Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Entry Door Panel Thickness

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Entry Door Panel Thickness

11/12/18       
Derek Member

I am currently making an entry door for my home from Oak. I have milled all the rails and stiles to 1.75" thick and I now will begin to make the doors raised panels. I will be using a raised panel bit with my router table to create the panels for the door. My question is at what thickness should my panels be?

I have both 4/4 and 8/4 rough material. I would like to use the 4/4 material for the panels however I am thinking this will be way to thin for the door.

I was wondering if I milled two panels to 7/8 thickness and created my raised profile so that the tounge on the panel was 1/4 thick. Dado a 1/2 inch groove in the door and stack two raised panels back to back to fit in the 1/2 inch groove. Are there any reasons that I am not seeing as to why this might be a bad idea? My other option would be to laminate the two panels but I would like to bypass laminating if possible to save myself some time.

11/12/18       #2: Entry Door Panel Thickness ...
mike

I have made an entry door for myself 2 inches thick and came across the same problem so what i did was to make 2 panels and put them back to back as you described except i put a 3/8 sheet of insulation between them. The insulation was the type used for vinyl siding. Never had a problem with it.

11/14/18       #3: Entry Door Panel Thickness ...
John Member

You will be better off if you use two separate panels. They will be able to slide past each other with the different RH levels inside vs. outside and have less tendency to warp/crack than one, full thickness panel. You can make them any thickness you want, really, even thicker than 1-3/4" when combined if you want though I don't like the look. Mine are usually 1-1/4 to 1-3/8" combined thickness with a 1-3/4" door with a tongue 5/16 - 3/8" on the edge of the raised panels. But there are no absolute rules (or at least I'm unaware if there are) so if you want to use 7/8" panels go to it.

Be sure to finish the panels on all edges and both sides, too. I put a sheet of aluminum foil between the panels as a vapor barrier, but if you use a wider dado or thinner panels you could use closed cell foam instead for slightly better thermal performance.

John

12/7/18       #4: Entry Door Panel Thickness ...
Larry

I do similar to John but use a sheet of stiff plastic between.

12/10/18       #5: Entry Door Panel Thickness ...
Derek Member

Thanks. I will definitely go with two panels then. This will actually be made for a house in Panama. Fortunately there is not much of a temperature change year round. Just tends to be a bit more humid during rainy season.

12/10/18       #6: Entry Door Panel Thickness ...
Larry

Temperature doesn't have much affect on wood, moisture does. Direct sun can heat the wood and drive the moisture out. The affect takes place first on the outside surface resulting in that surface trying to become concave. If enough force is generated, it will crack. I'm guessing that thinner panels are more likely to have less differential than thick ones. But they would also be weaker. Choose a moisture level in the lumber that will be at equilibrium with it's use location.

4/6/19       #7: Entry Door Panel Thickness ...
Jean Member

two panels options is great.

1/30/26       #9: Entry Door Panel Thickness ...
Seven Member

Website: https://www.zonledoors.com/

Furniture and door coordination is such a key detail for cohesive interior design! Matching the wood grain and finish of your cabinetry with your entry doors can elevate the whole space’s vibe. These solid wood door and furniture style matching tips share how to pick complementary tones without clashing.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)