Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Reclaimed Fence Boards on Plywood

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Reclaimed Fence Boards on Plywood

11/25/14       
John Eugster  Member

Website: http://www.woodworksbyjohn.com

I have a potential client that wants a media stand with drawers made with reclaimed materials. Where I live there isn't much available in reclaimed material (broad category) but I have found a lot of 1" x 6" Redwood fence boards. My idea is to laminate them to Baltic Birch plywood, possibly mitering the edges to make it appear as a solid, thick board. Has anyone done that? My thought is to glue and brad them to the ply then sand and finish. My concern is this -- will they start cupping and does the bottom side of the ply need boards as well to equalize things? Just like veneering a substrate but with 1" materials instead of a veneer.
If you have experience with this I'd appreciate your thoughts.

11/25/14       #2: Reclaimed Fence Boards on Plywood ...
Bill Richardson  Member

Website: http://www.awwtx.com

Shouldn't be a problem as far as attaching the boards to a substrate, however I've not done it with boards that width or with redwood. We build restaurant tables with repurposed wood. These tables are reclaimed gymnasium flooring with 1 1/2" particle board substrate. They are 30" wide, a total of 2 1/2" thick and 18 feet long.


View higher quality, full size image (2592 X 1944)


View higher quality, full size image (2592 X 1944)


View higher quality, full size image (2592 X 1944)

11/25/14       #3: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

Thanks Bill, appreciate your response and help. Now if the potential client just comes through with a deposit . !

11/25/14       #4: Reclaimed Fence Boards on Plywood ...
Bill Richardson  Member

Website: http://www.awwtx.com

If they are unfamiliar with the repurposed market, the sticker shock may take them out. Folks seem to think old wood is cheap wood.

11/25/14       #5: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

I agree Bill and with the current emphasis and popularity of the recycled stuff the folks that have it want a premium for it! This is a guy on Craigslist who says all boards are a dollar each so that's doable.

11/25/14       #6: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

Whoops, that's $5.00 each

11/26/14       #7: Reclaimed Fence Boards on Plywood ...
rich c.

John, You do know that solid wood shrinks and expands, right? So what moisture content are the fence boards? What happens to your glued and nailed assembly when the furnace starts running? Solid shrinks, plywood doesn't. Fence boards will split, you'll see the plywood between the boards, and it won't stay flat. It's going to be a mess.

11/26/14       #8: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

Bill, that is one of my major concerns too. I live in Las Vegas where humidity is generally in the single digits, winter time low teens. I've mentioned that to the client and he has a coffee table made in a similar fashion. I will probably rip the boards to narrower widths to hopefully counter the cupping concern. These boards are bone dry, usually if something built here stays here humidity changes aren't too much of an issue. Currently working on an Armoire of genuine Mahogany, the wood has been resawn and stickered (8/4) for a few days with no change in them. Appreciate your input, still waiting for the client to okay the job. Have a Happy Thanksgiving!

11/26/14       #9: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

Sorry, last response was meant for Rich C. in regards to the wood movement --- it's a problem. No place near here to get solid beams or other types of antique lumber

12/4/14       #10: Reclaimed Fence Boards on Plywood ...
Jesse Andreini Member

Gluing and brad nailing seems unnecessary and troublesome to me. Why wouldn't you simply build the drawer box and then apply a drawer face of redwood? Attach in such a way that it floats for movement and adjustment. If you want to get crazy, I have had success making panels of a lattice construction, two courses 1/2" thick, with 3/32" gaps between the edges, stapled and glued at each intersection. That's what the doors are on the fir coffee table recently posted here. I build with a lot of reclaimed fir in seattle, and the incredible stability of old fir may let me get away with too much cheating the rules of wood movement, but I always kind of considered them more guidelines. I hope that's some pretty nice redwood if it's ten bucks a board foot.
Also, I like the green tables, but with our general love of pointing out unbalanced panel construction, I am surprised no one has told bill he can't build them that way. I had a teacher who taught me that you can get away with cheating wood movement only as long as you don't know any better, and then it will stop working for you.

12/4/14       #11: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

Thanks for all of your input, I bought a couple of the boards ($5.00 each) and made a Nativity Scene as well as these samples. They are bone dry so will run them through the planer to flatten one side which will be glued and brad nailed to shop Maple ply; edged to give it thickness. Drawer unit on bottom same treatment but basically drawer boxes with the boards screwed to them to allow for any adjustments needed. Most definitely tell the client that wood can move and things may change -- he likes the look of the images attached which were simply wire brushed and top coated with varnish. I like your outlook Jesse on the wood movement, I suppose that ignorance is bliss!


View higher quality, full size image (608 X 319)

12/4/14       #12: Reclaimed Fence Boards on Plywood ...
Jesse Andreini

That is some nice redwood. Flatsawn, tight grain. That's what some of the best old fir I've seen is cut like, too; you probably couldn't get it new at any price. It's a vg world for old-growth softwoods now.

12/6/14       #13: Reclaimed Fence Boards on Plywood ...
Bill Richardson  Member

Website: http://www.awwtx.com

Jessie, I wanted to ask you about your comments. The tables I posted were tongue and groove flooring attached to substrate in the same manner as general flooring. I recognize there will still be some movement even though the material is over 50 years old. How, then, should I have configured those tables?

12/6/14       #14: Reclaimed Fence Boards on Plywood ...
Jesse Andreini

I went to a local college with a great woodworking program, loved it, and have been building furniture and casework for about four years. I'm a pretty crafty fellow, come from a long line of engineers, and have some good design sense. But I'm not even close to telling older or at least more experienced cabinetmakers how they ought to build. I was just poking a little fun at how often we woodwebbers tell each other what will and will not work. I think the tables are awesome, and they look well-made. They are more balanced than a lot of panels that also "work" even if they "shouldn't". I think if you laid up that flooring on a 3/4" substrate it would probably have some problems. But maybe not. As an aside, I often hear the idea that old wood won't move, and I don't find that to be true. I think often old wood is just stable wood in the first place, and stays stable in old age, as we all hope to.

12/7/14       #15: Reclaimed Fence Boards on Plywood ...
Bill Richardson  Member

Website: http://www.awwtx.com

I appreciate your comments. I'm always looking to learn, and try to better myself on every project.

I agree with ongoing wood movement for the most part. If the old wood is not substantially altered, in my experience it remains pretty stable. If milled heavily, it reverts back to a new wood behavior.

12/7/14       #16: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

The only thing I'd plan on doing is to remove about 1/16" from one side to give a bit of flatness and a better glue surface. Client's being kind of problematic so time will tell!

2/9/15       #17: Reclaimed Fence Boards on Plywood ...
John Eugster  Member

Website: http://www.woodworksbyjohn.com

If you're still following this thread here is a link to the final project. Also a picture of it sitting in the clients home. Hard to eliminate the distortion but you get the idea. Appreciate the input you all gave, thanks -- John


View higher quality, full size image (545 X 394)

Woodworks by John

2/9/15       #18: Reclaimed Fence Boards on Plywood ...
Bill Richardson  Member

Website: http://www.awwtx.com

Good Job!!!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)