Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: RE: Table Tops

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

RE: Table Tops

2/2/16       
Tommy

If I cut 3/8 inch thick x 14 -18 inches wide hardwood, that has nice grain for table tops, and I want the table top to look 2 to 2 ½ inch thick, can we put light weight MDF, what size, or what product is better, and take the 3/8 and apply a 45 degree angle to meet the top so that it would look like a solid, thick piece of wood, will that work?

Or is it better to put the 3/8 on the top and sides and lesser species on the bottom over the MDF or other wood to try to do for high-end furniture? The hardwood on the bottom would be stained the same as the top.

What are the thoughts on this?

2/2/16       #2: RE: Table Tops ...
Mvmatt Member

Website: http://ray woodworking.com

Tommy, I think that before you get into the stacked mdf vs. torsion box question or the solid edge vs veneered edge question you should take a step back and consider the issues that may result from your choice of hardwood thickness. A 3/8 inch board is just that, a board, and it will want to move across its width like a board. Veneer can be glued and fit into a mitered frame because it is so thin that the forces of expansion/contraction are so slight as to be easily held in check by the glue bond. I do not believe this to be so with 3/8 inch thick hardwood.
While I will be interested to hear from others regarding shop sawn veneer, I would be shooting for a final veneer thickness closer to 3/32 than 3/8.

2/3/16       #3: RE: Table Tops ...
Tom Gardiner

I agree with Mymatt, 3/8" thick "veneers" will be deadly. Even if you manage to press it flat which would only be possible with a moisture free adhesive such as epoxy or PU, the resulting top would crack with the first change in humidity.
I recommend looking at a veneer supplier such as Certainly Woods who sell thick veneer. I have pressed 1/16" for exterior doors but I would recommend 1/25" or 1/32" for table tops. You will have plenty of thickness for sanding.
For substrate substrate, I prefer particleboard and I would build a torsion box with 1/2" p-core.

2/4/16       #4: RE: Table Tops ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

A few years ago I made a flame cherry cabinet top that was about 18" x 84" x 1" thick. I only had one really nice 8" wide flame cherry board so had to come up with a way to make that one board into the entire top surface.

The solution was to resaw that board into three 1/4" layers that were glued to the face of a full width cherry blank I'd made out of non-figured cherry. I then profiled an edge detail (using a raised panel cutter) that hid the seam between the flame upper layer and the main cherry sub-surface.

This worked really well and the top has been stable for the 3 to 4 years since construction.

You could take the same concept and increase it to the thickness you require. However I'd be concerned about any 2 1/2" thick solid top unless handled correctly. If I were applying 1/4" to the top of a thick solid core I'd be inclined to apply a 1/4" layer to the bottom as well. That will give a glue line moisture barrier 1/4" in from both faces. I'd also want to use very stable boards for the core.....or perhaps edge glue 3" wide boards together to help in stability.

The alternative on the core is to make an approximately 1" thick top and band it with a thicker edge applied to the bottom surface around the edges. The ends would need end grain strips glued on as vs. picture framing the ends with length wise boards so they will expand and contract with the rest of the top.

BH Davis

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)