stain on the maple. Thanks again, this one will go down in the books.

12/22/25       #6: Clear Coating Maple without Yellowi ...
chris vickers

I use Renner finishes, not sure if you are able to source it locally, but you can have it shipped. It leaves a totally clear finish on maple, cherry walnut etc. Been really happy with it. The 765 series can be catalyzed if you need the extra protection, but you don't have too. They do have a harder finish that must be catalyzed.

12/22/25       #7: Clear Coating Maple without Yellowi ...
Michael R Member

Thanks Chris. I've heard a lot about Renner and I know they make a great product. It would have to be shipped in but that's not a problem. Thanks for the info and Merry Christmas!!!!

12/22/25       #8: Clear Coating Maple without Yellowi ...
chris vickers

I love that finish line, been using it for a couple years now and won't use anything else. Best of luck.

Merry Christmas

12/25/25       #9: Clear Coating Maple without Yellowi ...
JeffA

Besides a white wash, I have put a small amount of white pigment in my clears to help keep it as non yellow as possible. I can't remember how much. If you do a self seal I can't imagine it's much more than 5 grams per quart. But I don't imagine as well as I used to......

12/25/25       #10: Clear Coating Maple without Yellowi ...
Michael R Member

JeffA, if that works, that would skip the process of wood stain white washing. Glad I created this thread because I'm finding many ways of holding the true value of maple wood color.

When I was picking up cherry veneer core many months ago, one of the warehouse workers said to me that I must have an unbelievable amount of years of experience in the cabinet making trade. I told him I am still learning and he thought I was kidding him. It's so true. That's the purpose of these woodworking and finishing chat rooms. Thanks again!

12/25/25       #11: Clear Coating Maple without Yellowi ...
Chemmy

Michael R, sorry for the long time to respond, I was in the hospital.
Your correct, what I was offering was bout the finish itself not yellowing, not the maple itself, the other responses were on target as to using pigmented toner or stain/ glaze. Just keep in mind that not all white stains are made from or with titanium dioxide,
and you will get long lasting results..!!
Merry Christmas..!!

12/26/25       #12: Clear Coating Maple without Yellowi ...
Michael R Member

Chemmy, Sorry to hear you were in the hospital, hope all is well now with you. Thank you for referencing the other posts are in good favor with you. I use Zar wood stain and they do use the titanium dioxide, which is good news because I've been using them forever. Thanks again for chiming in and reading through this thread and checking back!!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!