Subject: Re: Table Top Curve/ Warp

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Table Top Curve/ Warp

1/24/18       
Thomas

I had a custom farm table made from red oak recently and after 3 days in my house it has bowed/ warped 3/16"... now at 7/16"

The red oak was air dried for about 20 months prior to milling. It seems the bottom (flat image) has dried more rapidly than the top (image with the X)
The grain orientation looks good, alternating and the overall construction looks fine as we..
At the same time we had them make a barn door, and there are no warping issues with that. Same tree, same wood, same room in my house.

The finish on the table is tung oil with a clear coat on the top. 2 coats tung oil on the bottom, 3 on the top.

The glass shown was on the table (photo 3, right side up) after about 24 hours, then removed. The table warped about 3/16 of an inch, then once the glass was removed, it continued to what is now 7/16. I took the table off the base and flipped (image 1 & 2) it to see if gravity would help and put the glass back to give it some weight... it did not. This is why you see a few different photos of the table on the base.

Now for my question:
1) What could be the main cause of this warping, considering the info above.
2) What are some suggestions to correct?

If you need more photos I can e-mail them. Thanks for your help and feedback in advance.


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)

1/24/18       #2: Table Top Curve/ Warp ...
duster

I see 3 issues:

1. the cross grain cleat on the ends of the table top are inhibiting the oak panel's abiltity to shrink or swell with humidity changes. Remove the cleats and most of the cupping on the top will probably go away. If the cleats were installed just to make the top look thicker, they should have matched the grain orientation of the top.

2. you stated that the clear coat was only applied to the top side. To keep solid wood panels stable, an equal amount of finish should be applied to both sides.

3. the glass on top of the wood is also causing the moisture transfer from humidity changes to be unequal. On a veneer top this wouldn't be an issue.

You don't show a photo of your barn door, but I imagine it has the same finish on both sides and no glass.

Your builder needs to redo the top, because it ain't gonna get better...

1/25/18       #3: Table Top Curve/ Warp ...
Kevin Jenness

As Duster points out, the cross-grain cleat on the end is the main problem.

Additionally, if "air dried" means in equilibrium with exterior conditions, the lumber should have been dried further to match its intended use.

The maker should redo the top after reviewing proper construction related to predictable moisture related wood movement.

1/25/18       #4: Table Top Curve/ Warp ...
David R Sochar Member

Your questions, answered:

1. Cross grain construction inhibiting the free movement of wood across grain is the direct result of not using a professional woodworker of good reputation. This is typically caused by a drive to save money, and asking the wrong person/people to do something they are not qualified to do.

2. Have the builder rework the top correctly and for no cost to you. But first, insist he learn his errors and know how to correct them. If he refuses, find a professional shop to do the work.

Suggestions:

1. 20 months air drying sounds good, but what is the moisture content of the wood? It can be used with as high as 12-14% MC, but the construction details are even more important. The top will move more than a kiln dried top as it reaches the EMC- equilibrium moisture content. Movement is OK, as long as it is understood and accommodated by the builder.

2. Do away with the glass top. That solution was from a time (60 yrs ago) when nitrocellulose finishes were so soft they had to be protected. Have a professional finisher spray a catalyzed varnish or lacquer designed for such an application. It will be very durable. Keep in mind that wood tables will age and not be perfect surfaces. They will reflect the life and activities of the household, as they should.

1/25/18       #5: Table Top Curve/ Warp ...
rich c.

Since the builder shows no regard for wood movement, he may have glued and screwed the base to the table top, adding to the issue.

3/21/18       #6: Table Top Curve/ Warp ...
Bruce H

Firstly this is a professional forum as stated in the posting rules and not suited for homeowner questions. That said, the original question was addressed as to a probable cause and possible fix.

I don't agree with asking the person who made the to fix it for free. Some of the blame lies with the owner who may or may not have made design decisions that are part of the issue. As David pointed out, "This is typically caused by a drive to save money, and asking the wrong person/people to do something they are not qualified to do. " The OP didn't ask for blame but those who responded fixed it squarely on the maker.

A "professional" shop might not have made the mistake but they weren’t hired to do the project. It's just my observation...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)