Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Dining table failure

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Dining table failure

12/20/13       
Mike Barker  Member

I recently made a trestle table for a client who supplied the lumber. Top dimensions are 40x83x1.25. The breadboard ends were attached with tenon, glued. A few months after delivery a crack developed in the end of the glued up panel not at a joint. I checked some residual lumber and the MC was 12%+, something I know I should have checked prior, hindsite, assume, etc. etc. My Bad! My question is could the split have been avoided or caused by the gluing of the breadboard ends?

12/20/13       #2: Dining table failure ...
Dave Nauman

The breadboard end should only be glued in the middle. The outside tenons on the top should have elongated holes drilled for pegging the breadboard to the top. Drawboring the peg holes, that is drilling the tenon hole slightly closer to the shoulder than the holes in the breadboard mortice draws everything up tight. With a breadboard edge there will be noticeable seasonal variations as far as whether or not the the top's edges are aligned with the breadboard's ends.

12/20/13       #3: Dining table failure ...
mark

There is certainly an incompatibility issue between the glued breadboard, air dried lumber, and (I assume) the climate controlled environment that the table lives in. Aside from yourself as the craftsperson, the glued breadboard should get the lion's share of the blame, as a traditional breadboard would not have resulted in a crack under the same circumstances. I will say that a glued breadboard does not necessarily result in failure, but it can't be left to luck. You said it: your bad.

12/22/13       #4: Dining table failure ...
Fonkee

Sounds like a classic cross grain situation compounded with bad woodworking. Hind "site" indeed.

12/23/13       #5: Dining table failure ...
Mike Barker  Member

Ouch! Uhhh thanks guys. Truth burns sometimes. Thanks for your help.

12/24/13       #6: Dining table failure ...
Jimbo

I hope you learn from your mistake. You do realize that the customer views you as the expert. You should take it seriously and become that expert. If you don't, then you are ripping people off. I don't understand why so many guys think that they can just open up a shop and do this stuff on their own, with little to no knowledge of the trade. Its disrespectful.

1/12/14       #7: Dining table failure ...
Bryant White

Website: http://www.bryantbuilds.com

I had the exact thing happen with a very large office desk. The lumber was sourced from a reputable yard and was kept in doors while in my possession. 9 months later after delivery the end cracked at the glue joint for about 1" then pulled a split into the adjoining board. The customer told me that the area that split had "putty" in the joint. The glue was not old (Titebond 3). This clued me in that the board had more moisture in it at on end and caused the failure. The office was also very very hot and dry in the winter. I replaced the table top at my cost. All I can figure is that it may have been exposed to weather before it was shipped to my shop.

1/12/14       #8: Dining table failure ...
Gary

Bryant, Did you also have fully glued bread board ends?

1/12/14       #9: Dining table failure ...
Bryant White

No I did not glue across the tenon in the bread board. It had a little glue in the center and was pinned. One in the center and two outside. The outer ones were driven through slots so they could move with expansion and contraction. The tenon of the top (which was hidden) was also cut shorter than the mortise length so it too could expand and contract. However I know another maker who did fully glue a breadboard and sure enough his table formed a split. A way around this can be a sliding dovetail bread board. It's a little tricky, but just requires some accurate router setup and a little hand fitting. I have seen it done successfully on some new and 18th cent. tables. Once in place you simply pin/nail/screw the center.

2/15/14       #10: Dining table failure ...
Gene Wengert-WoodDoc

When lumber is dried, sometimes there are very small end splits...maybe a big split right at the end, which will be cut off, but the split actually goes further...hard to see with the eye. So, if you put that end (with the microscopic split) in a top, when the top does shrink, even a little bit, that existing microscopic crack will open. End coating of lumber before drying is widely practiced to eliminate this issue (mostly), but not everyone end coats before drying or uses enough coating material.

2/25/15       #12: Dining table failure ...
markbattles

Website: http://v-dubfurniture.com/

The outer ones were driven through slots so they could move with expansion and contraction. The tenon of the top (which was hidden) was also cut shorter than the mortise length so it too could expand and contract. -

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)